# US 2013/0337631 A1 · Semiconductor Structure and Method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0337631 A1
- Document ID: US20130337631A1
- Status: Published application
- Kind: A1
- Application number: 13/525,041
- Filed: 2012-06-15
- Published: 2013-12-19
- Earliest claimed: 2012-06-15
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Sen-Hong Syue; Pu-Fang Chen; Shiang-Bau Wang
- Web page: https://patentgrep.com/patent/US20130337631A1

## CPC

- C30B 15/04: adding doping materials, e.g. for n-p-junction
- C30B 15/203: {the relationship of pull rate (v) to axial thermal gradient (G)}
- C30B 15/206: {the thermal history of growing the ingot}
- C30B 15/22: Stabilisation or shape controlling of the molten zone near the pulled crystal; Controlling the section of the crystal
- C30B 29/06: Silicon
- C30B 31/02: by contacting with diffusion materials in the solid state
- C30B 31/04: by contacting with diffusion materials in the liquid state
- C30B 31/165: {Diffusion sources}
- H10D 62/605: {Planar doped, e.g. atomic-plane doped or delta-doped}
- H10P 36/20: Intrinsic gettering, i.e. thermally inducing defects by using oxygen present in the silicon body
- H10P 50/28: of insulating materials
- H10P 90/12: {Preparing bulk and homogeneous wafers}
- H10P 95/062: {involving a dielectric removal step}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- C30B 15/00: Single-crystal growth by pulling from a melt, e.g. Czochralski method (under a protective fluid C30B27/00)
- C30B 33/00: After-treatment of single crystals or homogeneous polycrystalline material with defined structure (C30B31/00 takes precedence)
- H10D 30/60: Insulated-gate field-effect transistors [IGFET] (H10D30/40 takes precedence)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A system and method for providing support to semiconductor wafer is provided. An embodiment comprises introducing a vacancy enhancing material during the formation of a semiconductor ingot prior to the semiconductor wafer being separated from the semiconductor ingot. The vacancy enhancing material forms vacancies at a high density within the semiconductor ingot, and the vacancies form bulk micro defects within the semiconductor wafer during high temperature processes such as annealing. These bulk micro defects help to provide support and strengthen the semiconductor wafer during subsequent processing and helps to reduce or eliminate a fingerprint overlay that may otherwise occur.

## Claims

### Claim 1

A method for manufacturing a semiconductor device, the method comprising:
combining a semiconductor raw material and a vacancy enhancing raw material to form a combined raw material mixture; and
crystallizing the raw material mixture into a semiconductor ingot with a vacancy concentration of greater than about 1×1010 #/cm3.

### Claim 2 (depends on 1)

The method of claim 1, wherein the combining the semiconductor raw material and the vacancy enhancing raw material further comprises melting the semiconductor raw material into a semiconductor melt.

### Claim 3 (depends on 1)

The method of claim 1, wherein the vacancy enhancing raw material is a nitride.

### Claim 4 (depends on 1)

The method of claim 1, further comprising separating one or more semiconductor wafers from the semiconductor ingot.

### Claim 5 (depends on 4)

The method of claim 4, further comprising forming isolation regions within one of the one or more semiconductor wafers.

### Claim 6 (depends on 5)

The method of claim 5, wherein the forming isolation regions further comprises:
depositing a dielectric material within a trench in the one of the one or more semiconductor wafers; and
annealing the dielectric material, wherein the annealing the dielectric material generates bulk micro defects within the one of the one or more semiconductor wafers.

### Claim 7 (depends on 6)

The method of claim 6, wherein the bulk micro defects have a concentration of greater than about 1E9 #/cm3.

### Claim 8

A method of manufacturing a semiconductor device, the method comprising:
providing a semiconductor raw material;
introducing a vacancy enhancing raw material into the semiconductor raw material;
crystallizing the semiconductor raw material and the vacancy enhancing material into a semiconductor ingot, wherein the semiconductor ingot comprises a first set of vacancies and has an interstitial oxygen concentration greater than 7×1017 atoms/cm3;
separating a semiconductor wafer from the semiconductor ingot, the semiconductor wafer comprising the first set of vacancies; and
transforming the first set of vacancies into bulk micro defects using at least in part a thermal process.

### Claim 9 (depends on 8)

The method of claim 8, wherein the introducing the vacancy enhancing raw material introduces a concentration of vacancy enhancing raw material within the semiconductor raw material of between about 1E10 atom/cm3 and about 1E19 atoms/cm3.

### Claim 10 (depends on 8)

The method of claim 8, wherein the crystallizing the semiconductor raw material and the vacancy enhancing material further comprises performing a Czochralski process.

### Claim 11 (depends on 8)

The method of claim 8, further comprising:
forming a trench into the semiconductor wafer; and
filling the trench with a dielectric material; and
annealing the dielectric material and the semiconductor wafer, wherein the thermal process is at least in part the annealing the dielectric material and the semiconductor wafer.

### Claim 12 (depends on 11)

The method of claim 11, further comprising:
planarizing the dielectric material; and
annealing the dielectric material and the semiconductor wafer after the transforming the first set of vacancies.

### Claim 13 (depends on 8)

The method of claim 8, wherein the vacancy enhancing raw material is a nitride.

### Claim 14

(canceled)

### Claim 15

A method of manufacturing a semiconductor device, the method comprising:
placing a semiconductor raw material into a crucible;
introducing nitrogen into the crucible;
mixing the semiconductor raw material and the nitrogen to form a semiconductor melt; and
pulling a semiconductor ingot from the semiconductor melt, the semiconductor ingot comprising the nitrogen and having an interstitial oxygen concentration greater than 7×1017 atoms/cm3.

### Claim 16 (depends on 15)

The method of claim 15, wherein the introducing nitrogen further comprises placing silicon nitride into the crucible.

### Claim 17 (depends on 15)

The method of claim 15, further comprising separating the semiconductor ingot into semiconductor wafers.

### Claim 18 (depends on 17)

The method of claim 17, further comprising annealing at least one of the semiconductor wafers to generate bulk micro defects in the at least one of the semiconductor wafers.

### Claim 19 (depends on 18)

The method of claim 18, further comprising forming a dielectric material over the at least one of the semiconductor wafers, wherein the annealing the at least one of the semiconductor wafers also anneals the dielectric material.

### Claim 20 (depends on 15)

The method of claim 15, wherein the introducing the semiconductor melt has a concentration of the nitrogen of between about 1E10 atom/cm3 and about 1E19 atoms/cm3.