# US 2014/0235811 A1 · Raw materials and methods of manufacturing bio-based epoxy resins

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0235811 A1
- Document ID: US20140235811A1
- Status: Published application
- Kind: A1
- Application number: 14/264,774
- Filed: 2014-04-29
- Published: 2014-08-21
- Earliest claimed: 2010-12-14
- Assignees: Industrial Technology Research Institute
- Applicants: Industrial Technology Research Institute
- Inventors: Chia-Wei YANG; Yuung-Ching SHEEN; Su-Mei Chen WEI; Jer-Young CHEN; Yih-Her CHANG; Yi-Ting WANG
- Web page: https://patentgrep.com/patent/US20140235811A1

## CPC

- C08G 59/4223: {aromatic}
- C08G 59/027: {obtained by epoxidation of unsaturated precursor, e.g. polymer or monomer}
- C08G 59/245: {aromatic}
- C08G 59/42: Polycarboxylic acids; Anhydrides, halides or low molecular weight esters thereof
- C08G 59/687: {containing sulfur}
- C08H 6/00: {Macromolecular compounds derived from lignin, e.g. tannins, humic acids}
- C08L 63/00: Compositions of epoxy resins; Compositions of derivatives of epoxy resins
- C08L 97/005: {Lignin}
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08H: DERIVATIVES OF NATURAL MACROMOLECULAR COMPOUNDS (polysaccharides C08B; natural rubber C08C; natural resins or their derivatives C09F; bituminous materials C10)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Disclosed are methods for manufacturing bio-based epoxy resins. The raw materials of the resins include lignin, polyol, solvent, catalyst, acid anhydride, and multi-epoxy compound. The methods of manufacturing the resins include evenly mixing the lignin, the polyol, the catalyst, and the solvent together to form a mixture. The acid anhydride is added to the mixture to process esterification for forming an intermediate product. The multi-epoxy compound is added to the intermediate product to process epoxidation for forming the bio-based epoxy resins. The bio-based epoxy resin has excellent compatibility with the solvent, such that the solvent can be added to the bio-based epoxy resins to form coatings having a tunable solid content. As a result, the coating can be applied to the surfaces of every type of base material.

## Claims

### Claim 1

Raw materials of a bio-based epoxy in, comprising:
100 parts by weight of lignin;
0 to 300 parts by weight of polyol;
200 to 1800 parts by weight of a solvent;
0 to 30 parts by weight of a catalyst;
10 to 700 parts by weight of acid anhydride; and
50 to 1000 parts by weight of a multi-epoxy compound.

### Claim 2 (depends on 1)

The raw materials as claimed in claim 1, wherein the lignin comprises alkali lignin, organosolv lignin, lignosulfonate, or combinations thereof.

### Claim 3 (depends on 1)

The raw materials as claimed in claim 1, wherein the polyol comprises diol, triol, or combinations thereof.

### Claim 4 (depends on 1)

The raw materials as claimed in claim 1, Wherein the solvent comprises a polar aprotic solvent.

### Claim 5 (depends on 1)

The raw materials as claimed in claim 1, wherein the catalyst comprises phenylsulfonic acid or derivatives thereof, sulfuric acid, triphenyl phosphine, or combinations thereof.

### Claim 6 (depends on 1)

The raw materials as claimed in claim 1, wherein the acid anhydride comprises maleic acid anhydride, 1,2,4,5-benzenetetracarboxylic anhydride, trimellitic anhydride, derivatives thereof, or combinations thereof.

### Claim 7 (depends on 1)

The raw materials as claimed in claim 1, wherein an amount of the multi-epoxy compound comprises glycidyl ether, diglycidyl ether, bisphenol A diglycidyl ether, epoxidized vegetable oil, derivatives thereof, or combinations thereof.

### Claim 8 (depends on 1)

The raw materials as claimed in claim 1, wherein the multi-epoxy compound has an epoxy value of 0.02 mol/100 g to 0.8 mol/100 g.

### Claim 9

A method of manufacturing a bio-based epoxy resin, comprising:
mixing 100 parts by weight of lignin, 0 to 300 parts by weight of polyol, 0 to 30 parts by weight of a catalyst, and 200 to 1800 parts by weight of a solvent to form a mixture;
adding 10 to 700 parts by weight of acid anhydride to the mixture, which is heated and reacted to form an intermediate product;
adding 50 to 1000 parts by weight of a multi-epoxy compound to the intermediate product, which is heated and reacted to form a bio-based epoxy resin solution; and
removing the solvent of the bio-based epoxy resin solution to form a bio-based epoxy resin.

### Claim 10 (depends on 9)

The method as claimed in claim 9, further comprising adding 1 to 4 parts by weight of a crosslinker to 4 parts by weight of the bio-based epoxy resin solution before the step of removing the solvent of the bio-based epoxy resin solution to form a bio-based epoxy resin.

### Claim 11 (depends on 10)

The method as claimed in claim 10, wherein the crosslinker includes amine, anhydride, polyamide resin, phenolic resin, or biomass, wherein the biomass includes lignin, carbohydrate, starch, or cellulose.

### Claim 12 (depends on 9)

The method as claimed in claim 9, wherein the bio-based epoxy resin has an epoxy value of 0.01 mol/100 g to 0.2 mol/100 g.

### Claim 13 (depends on 9)

The method as claimed in claim 9, wherein the step of adding the acid anhydride to the mixture, which is heated and reacted to form the intermediate product, is performed at 110° C. to 160° C. for 2 hours to 5 hours.

### Claim 14 (depends on 9)

The method as claimed in claim 9, wherein the step of adding the multi-epoxy compound to the intermediate product, which is heated and reacted to form the bio-based epoxy resin solution, is performed at 70° C. to 150° C. for 0.5 hour to 6 hours.

### Claim 15 (depends on 13)

The method as claimed in claim 13, wherein the bio-based epoxy resin solution is further heated and reacted at 150° C. for 1 hour to 6 hours after the step of adding the multi-epoxy compound to the intermediate product, which is heated and reacted to form the bio-based epoxy resin solution being performed at 70° C. to 150° C. for 0.5 hour to 6 hours.

### Claim 16 (depends on 9)

The method as claimed in claim 9, wherein the step of removing the solvent of the bio-based epoxy resin solution is performed by baking the bio-based epoxy resin solution at 150° C. to 200° C. for 0.5 hour to 3 hours.

### Claim 17 (depends on 9)

The method as claimed in claim 9, further comprising a step of coating the bio-based epoxy resin solution on a substrate before the step of removing the solvent of the bio-based epoxy resin solution.

### Claim 18 (depends on 16)

The method as claimed in claim 16, wherein the step of coating the bio-based epoxy resin on the substrate comprises spin coating, dip coating, brush coating, spray coating, roll coating, or combinations thereof.

### Claim 19 (depends on 16)

The method as claimed in claim 16, wherein the substrate comprises glass, ceramic, stone, plastic, metal, or polymer.