# US 2014/0155520 A1 · Rubber composition for use in tires

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0155520 A1
- Document ID: US20140155520A1
- Status: Published application
- Kind: A1
- Application number: 14/131,829
- Filed: 2012-07-13
- Published: 2014-06-05
- Earliest claimed: 2011-07-14
- Assignees: The Yokohama Rubber Co., Ltd.
- Inventors: Shinya Takeda
- Web page: https://patentgrep.com/patent/US20140155520A1

## CPC

- C08L 47/00: Compositions of homopolymers or copolymers of compounds having one or more unsaturated aliphatic radicals, at least one having two or more carbon-to-carbon double bonds; Compositions of derivatives of such polymers (C08L45/00 takes precedence; of conjugated diene rubbers C08L9/00 - C08L21/00)
- B60C 1/00: Tyres characterised by the chemical composition or the physical arrangement or mixture of the composition
- B60C 1/0016: {Compositions of the tread}
- C08C 19/22: Incorporating nitrogen atoms into the molecule
- C08K 3/04: Carbon
- C08K 3/36: Silica
- C08L 9/00: Compositions of homopolymers or copolymers of conjugated diene hydrocarbons
- C08L 9/06: Copolymers with styrene
- C08L 15/00: Compositions of rubber derivatives (C08L11/00, C08L13/00 take precedence)
- C08L 91/00: Compositions of oils, fats or waxes; Compositions of derivatives thereof
- C08L 93/00: Compositions of natural resins; Compositions of derivatives thereof (of polysaccharides C08L1/00 - C08L5/00; of natural rubber C08L7/00)
- C08K 2201/006: Additives being defined by their surface area
- C08K 2201/014: Additives containing two or more different additives of the same subgroup in C08K
- Y02T 10/86: Optimisation of rolling resistance, e.g. weight reduction
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B60C: VEHICLE TYRES; TYRE INFLATION; TYRE CHANGING; CONNECTING VALVES TO INFLATABLE ELASTIC BODIES IN GENERAL; DEVICES OR ARRANGEMENTS RELATED TO TYRES
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION

## Abstract

A rubber composition comprises from 2 to 50 parts by weight of an aromatic modified terpene resin having a softening point of ≧100° C., and two types of silica, a silica X and a silica Y, at a total quantity of 60 to 130 parts by weight relative to 100 parts by weight of a diene rubber containing from 5 to 50 weight % of a modified S-SBR having a vinyl content of not lower than 60 weight %. A functional group in the modified S-SBR reacts with a silanol group, a proportion of silica relative to the total quantity of a reinforcing filler containing the silica and carbon black is not lower than 85 weight %, a nitrogen specific surface area of the silica X is not lower than 140 m2/g, and a nitrogen specific surface area of the silica Y is not lower than 100 m2/g but lower than 140 m2/g.

## Claims

### Claim 1

A rubber composition for use in tires comprising from 2 to 50 parts by weight of an aromatic modified terpene resin having a softening point of 100° C. or higher, and two types of silica, including a silica X and a silica Y, at a total quantity of 60 to 130 parts by weight relative to 100 parts by weight of a diene rubber containing from 5 to 50 weight % of a solution polymerization-produced terminally modified styrene-butadiene rubber (a modified S-SBR) having a vinyl unit content of not lower than 60 weight %, wherein a functional group in the modified S-SBR reacts with a silanol group on a surface of the silica, a proportion of silica relative to a total quantity of a reinforcing filler containing the silica and carbon black is not lower than 85 weight %, a nitrogen specific surface area of the silica X is not lower than 140 m2/g, a nitrogen specific surface area of the silica Y is not lower than 100 m2/g but lower than 140 m2/g, and where blending quantities of the silica X and the silica Y relative to 100 parts by weight of the diene rubber are deemed to be x parts by weight and y parts by weight respectively, the relationship x/7<y≦x is satisfied.

### Claim 2 (depends on 1)

The rubber composition for use in tires according to claim 1, wherein the functional group in the modified S-SBR is a hydroxyl group.

### Claim 3 (depends on 1)

The rubber composition for use in tires according to claim 1, wherein the functional group in the modified S-SBR is an amino group.

### Claim 4 (depends on 1)

A pneumatic tire that uses the rubber composition for use in tires according to claim 1.

### Claim 5 (depends on 1)

The rubber composition for use in tires according to claim 1, wherein the modified S-SBR has a vinyl unit content of from 60 to 80 weight %.

### Claim 6 (depends on 1)

The rubber composition for use in tires according to claim 1, wherein the functional group is at least one type selected from a hydroxyl group-containing polyorganosiloxane structure, an alkoxysilyl group, a hydroxyl group, an aldehyde group, a carboxyl group, an amino group, an imino group, an epoxy group, an amide group, a thiol group, or an ether group.

### Claim 7 (depends on 6)

The rubber composition for use in tires according to claim 6, wherein the functional group is the hydroxyl group or the amino group.

### Claim 8 (depends on 1)

The rubber composition for use in tires according to claim 1, comprising from 10 to 30 weight % of the modified S-SBR relative to 100 weight % of the diene rubber.

### Claim 9 (depends on 1)

The rubber composition for use in tires according to claim 1, wherein the diene rubber contains from 50 to 95 weight % of diene rubbers other than the modified S-SBR.

### Claim 10 (depends on 1)

The rubber composition for use in tires according to claim 1, wherein the diene rubber contains from 70 to 90 weight % of diene rubbers other than the modified S-SBR.

### Claim 11 (depends on 10)

The rubber composition for use in tires according to claim 10, wherein the diene rubbers other than the modified S-SBR include one or more diene rubbers selected from the group consisting of: natural rubbers, butadiene rubbers, emulsion polymerization-produced styrene-butadiene rubbers, unmodified solution polymerization-produced styrene-butadiene rubbers, solution polymerization-produced terminally modified styrene-butadiene rubbers other than the modified S-SBR, and brominated isobutylene/p-methylstyrene copolymer rubbers.

### Claim 12 (depends on 1)

The rubber composition for use in tires according to claim 1, wherein the aromatic modified terpene resin has a softening point of from 100° C. to 130° C.

### Claim 13 (depends on 1)

The rubber composition for use in tires according to claim 1, comprising from 5 to 50 parts by weight of the aromatic modified terpene resin relative to 100 parts by weight of the diene rubber.

### Claim 14 (depends on 1)

The rubber composition for use in tires according to claim 1, wherein the nitrogen specific surface area of the silica X is from 150 m2/g to 230 m2/g.

### Claim 15 (depends on 1)

The rubber composition for use in tires according to claim 1, wherein the nitrogen specific surface area of the silica X is from 150 m2/g to 185 m2/g.

### Claim 16 (depends on 1)

The rubber composition for use in tires according to claim 1, wherein the nitrogen specific surface area of the silica Y is higher than 100 m2/g and not higher than 130 m2/g.

### Claim 17 (depends on 1)

The rubber composition for use in tires according to claim 1, wherein the nitrogen specific surface area of the silica Y is from 105 m2/g to 130 m2/g.

### Claim 18 (depends on 1)

The rubber composition for use in tires according to claim 1, comprising a total quantity of 80 to 130 parts by weight of the silica relative to 100 parts by weight of the diene rubber.

### Claim 19 (depends on 1)

The rubber composition for use in tires according to claim 1, wherein the proportion of the silica relative to the total quantity of the reinforcing filler containing the silica and carbon black is from 90 to 100 weight %.

### Claim 20 (depends on 1)

The rubber composition for use in tires according to claim 1, further comprising a sulfur-containing silane coupling agent in an amount of from 50 to 12 weight % of the silica.