# US 2014/0213060 A1 · Method of patterning a low-k dielectric film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0213060 A1
- Document ID: US20140213060A1
- Status: Published application
- Kind: A1
- Application number: 14/159,832
- Filed: 2014-01-21
- Published: 2014-07-31
- Earliest claimed: 2013-01-29
- Assignees: Applied Materials, Inc.
- Inventors: Chia-Ling Kao; Sean S. Kang; Srinivas D. Nemani
- Web page: https://patentgrep.com/patent/US20140213060A1

## CPC

- H10P 50/73: {using masks for insulating materials}
- H10P 50/267: {using plasmas}
- H10P 50/283: {by chemical means}
- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- H10W 20/081: {by forming openings in the dielectric parts}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Methods of patterning low-k dielectric films are described. In an example, In an embodiment, a method of patterning a low-k dielectric film involves forming and patterning a metal nitride mask layer above a low-k dielectric layer. The low-k dielectric layer is disposed above a substrate. The method also involves passivating the metal nitride mask layer by treating with a plasma based on O2/N2/SixFy. The method also involves etching a portion of the low-k dielectric layer.

## Claims

### Claim 1

A method of patterning a low-k dielectric film, the method comprising:
forming and patterning a metal nitride mask layer above a low-k dielectric layer, the low-k dielectric layer disposed above a substrate;
passivating the metal nitride mask layer by treating with a plasma based on O2/N2/SixFy; and
etching a portion of the low-k dielectric layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein passivating the metal nitride mask layer comprises depositing a protecting material layer on the metal nitride layer.

### Claim 3 (depends on 2)

The method of claim 2, further comprising:
subsequent to etching the portion of the low-k dielectric layer, removing the protecting material layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein passivating the metal nitride mask layer comprises modifying a surface of the metal nitride layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein treating with the plasma based on O2/N2/SixFy further comprises forming a protecting layer on a second portion of the low-k dielectric layer, wherein the second portion is not etched during the etching of the portion of the low-k dielectric layer.

### Claim 6 (depends on 1)

The method of claim 1, wherein SixFy is SiF4.

### Claim 7 (depends on 1)

The method of claim 1, wherein the passivating the metal nitride mask layer by treating with the plasma based on O2/N2/SixFy is a carbon-free process.

### Claim 8 (depends on 1)

The method of claim 1, wherein forming and patterning the metal nitride mask layer above the low-k dielectric layer comprises forming a layer of titanium nitride or a layer of tantalum nitride above a porous carbon-doped oxide (SiCOH) layer having a dielectric constant of less than 2.7.

### Claim 9

A method of patterning a low-k dielectric film, the method comprising:
forming and patterning a metal nitride mask layer above a low-k dielectric layer, the low-k dielectric layer disposed above a substrate, wherein patterning the metal nitride layer comprises plasma etching performed at a pressure of approximately 40 mTorr, a source power (Ws) of approximately 200 W, a chemistry based on CF4, C4F8, N2 and Ar, at a showerhead to wafer gap of approximately 1.6 mm, for a duration of approximately 30 seconds;
passivating the metal nitride mask layer by treating with a plasma process performed at a pressure of approximately 20 mTorr, a source power (Ws) of approximately 150 W, a chemistry based on SiF4, N2, O2 and Ar, at a showerhead to wafer gap of approximately 1.25 mm, for a duration of approximately 220 seconds; and
etching a portion of the low-k dielectric layer, wherein the etching comprises plasma etching performed at a pressure of approximately 40 mTorr, a source power (Ws) of approximately 200 W, a chemistry based on SiF4, C4F8, N2 and Ar, at a showerhead to wafer gap of approximately 1.6 mm, for a duration of approximately 85 seconds.

### Claim 10 (depends on 9)

The method of claim 9, wherein passivating the metal nitride mask layer by treating with the plasma process further comprises forming a protecting layer on a second portion of the low-k dielectric layer, wherein the second portion is not etched during the etching of the portion of the low-k dielectric layer.

### Claim 11 (depends on 9)

The method of claim 9, wherein passivating the metal nitride mask layer comprises depositing a protecting material layer on the metal nitride layer.

### Claim 12 (depends on 11)

The method of claim 11, further comprising:
subsequent to etching the portion of the low-k dielectric layer, removing the protecting material layer with a plasma process performed at a pressure of approximately 15 mTorr, a chemistry based on N2 and O2, at a showerhead to wafer gap of approximately 3.5 mm, for a duration of approximately 15 seconds.

### Claim 13 (depends on 9)

The method of claim 9, wherein passivating the metal nitride mask layer comprises modifying a surface of the metal nitride layer.

### Claim 14 (depends on 9)

The method of claim 9, wherein the passivating the metal nitride mask layer by treating with the plasma process is a carbon-free process.

### Claim 15 (depends on 9)

The method of claim 9, wherein forming and patterning the metal nitride mask layer above the low-k dielectric layer comprises forming a layer of titanium nitride or a layer of tantalum nitride above a porous carbon-doped oxide (SiCOH) layer having a dielectric constant of less than 2.7.

### Claim 16

A method of patterning a low-k dielectric film, the method comprising:
forming and patterning a metal nitride mask layer above a low-k dielectric layer, the low-k dielectric layer disposed above a substrate;
passivating the metal nitride mask layer by treating with a plasma based on O2/N2/SixFy;
etching a portion of the low-k dielectric layer;
repeating the passivating and etching to form trenches having sidewalls in the low-k dielectric layer; and
subsequent to repeating the passivating and etching to form the trenches, passivating the metal nitride mask layer and the sidewalls of the trenches formed in the low-k dielectric layer by treating with a plasma based on O2/N2/SixFy, wherein the passivating comprises depositing a protecting material layer on the metal nitride layer and on the sidewalls of the trenches formed in the low-k dielectric layer; and
etching to extend the trenches in the low-k dielectric layer.

### Claim 17 (depends on 16)

The method of claim 16, further comprising:
subsequent to etching to extend the trenches in the low-k dielectric layer, removing the protecting material layer.

### Claim 18 (depends on 16)

The method of claim 16, wherein SixFy is SiF4.

### Claim 19 (depends on 16)

The method of claim 16, wherein the passivating the metal nitride mask layer by treating with the plasma based on O2/N2/SixFy is a carbon-free process.

### Claim 20 (depends on 16)

The method of claim 16, wherein forming and patterning the metal nitride mask layer above the low-k dielectric layer comprises forming a layer of titanium nitride or a layer of tantalum nitride above a porous carbon-doped oxide (SiCOH) layer having a dielectric constant of less than 2.7.