# US 2014/0150963 A1 · Halogen-free resin composition and method for preparation of copper clad laminate with same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2014/0150963 A1
- Document ID: US20140150963A1
- Status: Published application
- Kind: A1
- Application number: 14/239,045
- Filed: 2011-09-02
- Published: 2014-06-05
- Earliest claimed: 2011-09-02
- Assignees: Shengyi Technology Co., Ltd.
- Inventors: Yueshan He
- Web page: https://patentgrep.com/patent/US20140150963A1

## CPC

- C09D 163/10: Epoxy resins modified by unsaturated compounds
- B32B 15/08: of synthetic resin
- B32B 15/14: next to a fibrous or filamentary layer
- B32B 15/20: comprising aluminium or copper {(B32B15/016 and B32B15/017 take precedence)}
- B32B 37/10: characterised by the pressing technique, e.g. using action of vacuum or fluid pressure
- B32B 38/08: Impregnating
- C08K 5/0025: {Crosslinking or vulcanising agents; including accelerators}
- C08K 5/5399: Phosphorus bound to nitrogen
- C09D 143/02: Homopolymers or copolymers of monomers containing phosphorus
- C09D 145/00: Coating compositions based on homopolymers or copolymers of compounds having no unsaturated aliphatic radicals in a side chain, and having one or more carbon-to-carbon double bonds in a carbocyclic or in a heterocyclic system; Coating compositions based on derivatives of such polymers (based on polymers of cyclic esters of polyfunctional acids C09D131/00; based on polymers of cyclic anhydrides or imides C09D135/00)
- C09D 171/12: Polyphenylene oxides
- H05K 1/0346: {containing N}
- B32B 2260/023: Two or more layers
- B32B 2260/046: Synthetic resin
- B32B 2262/101: Glass fibres
- B32B 2305/076: Prepregs
- C08K 3/013: Fillers, pigments or reinforcing additives
- H05K 1/0373: {containing additives, e.g. fillers (H05K1/036 takes precedence)}
- H05K 3/022: {Processes for manufacturing precursors of printed circuits, i.e. copper-clad substrates}
- H05K 2201/012: Flame-retardant; Preventing of inflammation
- H05K 2201/0209: Inorganic, non-metallic particles
- Y10T 156/1075: of plural laminae from single stock and assembling to each other or to additional lamina
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A halogen-free resin composition and a method for preparation of copper clad laminate with the same, wherein based on total parts by weight of solid components, the halogen-free resin composition comprises a reactive allyl phenoxy cyclotriphosphazene or vinyl phenoxy cyclotriphosphazene of 5-50 parts, a thermosetting resin of 15-85 parts, a crosslinking curing agent of 1-35 parts, a crosslinking curing accelerant of 0-5 parts and a filler of 0-100 parts. In the present invention, the reactive allyl phenoxy cyclotriphosphazene or vinyl phenoxy cyclotriphosphazene having very low water absorption is introduced into the thermosetting resin, satisfying both the halogen-free and antiflaming requirements and improving the electrical properties of the system, and making it possible to prepare the halogen-free high-frequency high-speed substrate material. The resulted copper clad laminate satisfies the halogen-free requirement, and has advantages such as excellent resistance to heat and moisture, and low dielectric loss.

## Claims

### Claim 1

A halogen-free resin composition, comprising, based on the total weight parts of the solid components,
from 5 to 50 parts by weight of reactive allylphenoxylcyclo-triphosphazene or vinylcyclotriphosphazene;
from 15 to 85 parts by weight of a thermosetting resin;
from 1 to 35 parts by weight of a crosslinking curing agent;
from 0 to 5 parts by weight of a crosslinking curing accelerator; and
from 0 to 100 parts by weight of a packing.

### Claim 2 (depends on 1)

The halogen-free resin composition according to claim 1, wherein said reactive allylphenoxylcyclotriphosphazene or vinylcyclotriphosphazene has the following structural formula (I)
wherein m represents an integer of 3-25; X is phenoxyl
in an amount of 0-2m-1: Y is selected from the group consisting of p-allylphenoxyl
m-allylpheno
o-allyl-phenoxyl
p-vinylphenoxyl
and m-vinylphenoxyl
in an amount of 1-2m; X+Y=2m.

