# US 2014/0213048 A1 · Method of Making a FinFET Device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0213048 A1
- Document ID: US20140213048A1
- Status: Published application
- Kind: A1
- Application number: 13/756,104
- Filed: 2013-01-31
- Published: 2014-07-31
- Earliest claimed: 2013-01-31
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Sey-Ping Sun; Sung-Li Wang; Chin-Hsiang Lin; Neng-Kuo Chen; Clement Hsingjen Wann
- Web page: https://patentgrep.com/patent/US20140213048A1

## CPC

- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 30/62: Fin field-effect transistors [FinFET]
- H10D 30/751: {having composition variations in the channel regions}
- H10D 64/01: Manufacture or treatment
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A FinFET device is fabricated by first receiving a FinFET precursor. The FinFET precursor includes a substrate, fins on the substrate, isolation regions on sides of the fins and dummy gate stacks on the substrate including wrapping a portion of the fin, which is referred to as a gate channel region. The dummy gate stacks is removed to form a gate trench and a gate dielectric layer is deposited in the gate trench. A metal stressor layer (MSL) is conformably deposited on the gate dielectric layer. A capping layer is deposited on the MSL. A thermal treatment is applied to the MSL to achieve a volume expansion. Then the capping layer is removed and a metal gate (MG) is formed on the MSL.

## Claims

### Claim 1

A method for fabricating a fin-type field-effect transistor (FinFET) device, the method comprising:
receiving a FinFET precursor, the FinFET precursor including:
a substrate;
fins on the substrate;
isolation regions on sides of the fins; and
dummy gate stacks on the substrate including a portion wrapping the fin;
removing the dummy gate stacks to form a gate trench;
depositing a gate dielectric layer in the gate channel region in the gate trench;
forming a metal stressor layer (MSL) on the gate dielectric layer;
depositing a capping layer on the MSL;
performing a thermal treatment to the MSL;
removing the capping layer after the thermal treatment; and
forming a metal gate (MG) on the MSL.

### Claim 2 (depends on 1)

The method of claim 1, wherein the MSL is selected to have substantial larger volume expansion during the thermal treatment.

### Claim 3 (depends on 2)

The method of claim 2, wherein the MSL includes amorphous-tungsten (α-W).

### Claim 4 (depends on 2)

The method of claim 2, wherein the MSL includes one or more conductive materials from the group consisting of Ti, Ag, Al, TiAlN, TaC, TaCN, TaSiN, Mn, Zr, TiN, TaN, Ru, Mo, Al, WN, Co, Ni, TiC, TiAlC, TaAlC and Cu.

### Claim 5 (depends on 3)

The method of claim 3, wherein the α-W MSL is formed by atomic layer deposition (ALD).

### Claim 6 (depends on 3)

The method of claim 3, wherein the α-W is formed by:
substantial conformably depositing a poly-crystalline W layer is on the gate dielectric layer; and
then applying an implantation process to the poly-crystalline W layer to convert it to the α-W.

### Claim 7 (depends on 1)

The method of claim 1, wherein a temperature of the thermal treatment is substantial higher than a temperature of the deposition process of the MSL.

### Claim 8 (depends on 1)

The method of claim 1, wherein the capping layer is selected to have a substantial smaller volume expansion than the volume expansion of the MSL during the thermal treatment.

### Claim 9 (depends on 8)

The method of claim 8, wherein the capping layer includes silicon nitride while the MSL includes the α-W layer.

### Claim 10 (depends on 1)

The method of claim 1, wherein the capping layer includes silicon nitride and the MSL includes α-W.

### Claim 11 (depends on 1)

The method of claim 1, wherein a thickness of the capping layer is selected to meet a predetermined magnitude of induced strain of the gate channel.

### Claim 12 (depends on 1)

The method of claim 1, wherein a thickness of the MSL is selected to cooperate with a thickness of the capping layer to meet a predetermined magnitude of an induced strain of the gate channel.

### Claim 13 (depends on 1)

The method of claim 1, wherein after removing the capping layer, the MSL remains on the top of gate dielectric layer.

### Claim 14 (depends on 1)

The method of claim 1, wherein the MG includes poly-crystalline W layer deposited on the W MSL after receiving the thermal treatment.

### Claim 15

A method for fabricating a fin-type field-effect transistor (FinFET) device, the method comprising:
receiving a FinFET precursor, the FinFET precursor including:
a substrate;
fins on the substrate;
isolation regions on sides of the fins; and
dummy gate stacks on the substrate wrapping a portion of the fin (a gate channel region);
removing the dummy gate stack to expose the gate channel region;
depositing a gate dielectric layer in the channel region;
depositing a metal stressor layer (MSL) on the HK gate dielectric layer, wherein the MSL is selected to obtain a first volume expansion in a subsequent thermal treatment;
depositing a capping layer on the MSL, wherein the capping layer is selected to obtain a second volume expansion in the subsequent thermal treatment, wherein the second volume expansion is substantial smaller than the first volume expansion;
performing a thermal treatment to the MSL to achieve the first volume expansion, wherein a temperature of the thermal treatment is substantial higher than a temperature of MSL deposition;
removing the capping layer after the thermal treatment; and
forming metal gate (MG) on the MSL.

### Claim 16 (depends on 15)

The method of claim 15, wherein the MSL includes amorphous-tungsten (α-W).

### Claim 17 (depends on 16)

The method of claim 16, wherein the α-W MSL is formed by:
depositing a substantially conformable poly-crystalline W layer is on the gate dielectric layer; and
then applying an implantation process to the poly-crystalline W layer to convert it to the α-W.

### Claim 18 (depends on 15)

The method of claim 15, wherein the capping layer includes silicon nitride.

### Claim 19

A method for fabricating a fin field-effect transistor (FinFET) device, the method comprising:
receiving a FinFET precursor, the FinFET precursor including:
a substrate;
fins on the substrate;
isolation regions on sides of the fins; and
dummy gate stacks on the substrate, including at least one dummy gate stack wrapping a portion of the fin (a gate channel region);
removing the dummy gate stack to expose the gate channel region;
depositing a gate dielectric layer in the channel region;
depositing a amorphous-tungsten (α-W) metal stressor layer (MSL) on the HK gate dielectric layer;
depositing a silicon nitride (SiN) capping layer having on the α-W MSL;
performing a thermal treatment to the α-W MSL;
removing the SiN capping layer after the thermal treatment; and
forming metal gate (MG) on the thermally treated W MSL.

### Claim 20 (depends on 19)

The method of claim 19, wherein a temperature of the thermal treatment is substantial higher than a temperature of α-W MSL deposition.