# US 2014/0213044 A1 · Method for producing periodic crystalline silicon nanostructures

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0213044 A1
- Document ID: US20140213044A1
- Status: Published application
- Kind: A1
- Application number: 14/240,034
- Filed: 2012-08-22
- Published: 2014-07-31
- Earliest claimed: 2011-08-25
- Assignees: Helmholtz-Zentrum Berlin fuer Materialien und Energie GmbH
- Inventors: Christiane Becker; Tobias Sontheimer; Matthias Bockmeyer; Eveline Rudigier-Voigt; Bernd Rech
- Web page: https://patentgrep.com/patent/US20140213044A1

## CPC

- H10P 14/3802: {Crystallisation or recrystallisation of non-monocrystalline semiconductor materials, e.g. regrowth}
- G02B 1/005: {made of photonic crystals or photonic band gap materials (photonic band-gap structures or photonic lattices in integrated optics G02B6/1225; photonic band-gap structures or photonic lattices in optical fibres G02B6/02295)}
- G02B 6/13: Integrated optical circuits characterised by the manufacturing method
- H10D 62/40: Crystalline structures
- B82Y 20/00: Nanooptics, e.g. quantum optics or photonic crystals
- B82Y 40/00: Manufacture or treatment of nanostructures
- G02B 6/1225: {comprising photonic band-gap structures or photonic lattices}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A method for producing periodic crystalline silicon nanostructures of large surface area by: generating a periodic structure having a lattice constant of between 100 nm and 2 μm on a substrate, the substrate used being a material which is stable at up to at least 570° C., and the structure being produced with periodically repeating shallow and steep areas/flanks, and, subsequently, depositing silicon by directed deposition onto the periodically structured substrate, with a thickness in the range from 0.2 to 3 times the lattice constant, or 40 nm to 6 μm, at a substrate temperature of up to 400° C., followed by thermally treating the deposited Si layer to effect solid-phase crystallization, at temperatures between 570° C. and 1400° C., over a few minutes up to several days, and optionally subsequently wet-chemically selective etching to remove resultant porous regions of the Si layer.

## Claims

### Claim 1

A process for preparing a periodic crystalline silicon nanostructure, comprising:
generating a periodic structure with a lattice constant a between 200 nm and 2 μm on a substrate, the substrate comprising a material that is stable up to at least 570° C., to obtain a periodically structured substrate comprising periodically alternating flat regions and steep flanks; then
depositing silicon onto the periodically structured substrate in a directional deposition process with a substrate temperature of up to 400° C., to obtain a coated, structured substrate comprising a deposited Si layer having a thickness of from 0.2 to 3 times a Si lattice constant: and then
thermally treating the deposited Si layer at a temperature between 570° C. and 1,400° C. for a period lasting from a few minutes to several days, to at least partially solid phase crystallize the deposited Si layer.

### Claim 2 (depends on 1)

The process of claim 1, further comprising, after the thermally treating the deposited Si layer;
selectively etching the deposited Si layer in a wet chemical process to remove the porous Si regions formed.

### Claim 3 (depends on 1)

The process of claim 1, wherein the substrate comprises glass.

### Claim 4 (depends on 1)

The process of claim 1, wherein electron beam evaporation is used as a directed deposition method.

### Claim 5 (depends on 2)

The process of claim 2, wherein the selectively etching enhances solid phase crystallization.

### Claim 6 (depends on 1)

The process of claim 1, wherein the depositing deposits amorphous silicon.

### Claim 7 (depends on 1)

The process of claim 1, wherein the depositing deposits semi-crystalline silicon.

### Claim 8 (depends on 1)

The process of claim 1, wherein the depositing deposits amorphous silicon and semi-crystalline silicon.

### Claim 9 (depends on 1)

The process of claim 1, wherein a periodicity of the periodically alternating flat regions and steep flanks less than 2 μm.

### Claim 10 (depends on 1)

The process of claim 1, wherein the depositing deposits a silicon layer with a thickness of from 40 nm to 6 μm.

### Claim 11 (depends on 1)

The process of claim 1, wherein the thermally treating forms two silicon phases.

### Claim 12 (depends on 1)

The process of claim 1, wherein the thermally treating forms crystalline silicon in at least one of the fiat regions of the substrate.

### Claim 13 (depends on 1)

The process of claim 1, wherein the thermally treating forms porous nanocrystallinc material on at least one of the steep flanks of the texture.

### Claim 14 (depends on 1)

The process of claim 1, wherein the substrate temperature of the depositing is in a range of from 300° C. to 400° C.

### Claim 15 (depends on 1)

The process of claim 1, wherein the period of the thermally treating lasts from a few minutes to 20 hours.

### Claim 16 (depends on 1)

The process of claim 1, wherein the thermally treating is carried out at a temperature between 570° C. and 600° C.

### Claim 17 (depends on 1)

The process of claim 1, wherein the thermally treating is carried out at a temperature between 600° C. and 1,400° C.

### Claim 18 (depends on 2)

The process of claim 2, wherein the substrate comprises glass.

### Claim 19 (depends on 2)

The process of claim 2, wherein the etching is carried out for between 40 to 90 seconds.