# US 2014/0234551 A1 · Deposition of Coatings on Substrates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0234551 A1
- Document ID: US20140234551A1
- Status: Published application
- Kind: A1
- Application number: 14/350,714
- Filed: 2012-10-26
- Published: 2014-08-21
- Earliest claimed: 2011-10-28
- Assignees: Laser Fusion Technologies Ltd.
- Applicants: Laser Fusion technologies Ltd.
- Inventors: Martin Sparkes; William O'Neill; Andrew Cockburn; Rocco Lupoi; Matthew Bray
- Web page: https://patentgrep.com/patent/US20140234551A1

## CPC

- B05B 3/001: {incorporating means for heating or cooling, e.g. the material to be sprayed}
- B23K 26/034: {Observing the temperature of the workpiece}
- B23K 26/0823: {Devices involving rotation of the workpiece}
- B23K 26/083: {Devices involving movement of the workpiece in at least one axial direction}
- B23K 26/342: Build-up welding
- C23C 24/04: Impact or kinetic deposition of particles
- B23K 2101/06: Tubes
- B23K 2103/04: Steel {or steel} alloys
- B23K 2103/24: Ferrous alloys and titanium or alloys thereof
- B05B: SPRAYING APPARATUS; ATOMISING APPARATUS; NOZZLES (spray-mixers with nozzles B01F25/72; processes for applying liquids or other fluent materials to surfaces by spraying B05D)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A process and apparatus are disclosed for the deposition of a layer of a first material onto a substrate of a second material. Powder particles of the first material are entrained into a carrier gas flow to form a powder beam directed to impinge on the substrate. This defines a powder beam footprint region at the substrate. The powder beam and the substrate are moved relative to each other to move the powder beam footprint relative to the substrate, thereby to deposit the layer of the first material. A laser is operated to cause direct, local heating of at least one of a forward substrate region and a powder beam footprint region. The laser beam direction is defined with reference to a plane coincident with or tangential to a surface of the substrate at the centre of the laser beam footprint in terms of an elevation angle from the plane to the laser beam direction and in terms of an acute azimuthal angle from the movement direction to the laser beam direction. The elevation angle is 80° or less and the azimuthal angle is ±60° or less. In the apparatus, there are provided at least three laser sources arrayed around the powder beam footprint, the angular spacing between the laser sources being 120° or less.

## Claims

### Claim 1

A coating process for the deposition of a layer of a first material onto a substrate of a second material, the second material optionally being different from the first material, the process including the steps:
entraining powder particles of the first material into a carrier gas flow to form a powder beam directed to impinge on the substrate, thereby defining a powder beam footprint region at the substrate;
causing relative movement of the powder beam and the substrate in a movement direction to move the powder beam footprint relative to the substrate to deposit the layer of the first material; and
operating a laser source to direct a laser beam along a laser beam direction to provide a laser beam footprint to cause direct, local heating of at least one of the forward substrate region and the powder beam footprint region,
the laser beam direction being defined with reference to a plane coincident with or tangential to a surface of the substrate at the centre of the laser beam footprint in terms of an elevation angle from the plane to the laser beam direction and in terms of an acute azimuthal angle from the movement direction to the laser beam direction,
wherein the elevation angle is 80° or less and the azimuthal angle is ±60° or less.

### Claim 2 (depends on 1)

The coating process according to claim 1, wherein the elevation angle is 30° or more.

### Claim 3

The coating process according to claim wherein the movement direction is variable, in order to provide variation in the shape of the deposited layer.

### Claim 4 (depends on 1)

The coating process according to claim 1, wherein there are provided two or more laser sources and the azimuthal angle for at least one of the laser sources is non-zero.

### Claim 5 (depends on 1)

The coating process according to claim 1, wherein a single layer of the first material is deposited on a substrate of a second material, the first material having a different composition to the second material.

### Claim 6 (depends on 1)

The coating process according to claim 1, wherein multiple layers are applied sequentially, each previously-deposited layer acting as the substrate for the layer being applied.

