# US 2013/0296157 A1 · Glass composition having high thermal and chemical stability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0296157 A1
- Document ID: US20130296157A1
- Status: Published application
- Kind: A1
- Application number: 13/980,780
- Filed: 2012-01-25
- Published: 2013-11-07
- Earliest claimed: 2011-01-25
- Assignees: Corning Incorporated
- Inventors: Adam J. Ellison; Timothy J. Kiczenski
- Web page: https://patentgrep.com/patent/US20130296157A1

## CPC

- C03C 3/118: containing aluminium
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/091: containing aluminium
- C03C 3/093: containing zinc or zirconium
- C03C 3/11: containing halogen or nitrogen
- C03C 3/112: containing fluorine
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Described herein are alkali-free, boroalumino silicate glasses exhibiting desirable physical and chemical properties for use as substrates in flat panel display devices, such as, active matrix liquid crystal displays (AMLCDs) and active matrix organic light emitting diode displays (AMOLEDs). In accordance with certain of its aspects, the glasses possess good dimensional stability as a function of temperature. The glasses comprise in mol percent on an oxide basis: 70-74.5 SiO2, 10.5-13.5 AL2O3, 0-2.5 B2O3, 3-7 MgO, 3-7 CaO, 0-4 SrO, 1.5-6 BaO, 0-0.3 SnO2, 0-03 CeO2, 0-0.5 As2O3, 0-0.5 Sb2O3, 0.01-0.08 Fe2O3 and F+Cl+BrRO/Al2O31.7 and 0.2MgO/RO0.45, RO being the sum of MgO, BaO, SrO and CaO.

## Claims

### Claim 1

A glass comprising in mol percent on an oxide basis:
70≦SiO2≦74.5
10.5≦Al2O3≦13.5
0≦B2O3≦2.5
3≦MgO≦7
3≦CaO≦7
0≦SrO≦4
1.5≦BaO≦6
0≦SnO2≦0.3
0≦CeO2≦0.3
0≦As2O3≦0.5
0≦Sb2O3≦0.5
0.01≦Fe2O3≦0.08
F+Cl+Br≦0.4
wherein
1.05≦(MgO+CaO+SrO)/Al2O3≦1.7 a)
0.2≦MgO/(CaO+SrO+BaO)≦0.45 b)
where Al2O3, MgO, CaO, SrO and BaO represent the mol percents of the representative oxide components.

### Claim 2 (depends on 1)

The glass of claim 1, wherein SiO2+Al2O3=86.97−0.713*(MgO+CaO+SrO+BaO—Al2O3)±0.8.

### Claim 3 (depends on 1)

The glass of claim 1 further comprising a chemical fining agent.

### Claim 4 (depends on 3)

The glass of claim 3 wherein the fining agent is selected from the group consisting of: SnO2, Fe2O3, CeO2, Sb2O3, As2O3, or mixtures thereof.

### Claim 5 (depends on 1)

The glass of claim 1 further comprising less than 0.05% by weight of As2O3, Sb2O3 or combinations thereof.

### Claim 6 (depends on 1)

The glass of claim 1 further comprising less than 0.02% by weight of F, Cl, Br or combinations thereof.

### Claim 7 (depends on 1)

The glass of claim 1 further exhibiting a specific modulus in excess of 30 GPa cm3/gm.

### Claim 8 (depends on 1)

The glass of claim 1 further comprising less than about 1000 ppm of alkali oxides.

### Claim 9 (depends on 1)

The glass of claim 1 further comprising up to about 500 ppm ZrO2.

### Claim 10 (depends on 1)

The glass of claim 1 wherein 0.29≦MgO/(MgO+CaO+SrO+BaO)≦0.39.