# US 2014/0231743 A1 · Memory cells and methods of forming memory cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0231743 A1
- Document ID: US20140231743A1
- Status: Published application
- Kind: A1
- Application number: 14/259,376
- Filed: 2014-04-23
- Published: 2014-08-21
- Earliest claimed: 2012-10-15
- Assignees: Micron Technology, Inc.
- Applicants: Micron Technology, Inc.
- Inventors: D. V. Nirmal Ramaswamy; Murali Balakrishnan; Alessandro Torsi; Noel Rocklein
- Web page: https://patentgrep.com/patent/US20140231743A1

## CPC

- H10N 70/041: {Modification of switching materials after formation, e.g. doping (shaping H10N70/061)}
- H10N 70/24: {based on migration or redistribution of ionic species, e.g. anions, vacancies}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/841: {Electrodes}
- H10N 70/883: {Oxides or nitrides}
- G11C 13/0007: {comprising metal oxide memory material, e.g. perovskites}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- G11C: STATIC STORES (semiconductor memory devices H10B)

## Abstract

Some embodiments include memory cells having programmable material between a pair of electrodes. The programmable material includes a material selected from the group consisting of a metal silicate with a ratio of metal to silicon within a range of from about 2 to about 6, and metal aluminate with a ratio of metal to aluminum within a range of from about 2 to about 6. Some embodiments include methods of forming memory cells. First electrode material is formed. Programmable material is formed over the first electrode material, with the programmable material including metal silicate and/or metal aluminate. Second electrode material is formed over the programmable material, and then an anneal is conducted at a temperature within a range of from about 300° C. to about 500° C. for a time of from about 1 minute to about 1 hour.

## Claims

### Claim at position 1

1-29. (canceled)

### Claim 30

A method of forming a memory cell, comprising:
forming first electrode material over a base;
forming programmable material over the first electrode material; the programmable material comprising a region comprising a composition selected from the group consisting of a metal silicate with a ratio of metal to silicon within a range of from about 2 to about 6, and a metal aluminate with a ratio of metal to aluminum within a range of from about 2 to about 6; and
forming second electrode material over the programmable material and subsequently annealing the programmable material.

### Claim 31 (depends on 30)

The method of claim 30 wherein the forming of the programmable material further comprises forming a dielectric material over the region; the dielectric material having a thickness within a range of from about 10 Å to about 50 Å, and comprising one or more of hafnium oxide, lanthanum oxide, ruthenium oxide, titanium oxide and zirconium oxide.

### Claim 32 (depends on 31)

The method of claim 31 wherein the dielectric material comprises one or both of hafnium oxide and zirconium oxide.

### Claim 33 (depends on 30)

The method of claim 30 wherein the region is a first region; and further comprising forming an additional region of the programmable material, with said additional region comprising a composition selected from the group consisting of a metal silicate with a ratio of metal to silicon greater than 6, and a metal aluminate with a ratio of metal to aluminum greater than 6.

### Claim 34 (depends on 33)

The method of claim 33 wherein the additional region is formed before the first region.

### Claim 35 (depends on 33)

The method of claim 33 wherein the additional region is formed after the first region.

### Claim 36 (depends on 30)

The method of claim 30 wherein both electrode materials are directly against the programmable material; wherein one of the electrode materials is of a composition that chemically interacts with the programmable material, wherein the other of the electrode materials is of a composition that does not chemically interact with the programmable material; and wherein the programmable material comprises a higher concentration of metal adjacent said other of the electrode materials than adjacent said one of the electrode materials.

### Claim 37 (depends on 36)

The method of claim 36 wherein said one of the electrode materials consists of metal selected from the group consisting of hafnium, lanthanum, ruthenium, titanium, zirconium, and mixtures thereof.

### Claim 38

A memory cell containing programmable material which comprises:
a first region which includes a material selected from the group consisting of a metal silicate with a ratio of metal to silicon within a range of from about 2 to about 6, and a metal aluminate with a ratio of metal to aluminum within a range of from about 2 to about 6; and
a second region comprising a material selected from the group consisting of a metal silicate with a ratio of metal to silicon of greater than 6, and a metal aluminate with a ratio of metal to aluminum of greater than 6.

### Claim 39 (depends on 38)

The memory cell of claim 38 wherein the second region comprises a material selected from the group consisting of a metal silicate with a ratio of metal to silicon of at least about 8, and a metal aluminate with a ratio of metal to aluminum of at least about 8.

### Claim 40 (depends on 38)

The memory cell of claim 38 wherein the programmable material comprises a third region; and wherein the third region comprises a material selected from the group consisting of a metal silicate with a ratio of metal to silicon within a range of from about 2 to about 6, and a metal aluminate with a ratio of metal to aluminum within a range of from about 2 to about 6.

### Claim 41 (depends on 40)

The memory cell of claim 40 wherein the second region is between the first region and the third region.

### Claim 42 (depends on 40)

The memory cell of claim 40 wherein the programmable material comprises a fourth region; and wherein the fourth region comprises a material selected from the group consisting of a metal silicate with a ratio of metal to silicon of greater than 6, and a metal aluminate with a ratio of metal to aluminum of greater than 6.