- Inventors: You-Hwan Lee; Dong-Hyun Kim; Geun-Soo Ryu
- Web page: https://patentgrep.com/patent/US20140150934A1

## CPC

- C21D 9/0093: {for screws; for bolts}
- C21D 8/06: during manufacturing of rods or wires
- C21D 9/525: {for wire, for rods (C21D9/54 takes precedence)}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present invention relates to a wire rod used in bolts for automobile engines, for example, and more specifically to a wire rod having an improved resistance to hydrogen delayed fracture, to a manufacturing method for same, to a bolt using same and a method for manufacturing the bolt. Provided are a high strength wire rod having a superior resistance to hydrogen delayed fracture and a method for manufacturing same, a high strength bolt using the wire rod and a method for manufacturing same, wherein. the wire rod comprises, 0.3-0.7 wt % C, 0.05-2.0 wt % Si, 0.7-1.5 wt % Mn, 0.01-0.1 wt % Ni, and 30-70 ppm La, and the remainder thereof is comprised by Fe and inevitable impurities.

## Claims

### Claim 1

A wire rod having superior hydrogen delayed fracture resistance and comprising C: 0.3 to 0.7 wt %, Si: 0.05 to 2.0 wt %, Mn: 0.7 to 1.5 wt %, La: 30 to 70 ppm, Ni: 0.01 to 0.1 %, and a remainder configured of Fe and inevitable impurities.

### Claim 2 (depends on 1)

The wire rod of claim 1, wherein the wire rod includes a lanthanum (La)-based, a nickel (Ni)-based, or a LaNi-based precipitate.

### Claim 3 (depends on 2)

The wire rod of claim 2, wherein an aspect ratio of the precipitate is 1.2 to 2.0.

### Claim 4 (depends on 2)

The wire rod of claim 2, wherein an average circular-equivalent diameter of the precipitate is 100 to 400 nm.

### Claim 5 (depends on 2)

The wire rod of claim 2, wherein the precipitate is at least one of LaNi5, LaPO4 and La2O2S.

### Claim 6

A method for manufacturing a wire rod having superior hydrogen delayed fracture resistance, the method comprising:
heating steel including C: 0.3 to 0.7 wt %, Si: 0.05 to 2.0 wt %, Mn: 0.7 to 1.5 wt %, La: 30 to 70 ppm, Ni: 0.01 to 0.1%, and a remainder configured of Fe and inevitable impurities to a temperature of Ae3+150° C. to Ae3+250° C.;
cooling the heated steel at a rate of 5 to 15° C./s and rolling, the steel at a temperature of Ae3+50° C. to Ae3+150° C. to manufacture a wire rod; and
cooling the rolled wire rod to 600° C. or less at a rate of 0.5 to 3° C./s.

### Claim 7 (depends on 6)

The method of claim 6, wherein the heating is performed for 30 minutes to one and a half hours,

### Claim 8

A bolt comprising C: 0.3 to 0.7 wt %, Si: 0.05 to 2.0 wt %, Mn: 0.7 to 1.5 wt %, La: 30 to 70 ppm, Ni: 0.01 to 0.1%, and a remainder configured of Fe and inevitable impurities, and having a tensile strength of 1200 MPa or greater and superior hydrogen delayed fracture resistance.

### Claim 9 (depends on 8)

The bolt of claim 8, wherein a microstructure of the bolt includes a lanthanum (La)-based, a nickel (Ni)-based, or a LaNi-based precipitate having an aspect ratio of 1.2 to 2.0.

### Claim 10 (depends on 9)

The bolt of claim 9, wherein the aspect ratio of the precipitate is 1.2 to 2.0.

### Claim 11 (depends on 9)

The bolt of claim 9, wherein an average circular-equivalent diameter of the precipitate is 100 to 400nm,

### Claim 12 (depends on 9)

The bolt of claim 9, wherein the precipitate is at least one of LaNi5, LaPO4 and La2O2S.

### Claim 13

A method for manufacturing a bolt having superior hydrogen delayed fracture resistance, the method comprising:
heating steel including C: 0.3 to 0.7 wt %, Si: 0.05 to 2.0 wt %, Mn: 0.7 to 1.5 wt %, La: 30 to 70 ppm, Ni: 0.01 to 0.1%, and a remainder configured of Fe and inevitable impurities to a temperature of Ae3+150° C. to Ae3+250° C.;
cooling the heated steel at a rate of 5 to 15° C./s and rolling the steel at a temperature of Ae3+50° C. to Ae3+150° C. to manufacture a wire rod;
cooling the rolled wire rod to 600 ° C. or less at a rate of 0.5 to 3° C./s; and
bolt-forming using the cooled wire rod;
performing a heat treatment on the formed bolt at a temperature of 850 to 950° C.; and
performing quenching after the heat treatment, and then performing tempering at a temperature of 300 to 500° C.

### Claim 14 (depends on 13)

The method of claim 13, wherein the heating is performed for 30 minutes to one and a half hours.