# US 2014/0213034 A1 · Method for forming isolation structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0213034 A1
- Document ID: US20140213034A1
- Status: Published application
- Kind: A1
- Application number: 13/752,408
- Filed: 2013-01-29
- Published: 2014-07-31
- Earliest claimed: 2013-01-29
- Assignees: United Microelectronics Corp.
- Applicants: United Microelectronics Corp.
- Inventors: Chia-Lung Chang; Chih-Chien Liu; Jei-Ming Chen; Wen-Yi Teng; Jui-Min Lee; Keng-Jen Lin; Chin-Fu Lin
- Web page: https://patentgrep.com/patent/US20140213034A1

## CPC

- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/0145: {of trenches having shapes other than rectangular or V-shape (H10W10/0143 takes precedence)}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming an isolation structure includes the following steps. A hard mask layer is formed on a substrate and a trench is formed in the substrate and the hard mask layer. A protective layer is formed to cover the trench and the hard mask layer. A first isolation material is filled into the trench. An etching process is performed to etch back part of the first isolation material.

## Claims

### Claim 1

A method for forming an isolation structure, comprising:
forming a hard mask layer on a substrate and a trench in the substrate and the hard mask layer;
forming a protective layer to cover the trench and the hard mask layer;
filling a first isolation material in the trench; and
performing an etching process to etch back parts of the first isolation material.

### Claim 2 (depends on 1)

The method for forming an isolation structure according to claim 1, wherein the isolation structure comprises a shallow trench isolation structure.

### Claim 3 (depends on 1)

The method for forming an isolation structure according to claim 1, wherein the protective layer comprises a non-oxide layer.

### Claim 4 (depends on 1)

The method for forming an isolation structure according to claim 1, wherein the protective layer comprises a silicon layer.

### Claim 5 (depends on 1)

The method for forming an isolation structure according to claim 1, wherein the protective layer is formed through a plasma enhanced chemical vapor deposition (PECVD) process.

### Claim 6 (depends on 1)

The method for forming an isolation structure according to claim 1, wherein the hard mask layer comprises a pad oxide layer and a nitride layer stacked from bottom to top.

### Claim 7 (depends on 1)

The method for forming an isolation structure according to claim 1, wherein the first isolation material is formed through a chemical vapor deposition (CVD) process.

### Claim 8 (depends on 1)

The method for forming an isolation structure according to claim 1, wherein the first isolation material comprises oxide.

### Claim 9 (depends on 1)

The method for forming an isolation structure according to claim 1, wherein a top surface of the back etched first isolation material is lower than the level of a bottom surface of the hard mask layer.

### Claim 10 (depends on 1)

The method for forming an isolation structure according to claim 1, wherein the first isolation material comprises at least avoid, and the first isolation material is etched back until at least a void is exposed.

### Claim 11 (depends on 1)

The method for forming an isolation structure according to claim 1, wherein the etching rate of the etching process to the first isolation material is higher than the etching rate to the protective layer.

### Claim 12 (depends on 1)

The method for forming an isolation structure according to claim 1, further comprising:
filling a second isolation material on the first isolation material in the trench after the first isolation material is etched back.

### Claim 13 (depends on 12)

The method for forming an isolation structure according to claim 12, wherein the second isolation material is formed through a chemical vapor deposition (CVD) process.

### Claim 14 (depends on 12)

The method for forming an isolation structure according to claim 12, wherein the first isolation material and the second isolation material are the same materials.

### Claim 15 (depends on 12)

The method for forming an isolation structure according to claim 12, further comprising:
transforming the protective layer into a part of the first isolation material or the second isolation material after the second isolation material is filled.

### Claim 16 (depends on 15)

The method for forming an isolation structure according to claim 15, wherein the protective layer is transformed into a part of the first isolation material or the second isolation material by performing an annealing process.

### Claim 17 (depends on 16)

The method for forming an isolation structure according to claim 16, wherein the processing temperature of the annealing process is 700° C.˜1000° C.

### Claim 18 (depends on 15)

The method for forming an isolation structure according to claim 15, further comprising:
performing a polishing process to polish the second isolation material until the hard mask layer is exposed after the protective layer is transformed into a part of the first isolation material or the second isolation material.

### Claim 19 (depends on 18)

The method for forming an isolation structure according to claim 18, further comprising:
removing the hard mask layer after the polishing process is performed.