# US 2013/0309598 A1 · Half-tone phase shift mask blank and method for manufacturing half-tone phase shift mask

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0309598 A1
- Document ID: US20130309598A1
- Status: Published application
- Kind: A1
- Application number: 13/892,496
- Filed: 2013-05-13
- Published: 2013-11-21
- Earliest claimed: 2012-05-16
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Applicants: Shin-Etsu Chemical Co., Ltd.
- Inventors: Souichi FUKAYA; Hideo Nakagawa; Kouhei Sasamoto
- Web page: https://patentgrep.com/patent/US20130309598A1

## CPC

- G03F 1/32: Attenuating PSM [att-PSM], e.g. halftone PSM or PSM having semi-transparent phase shift portion,; Preparation thereof
- G03F 1/29: Rim PSM or outrigger PSM; Preparation thereof
- G03F 1/54: Absorbers, e.g. of opaque materials
- G03F 1/80: Etching
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A half-tone phase shift film 2 and a light-shielding film 3 are stacked on transparent substrate 1. The light-shielding film 3 has a monolayer structure or a multilayer structure. At least one layer is formed by film-formation with a chromium-containing material including tin. The half-tone phase shift film 2 is made of a molybdenum silicon nitride oxide. The layer made of a chromium-containing material including tin can cause a significant increase in the etching rate at the time of chlorine-containing dry-etching including oxygen. Thus, burden on the resist pattern or hard mask pattern at the time of transferring a pattern on the light-shielding film is reduced, and therefore it is possible to carry out pattern transfer with high precision. The present invention provides a novel technique that can increase a dry-etching rate of a light-shielding film made of a chromium-containing material while assuring various characteristics required for the light-shielding film.

## Claims

### Claim 1

A half-tone phase shift mask blank, comprising:
a light-shielding film having a monolayer structure or a multilayer structure, wherein
the light-shielding film is provided on the half-tone phase shifting layer, and includes at least one of layers made of a chromium-containing material, and
the at least one of the layers made of a chromium-containing material is made of a chromium-containing material including tin.

### Claim 2 (depends on 1)

The half-tone phase shift mask blank according to claim 1, wherein
the chromium-containing material including tin has a content of tin of not under 0.01 times and not over 2 times than the content of chromium in atomic ratio.

### Claim 3 (depends on 1)

The half-tone phase shift mask blank according to claim 1, wherein
all the layers of the light-shielding film are made of a chromium-containing material.

### Claim 4 (depends on 1)

The half-tone phase shift mask blank according to claim 1, wherein
the chromium-containing material is any one of a chromium metal, chromium oxide, chromium nitride, chromium carbide, chromium oxide nitride, chromium oxide carbide, chromium nitride carbide, and chromium oxide nitride carbide; and
the chromium-containing material including tin is any one of a tin-chromium metal, tin-chromium oxide, tin-chromium nitride, tin-chromium carbide, tin-chromium oxide nitride, tin-chromium oxide carbide, tin-chromium nitride carbide, and tin-chromium oxide nitride carbide.

### Claim 5 (depends on 1)

The half-tone phase shift mask blank according to claim 1, wherein
the half-tone phase shifting layer is made of a material etchable with fluorine-containing dry etching.

### Claim 6 (depends on 5)

The half-tone phase shift mask blank according to claim 5, wherein
the material etchable with fluorine-containing dry etching is a silicon-containing material including a transition metal.

### Claim 7 (depends on 6)

The half-tone phase shift mask blank according to claim 6, wherein
the silicon-containing material contains molybdenum and silicon, and further contains at least one of nitrogen and oxygen as a light element.

### Claim 8 (depends on 1)

The half-tone phase shift mask blank according to claim 1, further comprising
a hard mask film on the light-shielding film, where the hard mask film has etching resistance to chlorine-containing dry-etching including oxygen.

### Claim 9 (depends on 8)

The half-tone phase shift mask blank according to claim 8, wherein
the hard mask film contains silicon and further contains at least one of nitrogen and oxygen as a light element.

### Claim 10 (depends on 1)

A method for manufacturing a half-tone phase shift mask using a blank according to claim 1, the method comprising the steps of:
subjecting the layer made of the chromium-containing material including tin to an etching process with chlorine-containing dry-etching including oxygen; and
subjecting the half-tone phase shifting layer to an etching process with fluorine-containing dry etching.