- Number: US 2014/0192120 A1
- Document ID: US20140192120A1
- Status: Published application
- Kind: A1
- Application number: 13/851,579
- Filed: 2013-03-27
- Published: 2014-07-10
- Earliest claimed: 2013-01-07
- Assignees: Seiko Epson Corporation
- Applicants: Seiko Epson Corporation
- Inventors: Atsushi NOZAWA
- Web page: https://patentgrep.com/patent/US20140192120A1

## CPC

- B41J 2/01: Ink jet
- B41M 5/502: {characterised by structural details, e.g. multilayer materials (supports, backcoats or intermediate layers for thermal dye transfer donor and receiver sheets B41M5/41, B41M5/42)}
- B41M 5/52: Macromolecular coatings
- C09D 11/326: characterised by the pigment dispersant
- B41M 5/0011: {Pre-treatment or treatment during printing of the recording material, e.g. heating, irradiating (after-treatment of prints B41M7/00; printers for treating or overcoating copy materials before, during or after printing B41J11/0015)}
- B41M 5/5218: {characterised by inorganic additives, e.g. pigments, clays}
- B41J: TYPEWRITERS; SELECTIVE PRINTING MECHANISMS, i.e. MECHANISMS PRINTING OTHERWISE THAN FROM A FORME; CORRECTION OF TYPOGRAPHICAL ERRORS
- B41M: PRINTING, DUPLICATING, MARKING, OR COPYING PROCESSES; COLOUR PRINTING, (correction of typographical errors B41J; processes for applying transfer pictures or the like B44C1/16; fluid media for correction of typographical errors by coating C09D10/00; printing textiles D06P)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

Provided is a recording method of discharging ink including resin and a solvent to a heated recording medium to record an image on the recording medium by an ink jet recording apparatus, in which an absorption amount of the ink per unit mass of the recording medium is equal to or less than 1.0, and a wetting index of the recording medium measured based on JIS K6768 is equal to or more than 46, and when the wetting index is set as x, and the absorption amount of the ink per unit mass of the recording medium is set as y, a relationship of y≧0.002x−0.027 is satisfied.

## Claims

### Claim 1

A recording method of discharging ink including resin and a solvent onto a heated recording medium to record an image on the recording medium by an ink jet recording apparatus,
wherein an absorption amount of the ink per unit mass of the recording medium is equal to or less than 1.0, and a wetting index of the recording medium measured based on JIS K6768 is equal to or more than 46, and
when the wetting index is set as x, and the absorption amount of the ink per unit mass of the recording medium is set as y, a relationship of y≧0.002x−0.027 is satisfied.

### Claim 2 (depends on 1)

The recording method according to claim 1,
wherein, when the wetting index of the recording medium measured based on JIS K6768 is set as x, and the absorption amount of the ink per unit mass of the recording medium is set as y, a relationship of y≧5×1017×x−10.796 is satisfied.

### Claim 3 (depends on 1)

The recording method according to claim 1,
wherein, when the wetting index of the recording medium measured based on JIS K6768 is set as x, and the absorption amount of the ink per unit mass of the recording medium is set as y, a relationship of y≦−0.00552x+3.2429 is satisfied.

### Claim 4 (depends on 1)

The recording method according to claim 1,
wherein the recording medium includes an ink accommodation layer, and
the ink accommodation layer includes at least one kind of a material selected from a group consisting of urethane, acryl, and polyester, and/or at least two kinds of copolymer selected from a group consisting of urethane, acryl, and polyester.

### Claim 5 (depends on 1)

The recording method according to claim 1, wherein the resin included in the ink is thermoplastic resin.

### Claim 6 (depends on 1)

The recording method according to claim 1,
wherein the solvent included in the ink is at least one selected from a group consisting of 2-pyrrolidone, 1,2-hexanediol, dipropylene glycol, and propylene glycol.

### Claim 7 (depends on 1)

The recording method according to claim 1,
wherein a discharging amount of the ink with respect to the recording medium is equal to or more than 14 ng and equal to or less than 23 ng, and resolution of the image recorded on the recording medium is equal to or more than 720×720 dpi.

### Claim 8 (depends on 1)

The recording method according to claim 1,
wherein a surface temperature of the recording medium in a heated state is equal to or more than 40° C. and equal to or less than 60° C.