### Claim 3 (depends on 1)

The halogen-free resin composition according to claim 1, wherein said thermosetting resin comprises one or more of the following resins
epoxy resins, including bisphenol A epoxy resin, bisphenol F epoxy resin, dicyclopentadiene epoxy resin, triphenolic epoxy resin, biphenyl-type epoxy resin, naphthol epoxy resin, and phosphorous-containing epoxy resin;
benzoxazine resin, including bisphenol A-type benzoxazine resin, bisphenol F-type benzoxazine resin, dicyclopentadiene-type benzoxazine resin and phenolphthalein-type benzoxazine resin;
cyanate resin, including bisphenol A-type cyanate resin, dicyclopentadiene-type cyanate resin and phenolic aldehyde-type cyanate resin;
bismaleimide resin, including 4,4′-diphenylmothane bismaleimide resin, allyl-modified diphenylmothane bismaleimide resin;
reactive polyphenylene oxide resin, having a number average molecular weight of 1000-7000, wherein the reactive groups is hydroxyl or double bond; and
C5 hydrocarbon resin consisting of vinylbutylbenzene resin having a m molecular weight of 11000, vinylpolybutadiene resin with polar groups and a copolymer in which butadiene is grafted to styrene with maleic anhydride.

### Claim 4 (depends on 1)

The halogen-free resin composition according to claim 1, wherein said crosslinking curing agent is selected from the group consisting of dicyandiamide, aromatic amine, anhydride, phenols, fulminuric triene ester and phosphorous-containing phenolic aldehyde, or combinations thereof.

### Claim 5 (depends on 1)

The halogen-free resin composition according to claim 1, wherein said crosslinking curing accelerator is selected from the group consisting of 2-methylimidazole, 2-ethyl-4-methylimidazole, 2-phenylimidazole, tri-(dimethylaminomethyl), hexamethylene tetramine, dicumyl peroxide, tert-butyl peroxybenzoate, 2,5-di(2-ethylcaproyl peroxy)-2,5-dimethylhexane, acetopyruvic salts, and caprilate, or combinations thereof.

### Claim 6 (depends on 1)

The halogen-free resin composition according to claim 1, wherein said packing is one or more selected from the group consisting of aluminium hydroxide, magnesium hydroxide, zeolite, wollastonite, silicon dioxide, magnesia, calcium silicate, calcium carbonate, clay, talc and mica.

### Claim 7 (depends on 1)

A method for preparing a copper clad laminate with he halogen-free resin composition according to claim 1, comprising
Step 1: dissolving from 5 to 50 parts by weight of reactive allylphenoxycyclotriphosphazene or vinylphenoxycyclotriphosphazene in a solvent until complete dissolution at room temperature or moderate temperature;
Step 2: adding from 15 to 85 parts by weight of the corresponding thermosetting resin, form 1 to 35 parts by weight of a crosslinking curing agent, from 0 to 5 parts by weight of a crosslinking curing accelerator and from 0 to 100 parts by weight of a packing into said solution, homogeneously stirring to obtain a liquid cement;
Step 3: homogeneously coating with said liquid cement E-glass cloth having a flattening surface, and then baking to a B-stage prepreg;
Step 4: cutting the B-stage prepreg to a suitable size according to the press size, stacking several prepregs regularly, a copper foil being placed over and under the prepregs, pressing in a vacuum hot press to obtain a copper clad laminate.

### Claim 8 (depends on 7)

The method for preparing a copper clad laminate according to claim 7, wherein the solvent is one or more selected from benzene and ketone solvents; said moderate temperature is ≦80° C.

### Claim 9 (depends on 7)

The method for preparing a copper clad laminate according to claim 7, wherein, during the step 3 of baking the B-stage prepreg, the temperature is set up according to the boiling point of the solvent used therein, and ranges from 85 to 175° C., and the baking lasts 5-20 min.

### Claim 10 (depends on 7)

The method for preparing a copper clad laminate according to claim 7, wherein, in step 4, the pressing process is carried out by the bench pressing method, comprising the specific steps of increasing from room temperature to 150° C. within 15 min and remaining for 30 min, then increasing to 180° C. within 5 min and remaining for 2 h, finally decreasing to room temperature within 30 min; increasing the pressure from 0 to 0.6 Mpa within 1 min and remaining for 20 min, then increasing the pressure 1.0 Mpa within 1 min and remaining for 2.5 h and post-processing at 200-245° C. and remaining for 1-5 h.