# US 2014/0154578 A1 · Anode active material including porous silicon oxide-carbon material composite and method of preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0154578 A1
- Document ID: US20140154578A1
- Status: Published application
- Kind: A1
- Application number: 14/168,185
- Filed: 2014-01-30
- Published: 2014-06-05
- Earliest claimed: 2012-11-30
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Jung Woo Yoo; Je Young Kim; Yong Ju Lee; Seung Youn Choi; Yoon Ah Kang; Mi Rim Lee; Hye Ran Jung
- Web page: https://patentgrep.com/patent/US20140154578A1

## CPC

- H01M 4/366: {as layered products}
- H01M 4/0402: {Methods of deposition of the material}
- H01M 4/0428: {Chemical vapour deposition}
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided are an anode active material including a porous silicon oxide-carbon material composite which includes a porous silicon oxide including pores and a line-type carbon material coated on a surface, in the pores, or on the surface and in the pores of the porous silicon oxide, and a method of preparing the anode active material. Since the silicon oxide of the anode active material according to an embodiment of the present invention may include the plurality of pores, resistance to the mechanical stress due to a volume change may be improved. Also, since the line-type carbon material is bonded to the inside of the pores, conductivity may not be decreased even in the case in which internal cracks occur in the porous silicon oxide and lifetime characteristics may be improved.

## Claims

### Claim 1

An anode active material comprising a porous silicon oxide-carbon material composite, the porous silicon oxide-carbon material composite comprising:
a porous silicon oxide including pores; and
a line-type carbon material coated on a surface, in the pores, or on the surface and in the pores of the porous silicon oxide.

### Claim 2 (depends on 1)

The anode active material of claim 1, wherein the line-type carbon material is included in a direction perpendicular to a tangent line to the surface, an inside of the pores, or the surface and the inside of the pores of the porous silicon oxide.

### Claim 3 (depends on 1)

The anode active material of claim 1, wherein the line-type carbon material is formed both on the surface and in the pores of the porous silicon oxide.

### Claim 4 (depends on 1)

The anode active material of claim 1, wherein the porous silicon oxide comprises SiOx, where 0<x<2.

### Claim 5 (depends on 1)

The anode active material of claim 1, wherein a Brunauer-Emmett-Teller (BET) specific surface area of the porous silicon oxide is in a range of 10 m2/g to 100 m2/g.

### Claim 6 (depends on 1)

The anode active material of claim 1, wherein an average diameter of the pores of the porous silicon oxide is in a range of 10 nm to 1,000 nm when the average diameter is measured on the surface of the porous silicon oxide.

### Claim 7 (depends on 1)

The anode active material of claim 1, wherein the line-type carbon material is carbon nanofibers, carbon nanotubes, or a mixture thereof.

### Claim 8 (depends on 7)

The anode active material of claim 7, wherein an average diameter of the line-type carbon material is in a range of 1 nm to 200 nm, and an average length thereof is in a range of 100 nm to 5 μm.

### Claim 9 (depends on 1)

The anode active material of claim 1, wherein the line-type carbon material is included in an amount ranging from 1 wt % to 10 wt % based on 100 wt % of the porous silicon oxide-carbon material composite.

### Claim 10 (depends on 1)

The anode active material of claim 1, wherein the anode active material further comprises a graphite-based material.

### Claim 11 (depends on 10)

The anode active material of claim 10, wherein the graphite-based material comprises one or more selected from the group consisting of natural graphite, artificial graphite, and mesocarbon microbeads (MCMB).

### Claim 12

A method of preparing an anode active material, the method comprising:
bonding a metal catalyst to a surface, an inside of pores, or the surface and the inside of the pores of a porous silicon oxide; and
forming a line-type carbon material on the metal catalyst.

### Claim 13 (depends on 12)

The method of claim 12, wherein the porous silicon oxide comprises SiOx, where 0<x<2.

### Claim 14 (depends on 12)

The method of claim 12, wherein the metal catalyst comprises one or more selected from the group consisting of chromium (Cr), manganese (Mn), iron (Fe), cobalt (Co), nickel (Ni), copper (Cu), zinc (Zn), molybdenum (Mo), indium (In), tin (Sn), aluminum (Al), and platinum (Pt).

### Claim 15 (depends on 12)

The method of claim 12, wherein the bonding of the metal catalyst to the surface, the inside of the pores, or the surface and the inside of the pores of the porous silicon oxide is performed by a sputtering method, a vacuum deposition method, a chemical vapor deposition (CVD) method, a plating method, or a method of dipping the silicon oxide in a solution of a metal catalyst compound.

### Claim 16 (depends on 12)

The method of claim 12, wherein the forming of the line-type carbon material is performed by a CVD method.

### Claim 17 (depends on 1)

An anode comprising the anode active material of claim 1.

### Claim 18 (depends on 17)

A lithium secondary battery comprising the anode of claim 17.