# US 2013/0323414 A1 · Accelerated aging of phosphorus-doped optical fibers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0323414 A1
- Document ID: US20130323414A1
- Status: Published application
- Kind: A1
- Application number: 13/898,749
- Filed: 2013-05-21
- Published: 2013-12-05
- Earliest claimed: 2008-02-26
- Assignees: OFS Fitel, LLC
- Applicants: Ofs Fitel, LLC
- Inventors: David John DiGiovanni; Robert L. Lingle; Michael J. LuValle; George E. Oulundsen; Durgesh Vaidya
- Web page: https://patentgrep.com/patent/US20130323414A1

## CPC

- G02B 6/02: Optical fibres with cladding {with or without a coating}
- C03B 37/15: with heat application, e.g. for making optical fibres (fusion-splicing of light guides G02B6/255; treatment of light guides to shape optical elements {G02B6/2835, G02B6/2856})
- C03C 13/047: {containing deuterium}
- C03C 25/607: in the gaseous phase
- C03C 25/62: by application of electric or wave energy (for drying or dehydration C03C25/64); by particle radiation or ion implantation
- C03C 25/6286: Ion implantation
- C03B 2201/28: doped with phosphorus
- C03B 2201/31: doped with germanium
- G02B 6/0288: {Multimode fibre, e.g. graded index core for compensating modal dispersion}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Adverse hydrogen aging limitations in multiply-doped optical fibers are overcome by passivating these optical fibers using a deuterium passivation process. This treatment essentially pre-reacts the glass with deuterium so that the most active glass sites are no longer available to react with hydrogen in service. Optical fibers of main interest are doped with mixtures of germanium and phosphorus. Optimum passivating process conditions are described.

## Claims

### Claim 1

A method for passivation of optical fibers, the method comprising:
applying a first passivation step to an optical fiber, the first passivation step being in an environment comprising deuterium, the first passivation step being at a first pressure, the first passivation step being at a first temperature, the first passivation step being for a first period of time;
applying a first operation step to the optical fiber, the first operation step being in an atmosphere comprising hydrogen, the first operation step being at a second pressure, the first operation step being at a second temperature, the first operation step being for a second period of time, the first passivation step and the first operation step resulting in a first loss-time curve, the first loss-time curve having a first loss associated with the first loss-time curve;
applying a second passivation step to the optical fiber, the second passivation step being in the environment comprising deuterium, the second passivation step being at a third pressure, the second passivation step being at a third temperature, the third temperature being greater than the first temperature, the second passivation step being for a third period of time, the second passivation step resulting in a second loss-time curve, the second loss-time curve having a second loss associated with the second loss-time curve, the second passivation step being such that the first loss is less than the second loss; and
applying a second operation step to the optical fiber, the second operation step being in the atmosphere comprising hydrogen, the second operation step being at a fourth pressure, the second operation step being at a fourth temperature, the second operation step being applied for a fourth period of time.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
comparing the first loss-time curve to a third loss-time curve, the third loss-time curve having a third loss associated with the third loss-time curve, the third loss-time curve being derived from applying a third passivation step to the optical fiber, the third passivation step being in the environment comprising deuterium, the third passivation step being at a fifth pressure, the third passivation step being at a fifth temperature, the third passivation step being for a fifth period of time, the fifth temperature being less than the first temperature; and
applying a third operation step to the optical fiber, the third operation step being in the atmosphere comprising hydrogen, the third operation step being at a sixth pressure, the third operation step being at a sixth temperature, the third operation step being such that the first loss is less than the third loss.

### Claim 3 (depends on 1)

The method of claim 1, the first temperature being between approximately 65 degrees Celsius and approximately 100 degrees Celsius.

### Claim 4 (depends on 1)

The method of claim 1, the first pressure being between approximately 0.2 atmospheres and approximately 0.6 atmospheres of deuterium.

### Claim 5 (depends on 1)

The method of claim 1, the first time being between approximately 2 hours and approximately 4 hours.

### Claim 6 (depends on 1)

The method of claim 1, the first passivation step being followed by heating the optical fiber in an inert atmosphere, the second passivation step being followed by heating the optical fiber in the inert atmosphere.

### Claim 7 (depends on 6)

The method of claim 6, the heating of the optical fiber in the inert atmosphere occurring at a temperature between approximately 82 degrees Celsius and approximately 92 degrees Celsius.

### Claim 8 (depends on 6)

The method of claim 6, the heating of the optical fiber in the inert atmosphere occurring for approximately 16 hours to approximately 26 hours.

