# US 2014/0154127 A1 · Alloy and Sputtering Target Material for Soft-Magnetic Film Layer in Perpendicular Magnetic Recording Medium, and Method for Producing the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0154127 A1
- Document ID: US20140154127A1
- Status: Published application
- Kind: A1
- Application number: 14/175,409
- Filed: 2014-02-07
- Published: 2014-06-05
- Earliest claimed: 2007-09-18
- Assignees: Sanyo Special Steel Co., Ltd.
- Applicants: Sanyo Special Steel Co., Ltd.
- Inventors: Toshiyuki Sawada; Akihiko Yanagitani
- Web page: https://patentgrep.com/patent/US20140154127A1

## CPC

- C23C 14/3414: {Metallurgical or chemical aspects of target preparation, e.g. casting, powder metallurgy}
- C22C 33/0257: {characterised by the range of the alloying elements}
- H01F 41/183: {Sputtering targets therefor}
- B22F 2998/10: Processes characterised by the sequence of their steps
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER

## Abstract

There are provided a sputtering target material for a soft-magnetic film layer with a high saturation magnetic flux density and high amorphous properties and a method for producing the sputtering target material. The target material is made of an alloy comprising one or more of Zr, Hf, Nb, Ta and B in an amount satisfying 5 at %≦(Zr+Hf+Nb+Ta)+B/2≦10 at % and having 7 at % or less of B; 0 to 5 at % in total of Al and Cr; and the balance being Co and Fe in an amount satisfying 0.20≦Fe/(Fe+Co)≦0.65 (at % ratio) with unavoidable impurities.

## Claims

### Claim 1

A method for producing a sputtering target material, comprising the steps of:
a) mixing a first powder and a second powder to form a mixed powder,
wherein the first powder comprises:
one or more of Zr, Hf, Nb, Ta and B in an amount satisfying 3 at %≦(Zr+Hf+Nb+Ta)+B/2≦12 at %;
Al and Cr: 0 to 5 at % in total; and
the balance being Co and Fe in an amount of satisfying 1.00≧Fe/(Fe+Co)≧0.90 (at % ratio) with unavoidable impurities, and
wherein the second powder comprises:
one or more of Zr, Hf, Nb, Ta and B having an amount of satisfying 3 at %≦(Zr+Hf+Nb+Ta)+B/2≦12 at %;
Al and Cr: 0 to 5 at % in total; and
the balance being Co and Fe in an amount satisfying 0.00≦Fe/(Fe+Co)≦0.10 (at % ratio) with unavoidable impurities; and
b) consolidating the mixed powder at 800 to 1250° C. and at 100 to 1000 MPa to form the sputtering target material,
wherein the sputtering target material comprises:
one or more of Zr, Hf, Nb, Ta and B in an amount satisfying 5 at %≦(Zr+Hf+Nb+Ta)+B/2≦10 at % and having 7 at % or less of B;
Al and Cr: 0 to 5 at % in total; and
the balance being Co and Fe in an amount satisfying 0.20≦Fe/(Fe+Co)≦0.65 (at % ratio) with unavoidable impurities.

### Claim 2 (depends on 1)

The method according to claim 1, wherein only the first powder or both of the first powder and the second powder comprise 5 at % or less of Al+Cr, and wherein the target material comprises 5 at % or less of Al+Cr as a whole.

### Claim 3 (depends on 1)

The method according to claim 1, wherein a difference between a PTF value of the target material and a PFT value of a target material produced by the same method as the method according to claim 1 except for using a single powder of the same composition as a final composition of the target material in place of the mixed powder ranges from 5 to 15.

### Claim 4 (depends on 2)

The method according to claim 2, wherein a difference between a PTF value of the target material and a PFT value of a target material produced by the same method as the method according to claim 2 except for using a single powder of the same composition as a final composition of the target material in place of the mixed powder ranges from 5 to 15.