- Published: 2014-06-05
- Earliest claimed: 2012-12-05
- Applicants: ExxonMobil Chemical Patents Inc.
- Inventors: Pradeep P. Shirodkar; Jianya Cheng; Rahul R. Kulkarni
- Web page: https://patentgrep.com/patent/US20140155553A1

## CPC

- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08J 5/18: Manufacture of films or sheets
- C08L 23/06: Polyethylene
- C08J 2323/08: Copolymers of ethene (C08J2323/16 takes precedence)
- C08J 2423/06: Polyethene
- C08L 2203/16: used for films
- C08L 2207/062: HDPE
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

The present invention relates to polyethylene compositions comprising one or more ethylene polymers and one or more HDPE modifiers, in particular, this invention further relates to polyethylene blends comprising one or more ethylene polymers and one or more HDPE modifiers, wherein the modifier has: 1) a density of greater than 0.94 g/cc; 2) a Mw/Mn greater than 5; 3) a melt index (ASTM 1238, 190° C., 2.16 kg) of less than 0.7 dg/min; and 4) a g′vis of 0.96 or less.

## Claims

### Claim 1

A polyethylene blend composition comprising one or more ethylene polymers and one or more HDPE modifiers, wherein the modifier has: 1) a density of greater than 0.94 g/cc; 2) a Mw/Mn greater than 5; 3) a melt index (ASTM 1238, 190° C., 2.16 kg) of less than 0.7 dg/min; and 4) a g′vis of 0.96 or less.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the modifier has 5 wt % or less of xylene insoluble material.

### Claim 3 (depends on 1)

The composition of claim 1, wherein the blend is formed into a film and the film has a total haze of 20% or less, Elmendorf Tear-MD is greater than 300 grams/mil, dart drop impact is greater than 170 grams/mil, 1% Secant modulus(MD) is greater than 26,000 psi and the coefficient of variation for the film gauge is less than 7%.

### Claim 4 (depends on 1)

The composition of claim 1, wherein the modifier is present at 0.25 wt % to 10 wt %, based upon the weight of the blend.

### Claim 5 (depends on 1)

The composition of claim 1, wherein the polyethylene comprises a copolymer of ethylene and one or more C3 to C20 alphaolefins and has an Mw of 20,000 to 1,000,000 g/mol.

### Claim 6 (depends on 1)

The composition of claim 1, wherein the polyethylene has a density of 0.91 to 0.96 g/cm3.

### Claim 7 (depends on 1)

The composition of claim 1, wherein the modifier is present at from 0.1 wt % to 5 wt % (based upon the weight of the blend); and the polyethylene has a composition distribution breadth index of 60% or more and a density of 0.90 g/cc or more.

### Claim 8 (depends on 1)

The composition of claim 1, wherein the blend is formed into a film and the film has a total haze of 20% or less, a Gauge COV of less than 7%, and a 1% MD Secant Flexural Modulus of 25,000 psi or more.

### Claim 9 (depends on 1)

A polyethylene film comprising the composition of claim 1, said film having a gauge variation that is at least 10% lower than that of film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions and a dart impact strength that is within 20% of a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions.

### Claim 10 (depends on 1)

A polyethylene film comprising the composition of claim 1, said film having a gauge variation that is at least 10% lower than that of film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions and an MD Tear strength that is within 20% of a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions.

### Claim 11 (depends on 1)

A polyethylene film comprising the composition of claim 1, said film having a haze that is at least 10% lower than that of film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions and a dart impact strength that is within 20% of a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions.

### Claim 12 (depends on 1)

A polyethylene film comprising the composition of claim 1, said film having a haze that is at least 10% lower than that of film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions and an MD Tear strength that is within 20% of a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions.

### Claim 13 (depends on 1)

A film comprising the composition of claim 1, said film having a haze of 20% or less.

### Claim 14 (depends on 1)

A film comprising the composition of claim 1, wherein the film has a haze that is at least 15% less than the haze measured on a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions.

### Claim 15 (depends on 1)

A film comprising the composition of claim 1, wherein the film has a gauge variation that is at least 10% less than the gauge variation measured on a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions.

### Claim 16 (depends on 1)

A film comprising the composition of claim 1, wherein the film has a dart impact strength that is greater than or within 30% less than the dart impact strength measured on a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions.

### Claim 17 (depends on 1)

A film comprising the composition of claim 1, wherein the film has an MD Tear strength that is greater than or within 30% less than the MD Tear strength measured on a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions.

### Claim 18 (depends on 1)

A film comprising the blend of claim 1, wherein the film has a gauge variation that is at least 10% less than the gauge variation measured on a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions, and the film has a Dart Drop, in g/mil, that within 30% of the Dart Drop measured on a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions.

### Claim 19 (depends on 1)

A film comprising the blend of claim 1, wherein the film has a gauge variation that is at least 10% less than the gauge variation measured on a film of the same thickness and of the same composition, absent the HDPE modifier, prepared under the same conditions, and the film has an MD Tear strength that is greater than or within 30% less than the MD Tear strength measured on a film of the same thickness and of the same composition, absent the HDPE modifier, prepared under the same conditions.

### Claim 20 (depends on 1)

A film comprising the blend of claim 1, wherein the blend composition has a strain hardening ratio that is at least 10% greater than the strain hardening ratio measured on a composition, absent the modifier, and the film has a Dart Drop, in g/mil, that within 30% of the Dart Drop measured on a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions.

### Claim 21 (depends on 1)

A film comprising the blend of claim 1, wherein the film has a gauge variation that is at least 10% less than the gauge variation measured on a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions, and the film has a haze that is at least 10% less than haze measured on a film of the same thickness and of the same composition, absent the modifier, prepared under the same conditions.

### Claim 22 (depends on 1)

The composition of claim 1 comprising more than 25 wt % (based on the weight of the composition) of one or more ethylene polymers having a g′vis of 0.95 or more and an Mw of 20,000 g/mol or more and at least 0.1 wt % of the modifier, wherein the ethylene polymer has a g′vis of at least 0.25 units higher than the g′vis of the modifier.

### Claim 23 (depends on 1)

The composition of claim 1, wherein the blend is formed into a film and the film has a total haze of 20% or less; a Gauge COV of less than 7%; an Elmendorf tear (MD) of 315 or more g/mil; and a 1% (MD) Secant Flexural Modulus of 25,000 psi or more.