# US 2014/0271338 A1 · High Strength Alloys for High Temperature Service in Liquid-Salt Cooled Energy Systems

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0271338 A1
- Document ID: US20140271338A1
- Status: Published application
- Kind: A1
- Application number: 13/834,985
- Filed: 2013-03-15
- Published: 2014-09-18
- Earliest claimed: 2013-03-15
- Assignees: UT-Battelle, LLC
- Applicants: Ut-Battelle, LLC
- Inventors: David E. Holcomb; Govindarajan Muralidharan; Dane F. Wilson
- Web page: https://patentgrep.com/patent/US20140271338A1

## CPC

- C22C 19/057: {with the maximum Cr content being less 10%}
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

An essentially cobalt-free alloy consists essentially of, in terms of weight percent: 6.3 to 7.2 Cr, 0.5 to 2 Al, 0 to 5 Fe, 0.7 to 0.8 Mn, 9 to 12.5 Mo, 0 to 6 Ta, 0.75 to 3.5 Ti, 0.01 to 0.25 Nb, 0.2 to 0.6 W, 0.02 to 0.04 C, 0 to 0.001 B, 0.0001 to 0.002 N, balance Ni. The alloy is characterized by a γ′ microstructural component in the range of 3 to 17.6 weight percent of the total composition. The alloy is further characterized by, at 850° C., a yield strength of at least 60 Ksi, a tensile strength of at least 70 Ksi, a creep rupture life at 12 Ksi of at least 700 hours, and a corrosion rate, expressed in weight loss [g/(cm2sec)]10−11 during a 1000 hour immersion in liquid FLiNaK at 850° C., in the range of 5.5 to 17.

## Claims

### Claim 1

An essentially cobalt-free, γ′-strengthened alloy consisting essentially of, expressed in weight percent of the total composition:
Cr 6.3 to 7.2
Al 0.5 to 2
Fe 0 to 5
Mn 0.7 to 0.8
Mo 9 to 12.5
Ta 0 to 6
Ti 0.75 to 3.5
Nb 0.01 to 0.25
W 0.2 to 0.6
C 0.02 to 0.04
B 0 to 0.001
N 0.0001 to 0.002
Ni balance
said alloy having a γ′ microstructural component in an amount of a calculated weight percent of at least 3 and no more than 17.6; and
said alloy being characterized by, at 850° C., a yield strength of at least 60 Ksi, a tensile strength of at least 70 Ksi, and a creep rupture life at 12 Ksi of at least 700 hours, and a corrosion rate, expressed in weight loss [g/(cm2sec)]10−11 during a 1000 hour immersion in liquid FLiNaK at 850° C., in the range of 5.5 to 17.

### Claim 2 (depends on 1)

An alloy in accordance with claim 1 wherein the range of Al is 0.75 to 2 weight percent.

### Claim 3 (depends on 1)

An alloy in accordance with claim 1 wherein the range of Fe is 0 to 0.05 weight percent.

### Claim 4 (depends on 1)

An alloy in accordance with claim 1 wherein said γ′ microstructural component in an amount of a calculated weight percent of at least 3 and no more than 11.8.

### Claim 5 (depends on 4)

An alloy in accordance with claim 4 wherein said γ′ microstructural component in an amount of a calculated weight percent of at least 3 and no more than 9.4.

### Claim 6 (depends on 1)

An alloy in accordance with claim 1 wherein said yield strength is at least 65 Ksi.

### Claim 7 (depends on 1)

An alloy in accordance with claim 1 wherein said tensile strength is at least 75 Ksi.

### Claim 8 (depends on 1)

An alloy in accordance with claim 1 wherein said creep rupture life is at least 750 hours.

### Claim 9 (depends on 1)

An alloy in accordance with claim 1 wherein said corrosion rate is no more than 8.4.

### Claim 10 (depends on 1)

An alloy in accordance with claim 1 wherein said alloy is further characterized by a corrosion susceptibility index of no less than about 0.14 and no more than about 0.2.