# US 2014/0193287 A1 · Method of producing a shaped part

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0193287 A1
- Document ID: US20140193287A1
- Status: Published application
- Kind: A1
- Application number: 14/204,500
- Filed: 2014-03-11
- Published: 2014-07-10
- Earliest claimed: 2009-12-15
- Assignees: Plansee SE
- Applicants: Plansee SE
- Inventors: MARCO BRANDNER; STEFAN GERZOSKOVITZ; WOLFGANG KRAUSSLER; ALEXANDER LEUPRECHT; ANDREAS VENSKUTONIS
- Web page: https://patentgrep.com/patent/US20140193287A1

## CPC

- B22F 3/12: Both compacting and sintering (by forging B22F3/17)
- B22F 3/02: Compacting only
- B22F 5/00: Manufacture of workpieces or articles from metallic powder characterised by the special shape of the product
- B22F 5/06: of threaded articles, e.g. nuts
- B22F 5/08: of toothed articles, e.g. gear wheels; of cam discs
- C22C 27/06: Alloys based on chromium
- C22C 33/0207: {Using a mixture of pre-alloyed powders or a master alloy}
- C22C 33/0285: {with Cr, Co, or Ni having a minimum content higher than 5%}
- H01M 8/0206: Metals or alloys
- H01M 8/021: Alloys based on iron
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A shaped part that is particularly suited as an interconnector or an end plate for a fuel cell stack, is produced by pressing and sintering a pulverulent starting material. The shaped part has a basic body with a multiplicity of knob-like and/or ridge-like elevations with a height h. Each elevation has two inclined side flanks which lead, proceeding from an end contour of the elevation, via rounded corner portions, directly or via intermediate rectilinear portions, into curved portions with a radius R or R′, which in turn merge into the surface contour, of the basic body. A ratio of the radius R:h or R′:h ranges from 0.25, or preferably from 0.5 to 1.

## Claims

### Claim 1

A method of producing a shaped part, the method comprising:
providing a pulverulent starting material containing at least 20% by weight chromium;
providing a press mold having a mold shape substantially corresponding to a final shape of the shaped part, the shaped part having a disc-shaped or plate-shaped basic body formed with a multiplicity of elevations selected from the group consisting of knob-shaped and ridge-shaped elevations and a surface contour between the elevations;
filling the starting material into the mold having the mold shape substantially corresponding to the final shape of the shaped part and pressing the starting material substantially into the final shape of the shaped part; and
subsequently sintering the shaped part;
defining the final shape with the elevations having a height h from the surface contour of the basic body to an end contour of the elevations, each of the elevations, in cross section, having two inclined side flanks extending from the end contour of the elevation, via rounded corner portions, into curved portions having a radius R and R′, respectively, and merging into the surface contour of the basic body; and
the radius R and R′ lying in a range from 0.15 to 1 mm and a ratio of the radius R and R′ to the height h (R:h, R′:h) lying in a range from 0.5 to 1.

### Claim 2 (depends on 1)

The method according to claim 1, which comprises dimensioning the mold so that the rounded corner portions transition directly into the curved portions.

### Claim 3 (depends on 1)

The method according to claim 1, which comprises dimensioning the mold so that the rounded corner portions are connected to the curved portions via intermediate rectilinear portions having the angle of inclination α and α′, respectively, with regard to the surface contour in a range of 95° to 135°.

### Claim 4 (depends on 3)

The method according to claim 3, which comprises setting the angle of inclination α, α′ within a range of 95° to 120°.

### Claim 5 (depends on 1)

The method according to claim 1, which comprises setting the radius R or R′ within a range of 0.3 to 1 mm.

### Claim 6 (depends on 3)

The method according to claim 3, which comprises setting the angle of inclination α, α′ within a range of 95° to 110°.

### Claim 7 (depends on 1)

The method according to claim 1, which comprises setting the radius R or R′ within a range of 0.3 to 1 mm, and setting the ratio R:h or R′:h within a range of 0.7 to 1.

### Claim 8 (depends on 1)

The method according to claim 1, which comprises setting processing parameters relating to the starting material, the press mold, the single pressing and the sintering to form a shaped part suitable as an interconnector or an end plate of a fuel cell stack.

### Claim 9 (depends on 1)

The method according to claim 1, which comprises providing the pulverulent starting material containing chromium, iron, and at least one rare earth metal.

### Claim 10 (depends on 9)

The method according to claim 9, which comprises providing the pulverulent starting material containing 20 to 30% by weight chromium and 70 to 80% by weight iron with 0.5 to 0.8% by weight of the at least one rare earth metal.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the rare earth metal is yttrium.