# US 2013/0295745 A1 · Method of manufacturing nonvolatile memory device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0295745 A1
- Document ID: US20130295745A1
- Status: Published application
- Kind: A1
- Application number: 13/997,818
- Filed: 2012-03-09
- Published: 2013-11-07
- Earliest claimed: 2011-03-10
- Assignees: Panasonic Corporation
- Inventors: Ichirou Takahashi; Takumi Mikawa
- Web page: https://patentgrep.com/patent/US20130295745A1

## CPC

- H10N 70/041: {Modification of switching materials after formation, e.g. doping (shaping H10N70/061)}
- H10N 70/026: {by physical vapor deposition, e.g. sputtering}
- H10N 70/063: {by etching of pre-deposited switching material layers, e.g. lithography}
- H10N 70/20: Multistable switching devices, e.g. memristors
- H10N 70/24: {based on migration or redistribution of ionic species, e.g. anions, vacancies}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/8833: {Binary metal oxides, e.g. TaOx}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

A method of manufacturing a nonvolatile memory device includes: forming a tantalum oxide material layer including an oxygen-deficient transition metal oxide; forming a tantalum oxide material layer including a transition metal oxide and having a degree of oxygen deficiency lower than a degree of oxygen deficiency of the tantalum oxide material layer; and exposing, after the forming of a tantalum oxide material layer, the tantalum oxide material layer to plasma generated from a noble gas.

## Claims

### Claim 1

A method of manufacturing a nonvolatile memory device, the method comprising:
forming a first oxide material layer comprising an oxygen-deficient transition metal oxide;
forming a second oxide material layer comprising a transition metal oxide and having a degree of oxygen deficiency lower than a degree of oxygen deficiency of the first oxide material layer; and
exposing the second oxide material layer to plasma after the forming of a second oxide material layer, the plasma being generated from a noble gas.

### Claim 2 (depends on 1)

The method of manufacturing a nonvolatile memory device according to claim 1,
wherein in the exposing, the second oxide material layer is exposed to plasma generated from a noble gas only.

### Claim 3 (depends on 2)

The method of manufacturing a nonvolatile memory device according to claim 2,
wherein in the exposing, the noble gas is a single kind of noble gas.

### Claim 4 (depends on 1)

The method of manufacturing a nonvolatile memory device according to claim 1, further comprising:
forming a first electrode material layer above a substrate; and
forming a second electrode material layer on the second oxide material layer,
wherein in the forming of a first oxide material layer, the first oxide material layer is formed on the first electrode material layer, and
in the forming of a second oxide material layer, the second oxide material layer is formed on the first oxide material layer.

### Claim 5 (depends on 1)

The method of manufacturing a nonvolatile memory device according to claim 1, further comprising:
forming a first electrode material layer above a substrate; and
forming a second electrode material layer on the first oxide material layer,
wherein in the forming of a second oxide material layer, the second oxide material layer is formed on the first electrode material layer, and
in the forming of a first oxide material layer, the first oxide material layer is formed on the second oxide material layer.

### Claim 6

A method of manufacturing a nonvolatile memory device, the method comprising:
forming a first electrode material layer above a substrate;
depositing, on the first electrode material layer, a first oxide material layer comprising an oxygen-deficient transition metal oxide;
depositing, on the first oxide material layer, a second oxide material layer comprising a transition metal oxide and having a degree of oxygen deficiency lower than a degree of oxygen deficiency of the first oxide material layer;
exposing the second oxide material layer to plasma after the depositing of a second oxide material layer, the plasma being generated from gas containing at least a noble gas;
forming a second electrode material layer on the second oxide material layer after the exposing; and
applying an initialization voltage pulse between a first electrode layer and a second electrode layer to form a conductive path in a variable resistance element including the first electrode layer, a first variable resistance layer, a second variable resistance layer, and the second electrode layer which are formed through patterning of the first electrode material layer, the first oxide material layer, the second oxide material layer, and the second electrode material layer, respectively, the conductive path extending from one surface to another of the second variable resistance layer, the one surface being in contact with the second electrode layer, and the other surface being in contact with the first variable resistance layer.