### Claim 7 (depends on 1)

The coating process according to claim 1 wherein the first material is an anti-corrosion coating or a wear coating.

### Claim 8 (depends on 1)

The coating process according to claim 1, wherein the laser is operated directly to heat the forward substrate region but not the powder beam footprint region.

### Claim 9 (depends on 1)

The coating process according to claim 1, wherein the heating means is operated directly to heat the forward substrate region using a first intensity profile and to heat at least part of the powder beam footprint region using a second intensity profile, wherein the average intensity of the first intensity profile is greater than the average intensity of the second intensity profile.

### Claim 10 (depends on 1)

The coating process according to claim 1, wherein the carrier gas is selected from: nitrogen and air.

### Claim 11 (depends on 1)

The coating process according to claim 1, wherein the carrier gas is not heated.

### Claim 12 (depends on 1)

The coating process according to claim 1, wherein the powder particles in the powder beam have average kinetic energy Ek, Ek optionally varying with position across the powder beam, and Ek is selected so that without direct heating of the forward substrate region and/or the powder footprint region, the powder particles do not adhere to the substrate, the process including the step of selectively deactivating the laser in order to prevent the powder particles from adhering to the substrate.

### Claim 13 (depends on 1)

The coating process according to claim 1, wherein the deposited layer is at least 0.1 mm thick.

### Claim 14 (depends on 1)

The coating process according to claim 1, the process further including the steps:
controlling the laser and the relative movement of the powder beam and the substrate to provide a spatial temperature distribution at the powder footprint region of the substrate in which the local temperature of the substrate is in the range 0.5 Ts to less than Ts in a volume from the surface of the substrate at least up to a depth of 0.2 mm from the surface of the substrate and not more than 0.25 Ts at a depth of 1 mm from the surface of the substrate,
wherein Ts is the solidus temperature (in K) of the second material.

### Claim 15

An apparatus for carrying out a coating process for the deposition of a layer of a first material onto a substrate of a second material, the second material optionally being different from the first material, the process including the steps:
entraining powder particles of the first material into a carrier gas flow to form a powder beam directed to impinge on the substrate, thereby defining a powder beam footprint region at the substrate:
causing relative movement of the powder beam and the substrate in a movement direction to move the powder beam footprint relative to the substrate to deposit the layer of the first material: and
operating a laser source to direct a laser beam along a laser beam direction to provide a laser beam footprint to cause direct. local heating of at least one of the forward substrate region and the powder beam footprint region.
the laser beam direction being defined with reference to a plane coincident with or tangential to a surface of the substrate at the centre of the laser beam footprint in terms of an elevation angle from the plane to the laser beam direction and in terms of an acute azimuthal angle from the movement direction to the laser beam direction,
wherein the elevation angle is 80° or less and the azimuthal angle is ±60° or less,
wherein in the apparatus there are provided at least three laser sources arrayed around the powder beam footprint, the angular spacing between the laser sources being 120° or less.

### Claim 16

An apparatus for carrying out a coating process for the deposition of a layer of a first material onto a substrate of a second material, the second material optionally being different from the first material the process including the steps:
entraining powder particles of the first material into a carrier gas flow to form a powder beam directed to impinge on the substrate, thereby defining a powder beam footprint region at the substrate;
causing relative movement of the powder beam and the substrate in a movement direction to move the powder beam footprint relative to the substrate to deposit the layer of the first material: and
operating a laser source to direct a laser beam along laser beam direction to provide a laser beam footprint to cause direct, local heating of at least one of the forward substrate region and the powder beam footprint region,
the laser beam direction being defined with reference to a plane coincident with or tangential to a surface of the substrate at the centre of the laser beam footprint in terms of an elevation angle from the plane to the laser beam direction and in terms of an acute azimuthal angle from the movement direction to the laser beam direction,
wherein the elevation angle is 80° or less and the azimuthal angle is ±60° or less,
wherein in the apparatus there are provided at least two laser sources arrayed around the powder beam footprint, each providing a different laser beam direction and each laser beam direction satisfying the requirement of an elevation angle of 80° or less and an azimuthal angle of ±60° or less.