# US 2014/0235795 A1 · Highly functional graft copolymer and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0235795 A1
- Document ID: US20140235795A1
- Status: Published application
- Kind: A1
- Application number: 14/347,212
- Filed: 2011-12-30
- Published: 2014-08-21
- Earliest claimed: 2011-10-18
- Assignees: Korea Institute of Industrial Technology
- Inventors: Dong Hyun Kim; Joon Chul Lee; Hyun Ki Kim; Tae Wan Kim
- Web page: https://patentgrep.com/patent/US20140235795A1

## CPC

- C08F 220/16: of phenols or of alcohols containing two or more carbon atoms
- C08F 4/52: selected from boron, aluminium, gallium, indium, thallium or rare earths (C08F4/14 takes precedence)
- C08F 255/02: on to polymers of olefins having two or three carbon atoms
- C08F 257/02: on to polymers of styrene or alkyl-substituted styrenes
- C08F 255/04: on to ethylene-propylene copolymers {(C08F255/023 takes precedence)}
- C08F 255/08: on to polymers of olefins having four or more carbon atoms
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

This invention relates to a highly functional graft copolymer and a method of preparing the same, and more particularly, to a highly functional graft copolymer including a main chain of a highly elastic ethylene-based terpolymer including, at a predetermined molar ratio, an ethylene unit, an α-olefin unit having 6 to 12 carbon atoms, and at least one functional unit selected from the group consisting of divinylbenzene and p-methylstyrene, and a side chain of a polar polymer for imparting functionality, and to a method of preparing the highly functional graft copolymer by performing anionic polymerization after catalytic polymerization using a metallocene catalyst.

## Claims

### Claim 1

A graft copolymer, comprising:
a main chain of a highly elastic ethylene-based terpolymer comprising 60˜95 mol % of an ethylene unit, 3˜35 mol % of an α-olefin unit having 6 to 12 carbon atoms, and 0.5˜5 mol % of at least one functional unit selected from the group consisting of divinylbenzene and p-methylstyrene; and
a side chain of a polar polymer; and
having a glass transition temperature of −60˜−20° C. and a fracture strength of 20˜60 MPa.

### Claim 2 (depends on 1)

The graft copolymer of claim 1, wherein the main chain comprises 80˜95 mol % of an ethylene unit, 4˜18 mol % of an α-olefin unit having 6 to 12 carbon atoms, and 0.5˜2 mol % of at least one functional unit selected from the group consisting of divinylbenzene and p-methylstyrene.

### Claim 3 (depends on 1)

The graft copolymer of claim 1, wherein the polar polymer is a polar polymer having at least one polar group selected from among OH group and NH2 group, or an acrylate-based homopolymer or copolymer.

### Claim 4 (depends on 1)

The graft copolymer of claim 1, which has a scratch resistance of 13˜20 N.

### Claim 5 (depends on 1)

The graft copolymer of claim 1, which has a hardness of 60˜90 A.

### Claim 6 (depends on 1)

The graft copolymer of claim 1, which has an elongation of 500˜1,200%.

### Claim 7

A method of preparing a graft copolymer, comprising:
polymerizing 60˜95 mol % of an ethylene monomer, 3˜35 mol % of an α-olefin monomer having 6 to 12 carbon atoms, and 0.5˜5 mol % of at least one functional monomer selected from the group consisting of divinylbenzene and p-methylstyrene using a metallocene catalyst (step 1); and
adding a polymer obtained in step 1 with a polar monomer and performing anionic polymerization (step 2).

### Claim 8 (depends on 7)

The method of claim 7, wherein the metallocene catalyst has a center metal comprising a Group 4 transition metal and a ligand comprising cyclopentadienyl or a derivative thereof; fluorenyl or a derivative thereof; or indenyl or a derivative thereof; and has a bridge (ansa) structure or a non-bridge structure.

### Claim 9 (depends on 8)

The method of claim 8, wherein the metallocene catalyst is used.

### Claim 10 (depends on 7)

The method of claim 7, wherein a catalytic activity upon polymerizing is 2,500˜15,000.

### Claim 11 (depends on 7)

The method of claim 7, wherein the metallocene catalyst is used together with an alkyl aluminoxane cocatalyst, an organic alkyl aluminum cocatalyst, a boron compound cocatalyst, or mixtures thereof.

### Claim 12 (depends on 11)

The method of claim 11, wherein the alkyl aluminoxane cocatalyst is selected from the group consisting of methyl aluminoxane, ethyl aluminoxane, propyl aluminoxane, butyl aluminoxane and isobutyl aluminoxane;
the organic alkyl aluminum cocatalyst is selected from the group consisting of trimethylaluminum, triethylaluminum and diisobutylaluminum chloride; and
the boron compound cocatalyst is selected from the group consisting of tris(pentafluorophenyl)borane, N,N-dimethylanilium tetrakis(pentafluorophenyl)borate, and triphenylmethyliniumtetrakispentafluoroborate.

### Claim 13 (depends on 7)

The method of claim 7, wherein the polymerizing in step 1 is performed at 20˜70° C.

### Claim 14 (depends on 7)

The method of claim 7, wherein the polymerizing in step 1 is performed for a period of time ranging from 20 min to 1 hr.

### Claim 15 (depends on 7)

The method of claim 7, wherein the polar monomer is a polar monomer having at least one polar group selected from among OH group and NH2 group, or at least one acrylate-based monomer.

### Claim 16 (depends on 7)

The method of claim 7, wherein an initiator for the anionic polymerization in step 2 is at least one selected from the group consisting of an alkali metal suspension, an alkyl lithium reagent, an aryl lithium reagent, a Grignard reagent, alkylated aluminum, an organic radical anion, a transition metal π-allyl complex and an ionization radiation.

### Claim 17 (depends on 7)

The method of claim 7, wherein the polymerization in step 2 is performed at −20˜0° C.

### Claim 18 (depends on 7)

The method of claim 7, wherein the polymerization in step 2 is performed for a period of time ranging from 20 min to 3 hr.