# US 2014/0213706 A1 · Unvulcanized rubber composition for calendaring and method for manufacturing topping rubber using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0213706 A1
- Document ID: US20140213706A1
- Status: Published application
- Kind: A1
- Application number: 14/147,933
- Filed: 2014-01-06
- Published: 2014-07-31
- Earliest claimed: 2013-01-25
- Assignees: Sumitomo Rubber Industries, Ltd.
- Applicants: Sumitomo Rubber Industries, Ltd.
- Inventors: Shinichiro HONDA
- Web page: https://patentgrep.com/patent/US20140213706A1

## CPC

- C08L 7/00: Compositions of natural rubber
- B29D 30/0681: {Parts of pneumatic tyres; accessories, auxiliary operations}
- C08K 3/04: Carbon
- C08L 9/00: Compositions of homopolymers or copolymers of conjugated diene hydrocarbons
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29D: PRODUCING PARTICULAR ARTICLES FROM PLASTICS OR FROM SUBSTANCES IN A PLASTIC STATE (making granules B29B9/00; making preforms B29B11/00)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

An unvulcanized rubber composition for calendaring has an elongational viscosity of not more than 102 kPa when measured at a temperature of 95 deg. C., and a shear velocity of 500 to 2000 (1/second). A method for manufacturing a topping rubber for a cord ply embedded in a pneumatic tire is characterized in that, the unvulcanized rubber composition is extended and shaped with the use of calender rolls whose surface temperature is 60 to 100 deg. C.

## Claims

### Claim 1

An unvulcanized rubber composition for calendaring during which the unvulcanized rubber composition is subjected to elongation deformation by calender rolls and which is characterized by having an elongational viscosity of not more than 102 kPa when measured at a temperature of 95 deg. C., and a shear velocity of 500 to 2000(1/second).

### Claim 2 (depends on 1)

The unvulcanized rubber composition according to claim 1, wherein the elongational viscosity is not less than 2 kPa.

### Claim 3 (depends on 1)

The unvulcanized rubber composition according to claim 1 which is used as topping rubber for a cord ply embedded in a pneumatic tire.

### Claim 4 (depends on 3)

The unvulcanized rubber composition according to claim 3, wherein the cord ply is a tread reinforcing belt ply embedded in a tread portion of the pneumatic tire.

### Claim 5 (depends on 1)

The unvulcanized rubber composition according to claim 1 which comprises: base rubber including 55 to 100 parts by weight of natural rubber and 45 to 0 parts by weight of isoprene rubber; and 40 to 60 parts by weight of carbon black with respect to 100 parts by weight of the base rubber.

### Claim 6 (depends on 1)

A method for manufacturing a topping rubber for a cord ply embedded in a pneumatic tire, comprising a step of extending and shaping the unvulcanized rubber composition as set forth in claim 1 with the use of calender rolls whose surface temperature is 60 to 100 deg. C. so that the unvulcanized rubber composition is shaped into the topping rubber within a temperature range of from 60 to 140 deg. C.

### Claim 7 (depends on 2)

The unvulcanized rubber composition according to claim 2 which is used as topping rubber for a cord ply embedded in a pneumatic tire.

### Claim 8 (depends on 2)

The unvulcanized rubber composition according to claim 2 which comprises: base rubber including 55 to 100 parts by weight of natural rubber and 45 to 0 parts by weight of isoprene rubber; and 40 to 60 parts by weight of carbon black with respect to 100 parts by weight of the base rubber.

### Claim 9 (depends on 3)

The unvulcanized rubber composition according to claim 3 which comprises: base rubber including 55 to 100 parts by weight of natural rubber and 45 to 0 parts by weight of isoprene rubber; and 40 to 60 parts by weight of carbon black with respect to 100 parts by weight of the base rubber.

### Claim 10 (depends on 4)

The unvulcanized rubber composition according to claim 4 which comprises: base rubber including 55 to 100 parts by weight of natural rubber and 45 to 0 parts by weight of isoprene rubber; and 40 to 60 parts by weight of carbon black with respect to 100 parts by weight of the base rubber.

### Claim 11 (depends on 2)

A method for manufacturing a topping rubber for a cord ply embedded in a pneumatic tire, comprising a step of extending and shaping the unvulcanized rubber composition as set forth in claim 2 with the use of calender rolls whose surface temperature is 60 to 100 deg. C. so that the unvulcanized rubber composition is shaped into the topping rubber within a temperature range of from 60 to 140 deg. C.

### Claim 12 (depends on 3)

A method for manufacturing a topping rubber for a cord ply embedded in a pneumatic tire, comprising a step of extending and shaping the unvulcanized rubber composition as set forth in claim 3 with the use of calender rolls whose surface temperature is 60 to 100 deg. C. so that the unvulcanized rubber composition is shaped into the topping rubber within a temperature range of from 60 to 140 deg. C.

### Claim 13 (depends on 4)

A method for manufacturing a topping rubber for a cord ply embedded in a pneumatic tire, comprising a step of extending and shaping the unvulcanized rubber composition as set forth in claim 4 with the use of calender rolls whose surface temperature is 60 to 100 deg. C. so that the unvulcanized rubber composition is shaped into the topping rubber within a temperature range of from 60 to 140 deg. C.

### Claim 14 (depends on 5)

A method for manufacturing a topping rubber for a cord ply embedded in a pneumatic tire, comprising a step of extending and shaping the unvulcanized rubber composition as set forth in claim 5 with the use of calender rolls whose surface temperature is 60 to 100 deg. C. so that the unvulcanized rubber composition is shaped into the topping rubber within a temperature range of from 60 to 140 deg. C.