### Claim 9 (depends on 1)

The method of claim 1, the environment comprising deuterium further comprising nitrogen.

### Claim 10 (depends on 1)

The method of claim 1, the second loss-time curve not intersecting the first loss-time curve.

### Claim 11 (depends on 2)

The method of claim 2, third loss-time curve intersecting the first loss-time curve during the first operation step.

### Claim 12 (depends on 11)

The method of claim 11, the third loss-time curve not intersecting the first loss-time curve during the first passivation step.

### Claim 13

A method for passivation of optical fibers, the method comprising:
applying a first passivation step to an optical fiber, the first passivation step being in an environment comprising deuterium, the first passivation step being at a first pressure, the first passivation step being at a first temperature, the first temperature being between approximately 65 degrees Celsius and approximately 100 degrees Celsius, the first passivation step being for a first period of time;
heating the optical fiber in an environment comprising an inert gas;
applying a first operation step to the optical fiber, the first operation step being in an atmosphere comprising hydrogen, the first operation step being at a second pressure, the first operation step being at a second temperature, the first operation step being for a second period of time, the first passivation step and the first operation step resulting in a first loss-time curve, the first loss-time curve having a first loss associated with the first loss-time curve;
applying a second passivation step to the optical fiber, the second passivation step being in the environment comprising deuterium, the second passivation step being at a third pressure, the second passivation step being at a third temperature, the third temperature being greater than the first temperature, the second passivation step being for a third period of time, the second passivation step resulting in a second loss-time curve, the second loss-time curve having a second loss associated with the second loss-time curve;
applying a second operation step to the optical fiber, the second operation step being in the atmosphere comprising hydrogen, the second operation step being at a fourth pressure, the second operation step being at a fourth temperature, the second operation step being for a fourth period of time, the second operation step being such that the first loss is less than the second loss.

### Claim 14 (depends on 13)

The method of claim 13, the second loss-time curve not intersecting the first loss-time curve.

### Claim 15 (depends on 14)

The method of claim 14, the third loss-time curve intersecting the first loss-time curve during the first operation step.

### Claim 16

A method for passivation of optical fibers, the method comprising:
applying a first passivation step to the optical fiber, the first passivation step being in an environment comprising deuterium, the first passivation step being at a first pressure, the first pressure being between approximately 0.2 atmospheres of deuterium and approximately 0.6 atmospheres of deuterium, the first passivation step being at a first temperature, the first temperature being between approximately 65 degrees Celsius and approximately 100 degrees Celsius, the first passivation step being for a first period of time;
heating the optical fiber in an environment comprising an inert gas;
applying a first operation step to the optical fiber, the first operation step being in an atmosphere comprising hydrogen, the first operation step being at a second pressure, the first operation step being at a second temperature, the first operation step being for a second period of time, the first passivation step and the first operation step resulting in a first loss-time curve, the first loss-time curve having a first loss associated with the first loss-time curve;
applying a second passivation step to the optical fiber, the second passivation step being in the environment comprising deuterium, the second passivation step being at a third pressure, the second passivation step being at a third temperature, the third temperature being greater than the first temperature, the second passivation step being for a third period of time, the second passivation step resulting in a second loss-time curve, the second loss-time curve having a second loss associated with the second loss-time curve;
applying a second operation step to the optical fiber, the second operation step being in the atmosphere comprising hydrogen, the second operation step being at a fourth pressure, the second operation step being at a fourth temperature, the second operation step being for a fourth period of time, the second operation step being such that the first loss is less than the second loss;
comparing the first loss-time curve to a third loss-time curve, the third loss-time curve having a third loss associated with the third loss-time curve, the third loss-time curve being derived from applying a third passivation step to the optical fiber, the third passivation step being in the environment comprising deuterium, the third passivation step being at a fifth pressure, the third passivation step being at a fifth temperature, the third passivation step being for a fifth period of time, the fifth temperature being less than the first temperature; and
applying a third operation step to the optical fiber, the third operation step being in the atmosphere comprising hydrogen, the third operation step being at a sixth pressure, the third operation step being at a sixth temperature, the third operation step being such that the first loss is less than the third loss.

### Claim 17 (depends on 16)

The method of claim 16, the second loss-time curve not intersecting the first loss-time curve.

### Claim 18 (depends on 17)

The method of claim 17, the third loss-time curve intersecting the first loss-time curve during the first operation step.