# US 2014/0271339 A1 · Copper alloy for electronic device, method for producing copper alloy for electronic device, and copper alloy rolled material for electronic device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0271339 A1
- Document ID: US20140271339A1
- Status: Published application
- Kind: A1
- Application number: 14/291,335
- Filed: 2014-05-30
- Published: 2014-09-18
- Earliest claimed: 2010-05-14
- Assignees: Mitsubishi Materials Corporation
- Applicants: Mitsubishi Materials Corporation
- Inventors: Yuki Ito; Kazunari Maki
- Web page: https://patentgrep.com/patent/US20140271339A1

## CPC

- H01B 1/026: {Alloys based on copper}
- C22C 1/02: by melting {(C22C1/1036 takes precedence)}
- C22C 1/03: using master alloys
- C22C 9/04: with zinc as the next major constituent
- C22F 1/08: of copper or alloys based thereon
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

One aspect of this copper alloy for an electronic device is composed of a binary alloy of Cu and Mg which includes Mg at a content of 3.3 to 6.9 atomic %, with a remainder being Cu and inevitable impurities, and a conductivity σ (% IACS) is within the following range when the content of Mg is given as A atomic %, σ≦{1.7241/(−0.0347×A2+0.6569×A+1.7)}×100. Another aspect of this copper alloy is composed of a ternary alloy of Cu, Mg, and Zn which includes Mg at a content of 3.3 to 6.9 atomic % and Zn at a content of 0.1 to 10 atomic %, with a remainder being Cu and inevitable impurities, and a conductivity σ (% IACS) is within the following range when the content of Mg is given as A atomic % and the content of Zn is given as B atomic %, σ≦{1.7241/(X+Y+1.7)}×100, X=−0.0347×A2+0.6569×A and Y=−0.0041×B2+0.2503×B.

## Claims

### Claim at position 1

1-7. (canceled)

### Claim 8

A copper alloy for an electronic device,
wherein the copper alloy is composed of a ternary alloy of Cu, Mg, and Zn,
the ternary alloy comprises Mg at a content in a range of 3.3 to 6.9 atomic % and Zn at a content in a range of 0.1 to 10 atomic %, with a remainder being Cu and inevitable impurities, and
a conductivity σ (% IACS) is within the following range when the content of Mg is given as A atomic % and the content of Zn is given as B atomic %,
σ≦{1.7241/(X′+Y′+1.7)}×100
X′=−0.0292×A2+0.6797×A
Y′=−0.0038×B2+0.2488×B.

### Claim 9

A copper alloy for an electronic device,
wherein the copper alloy is composed of a ternary alloy of Cu, Mg, and Zn,
the ternary alloy comprises Mg at a content in a range of 3.3 to 6.9 atomic % and Zn at a content in a range of 0.1 to 10 atomic %, with a remainder being Cu and inevitable impurities, and
with regard to scanning electron microscope observation, an average number of intermetallic compounds having grain sizes of 0.1 μm or more is in a range of 1/μm2 or less.

### Claim 10

A copper alloy for an electronic device,
wherein the copper alloy is composed of a ternary alloy of Cu, Mg, and Zn,
the ternary alloy comprises Mg at a content in a range of 3.3 to 6.9 atomic % and Zn at a content in a range of 0.1 to 10 atomic %, with a remainder being Cu and inevitable impurities,
a conductivity σ (% IACS) is within the following range when the content of Mg is given as A atomic % and the content of Zn is given as B atomic %, and
with regard to scanning electron microscope observation, an average number of intermetallic compounds having grain sizes of 0.1 μm or more is in a range of 1/μm2 or less,
σ≦{1.7241/(X′+Y′+1.7)}×100
X′=−0.0292×A2+0.6797×A
Y′=−0.0038×B2+0.2488×B.

### Claim 11 (depends on 8)

The copper alloy for an electronic device according to claim 8,
wherein a Young's modulus E is in a range of 125 GPa or less, and a 0.2% proof stress σ0.2 is in a range of 400 MPa or more.

### Claim 12

(canceled)

### Claim 13 (depends on 8)

A rolled copper alloy for an electronic device, which is composed of the copper alloy for an electronic device according to claim 8,
wherein a Young's modulus E is in a range of 125 GPa or less, and a 0.2% proof stress σ0.2 is in a range of 400 MPa or more.

### Claim 14 (depends on 13)

The rolled copper alloy for an electronic device according to claim 13,
wherein the rolled copper alloy is used as a copper material that constitutes a terminal, a connector, or a relay.

### Claim 15 (depends on 9)

The copper alloy for an electronic device according to claim 9,
wherein a Young's modulus E is in a range of 125 GPa or less, and a 0.2% proof stress σ0.2 is in a range of 400 MPa or more.

### Claim 16 (depends on 10)

The copper alloy for an electronic device according to claim 10,
wherein a Young's modulus E is in a range of 125 GPa or less, and a 0.2% proof stress σ0.2 is in a range of 400 MPa or more.