# US 2013/0296457 A1 · Method For Modifying Polymers Comprising Hydroxyl Groups

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0296457 A1
- Document ID: US20130296457A1
- Status: Published application
- Kind: A1
- Application number: 13/976,787
- Filed: 2011-12-08
- Published: 2013-11-07
- Earliest claimed: 2010-12-30
- Assignees: Clariant Finance (BVI) Limited
- Inventors: Matthias Krull; Roman Morschhaeuser; Hans Juergen Scholz
- Web page: https://patentgrep.com/patent/US20130296457A1

## CPC

- C08J 3/28: Treatment by wave energy or particle radiation
- C08F 8/14: Esterification
- C08F 8/34: Introducing sulfur atoms or sulfur-containing groups
- C08F 2810/20: leading to a crosslinking, either explicitly or inherently
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The invention relates to a method for reacting polymers (A) comprising hydroxyl groups and which have repetitive structural units of general formula (I), wherein D represents a direct bond between the polymer backbone and a hydroxyl group, a C1- to C6-alkene group, a C5- to C12-arylene group, an oxyalkylene group of formula —O—R2—, an ester group of formula —C(O)—O—R2— or an amide group of formula —C(O)—N(R8)R2—, R2 represents a C2- to C10-alkene group, R8 represents hydrogen or an optionally substituted C2- to C10-alkyl group and n represents a number between 3 and 5000, with carboxylic acids B1) of formula (II) or carboxylic acid esters B2) of formula (III) R1—COOH (II) R1—COOR7 (III), wherein R1 represents a hydrocarbon group having 2 to 50 C atoms, and R7 represents a C1C4-alkyl group, in which the polymers (A); comprising the hydroxyl groups are exposed to microwaves in the presence of carboxylic acids of formula (II) or carboxylic acid esters of formula (III) and in the presence of water. The reaction mixture is heated to temperatures over 100° C. by microwave rays.

## Claims

### Claim 1

A process for reacting a hydroxyl-bearing polymer A) having repeat structural units of the formula (I)
in which
D is a direct bond between polymer backbone and hydroxyl group, a C1- to C6-alkylene group, a C5- to C12-arylene group, an oxyalkylene group of the formula —O—R2—, an ester group of the formula —C(O)—O—R2— or an amide group of the formula —C(O)—N(R8)R2—,
R2 is a C2- to C10-alkylene radical,
R8 is hydrogen or a C2- to C10-alkyl radical which may bear substituents, and
n is a number between 3 and 5000,
with at least one carboxylic acid B1) of the formula (II) or carboxylic ester B2) of the formula (III)
R1—COOH (II)
R1—COOR7 (III)
in which
R1 is a hydrocarbyl radical having 2 to 50 carbon atoms, and
R7 is a C1-C4-alkyl radical,
by irradiating the hydroxyl-bearing polymer A) with microwaves in the presence of the carboxylic acid of the formula (II) or the carboxylic ester of the formula (III), and in the presence of water, wherein the reaction mixture is heated by the microwave irradiation to temperatures above 100° C.

### Claim 2 (depends on 1)

The process as claimed in claim 1, in which the hydroxyl-bearing polymer comprises, as well as the structural units of the formula (I), additional structural units derived from further ethylenically unsaturated monomers.

### Claim 3 (depends on 1)

The process as claimed in claim 1, in which the structural units of the formula (I) derive from vinyl alcohol.

### Claim 4 (depends on 1)

The process as claimed in claim 1, wherein the hydroxyl-bearing polymer also comprises, as well as the structural units of the formula (I), structural units derived from vinyl acetate.

### Claim 5 (depends on 1)

The process as claimed in claim 1, in which R1 is an alkyl radical.

### Claim 6 (depends on 1)

The process as claimed in claim 1, in which the carboxylic acid B1) or the carboxylic ester B2) is a mixture of at least one carboxylic acid and at least one dicarboxylic acid or a mixture of at least one carboxylic ester and at least one dicarboxylic ester.

### Claim 7 (depends on 1)

The process as claimed in claim 1, in which the reaction mixture used for conversion contains 5 to 98% by weight of water.

### Claim 8 (depends on 1)

The process as claimed in claim 1, in which the reaction mixture used for conversion contains 5 to 98% by weight of a mixture of water and one or more water-miscible organic solvents.

### Claim 9 (depends on 8)

The process as claimed in claim 8, in which the proportion of the water-miscible organic solvent in the solvent mixture is between 1 and 75% by weight.

### Claim 10 (depends on 1)

The process as claimed in claim 1, in which the reaction mixture is heated by means of microwave radiation to temperatures above 110° C.

### Claim 11 (depends on 1)

The process as claimed in claim 1, in which ester-bearing comonomer units of polymer A) are transesterified with carboxylic acids B1) or carboxylic esters B2).

### Claim 12 (depends on 1)

The process as claimed in claim 1, in which the microwave irradiation is effected in a flow tube made from microwave-transparent, high-melting material.

### Claim 13 (depends on 12)

The process as claimed in claim 12, in which the longitudinal axis of the reaction tube in the direction of propagation of the microwaves is within a monomode microwave applicator.

### Claim 14 (depends on 1)

The process as claimed in claim 1, in which the microwave applicator takes the form of a cavity resonator.