### Claim 7

A method of manufacturing a nonvolatile memory device, the method comprising:
forming a first electrode material layer above a substrate;
depositing, on the first electrode material layer, a second oxide material layer comprising a transition metal oxide;
depositing, on the second oxide material layer, a first oxide material layer comprising an oxygen-deficient transition metal oxide and having a degree of oxygen deficiency higher than a degree of oxygen deficiency of the second oxide material layer;
exposing the second oxide material layer to plasma before the depositing of a first oxide material layer after the depositing of a second oxide material layer, the plasma being generated from gas containing at least a noble gas;
forming a second electrode material layer on the first oxide material layer after the depositing of a first oxide material layer; and
applying an initialization voltage pulse between a first electrode layer and a second electrode layer to form a conductive path in a variable resistance element including the first electrode layer, a second variable resistance layer, a first variable resistance layer, and the second electrode layer which are formed through patterning of the first electrode material layer, the second oxide material layer, the first oxide material layer, and the second electrode material layer, respectively, the conductive path extending from one surface to another of the second variable resistance layer, the one surface being in contact with the first electrode layer, and the other surface being in contact with the first variable resistance layer.

### Claim 8 (depends on 6)

The method of manufacturing a nonvolatile memory device according to claim 6,
wherein the exposing includes mixture plasma treatment of exposing the second oxide material layer to plasma generated from a gas mixture of a noble gas and oxygen.

### Claim 9 (depends on 8)

The method of manufacturing a nonvolatile memory device according to claim 8,
wherein the exposing further includes, before the mixture plasma treatment, single-gas plasma treatment of exposing the second oxide material layer to plasma generated from single kind of noble gas.

### Claim 10 (depends on 8)

The method of manufacturing a nonvolatile memory device according to claim 8,
wherein the exposing further includes, after the mixture plasma treatment, annealing which is thermal treatment in a nitrogen gas atmosphere.

### Claim 11 (depends on 1)

The method of manufacturing a nonvolatile memory device according to claim 1,
wherein the forming of a second oxide material layer and the exposing are continuously repeated more then once.

### Claim 12 (depends on 1)

The method of manufacturing a nonvolatile memory device according to claim 1,
wherein the first oxide material layer comprises tantalum oxide having a composition represented as TaOx (where 0.8≦x≦1.9), and
the second oxide material layer comprises tantalum oxide having a composition represented as TaOy (where x<y).

### Claim 13 (depends on 1)

The method of manufacturing a nonvolatile memory device according to claim 1,
wherein the second oxide material layer is formed as a deposited film.

### Claim 14 (depends on 1)

The method of manufacturing a nonvolatile memory device according to claim 1,
wherein the second oxide material layer is deposited by sputtering.

### Claim 15 (depends on 7)

The method of manufacturing a nonvolatile memory device according to claim 7,
wherein the exposing includes mixture plasma treatment of exposing the second oxide material layer to plasma generated from a gas mixture of a noble gas and oxygen.

### Claim 16 (depends on 15)

The method of manufacturing a nonvolatile memory device according to claim 15,
wherein the exposing further includes, before the mixture plasma treatment, single-gas plasma treatment of exposing the second oxide material layer to plasma generated from single kind of noble gas.

### Claim 17 (depends on 15)

The method of manufacturing a nonvolatile memory device according to claim 15,
wherein the exposing further includes, after the mixture plasma treatment, annealing which is thermal treatment in a nitrogen gas atmosphere.

### Claim 18 (depends on 6)

The method of manufacturing a nonvolatile memory device according to claim 6,
wherein the forming of a second oxide material layer and the exposing are continuously repeated more then once.

### Claim 19 (depends on 7)

The method of manufacturing a nonvolatile memory device according to claim 7,
wherein the forming of a second oxide material layer and the exposing are continuously repeated more then once.

### Claim 20 (depends on 6)

The method of manufacturing a nonvolatile memory device according to claim 6,
wherein the first oxide material layer comprises tantalum oxide having a composition represented as TaOx (where 0.8≦x≦1.9), and
the second oxide material layer comprises tantalum oxide having a composition represented as TaOy (where x<y).

### Claim 21 (depends on 7)

The method of manufacturing a nonvolatile memory device according to claim 7,
wherein the first oxide material layer comprises tantalum oxide having a composition represented as TaOx (where 0.8≦x≦1.9), and
the second oxide material layer comprises tantalum oxide having a composition represented as TaOy (where x<y).

### Claim 22 (depends on 6)

The method of manufacturing a nonvolatile memory device according to claim 6,
wherein the second oxide material layer is deposited by sputtering.

### Claim 23 (depends on 7)

The method of manufacturing a nonvolatile memory device according to claim 7,
wherein the second oxide material layer is deposited by sputtering.