# US 2013/0295731 A1 · Thin film transistor array panel and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0295731 A1
- Document ID: US20130295731A1
- Status: Published application
- Kind: A1
- Application number: 13/940,761
- Filed: 2013-07-12
- Published: 2013-11-07
- Earliest claimed: 2007-02-07
- Assignees: Samsung Display Co., Ltd.
- Applicants: Samsung Display Co., Ltd.
- Inventors: BYOUNG-JUNE KIM; Jae-Ho Choi; Chang-Oh Jeong; Sung-Hoon Yang; Je-Hun Lee; Do-Hyun Kim; Hwa-Yeul Oh; Yong-Mo Choi
- Web page: https://patentgrep.com/patent/US20130295731A1

## CPC

- H10D 86/60: wherein the TFTs are in active matrices
- H10D 30/031: {of thin-film transistors [TFT]}
- H10D 30/0316: {of lateral bottom-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 30/6739: {Conductor-insulator-semiconductor electrodes}
- H10D 86/00: Integrated devices formed in or on insulating or conducting substrates, e.g. formed in silicon-on-insulator [SOI] substrates or on stainless steel or glass substrates
- H10D 86/40: characterised by multiple TFTs
- H10D 86/441: {Interconnections, e.g. scanning lines}
- H10D 86/481: {integrated with passive devices, e.g. auxiliary capacitors}
- H10D 30/6729: {characterised by the electrodes}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A manufacturing method of a thin film transistor (TFT) includes forming a gate electrode including a metal that can be combined with silicon to form silicide on a substrate and forming a gate insulation layer by supplying a gas which includes silicon to the gate electrode at a temperature below about 280° C. The method further includes forming a semiconductor on the gate insulation layer, forming a data line and a drain electrode on the semiconductor and forming a pixel electrode connected to the drain electrode.

## Claims

### Claim 1

A method of manufacturing a thin film transistor array panel, comprising:
forming a gate electrode including a metal that can be combined with silicon to form silicide;
forming a first silicon nitride layer on the gate electrode by supplying a gas which includes silicon and a gas which includes nitrogen;
forming a second silicon nitride layer by supplying a gas which includes silicon and a gas which includes nitrogen on the first silicon nitride layer, wherein a flow amount ratio of the two gases is different from a flow amount ratio supplied for forming the first silicon nitride layer;
forming a semiconductor on the second silicon nitride layer;
forming a data line and a drain electrode on the semiconductor; and
forming a pixel electrode connected to the drain electrode,
wherein a [N—H]/[Si—H] binding number ratio of the second silicon nitride layer is less than that of the first silicon nitride layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first silicon nitride layer is deposited for a deposition speed of less than 15 Å/sec.

### Claim 3 (depends on 2)

The method of claim 2, wherein the second silicon nitride layer is deposited for a deposition speed of more than 20 Å/sec.

### Claim 4 (depends on 2)

The method of claim 2, wherein the ratio of the [N—H]/[Si—H] binding number of the first silicon nitride layer is 10 times higher than a ratio of the [N—H]/[Si—H] binding number of the second silicon nitride layer.

### Claim 5 (depends on 4)

The method of claim 4, wherein a [N—H]/[Si—H] binding number ratio of the first silicon nitride layer is about 20 to about 40, and a [N—H]/[Si—H] binding number ratio of the second silicon nitride layer is about 1.5 to about 2.5.

### Claim 6 (depends on 4)

The method of claim 4, wherein the first silicon nitride layer has a thickness of about 50 to about 600 angstroms (Å).

### Claim 7 (depends on 6)

The method of claim 6, wherein the gate line comprises copper.

### Claim 8 (depends on 1)

The method of claim 1, wherein the ratio of the [N—H]/[Si—H] binding number of the first silicon nitride layer is 10 times higher than a ratio of the [N—H]/[Si—H] binding number of the second silicon nitride layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein a [N—H]/[Si—H] binding number ratio of the first silicon nitride layer is about 20 to about 40, and a [N—H]/[Si—H] binding number ratio of the second silicon nitride layer is about 1.5 to about 2.5.

### Claim 10 (depends on 8)

The method of claim 8, wherein the first silicon nitride layer has a thickness of about 50 to about 600 angstroms (Å).

### Claim 11 (depends on 10)

The method of claim 10, wherein the gate line comprises copper.

### Claim 12 (depends on 1)

The method of claim 1, wherein the first silicon nitride layer has a thickness of about 50 to about 600 angstroms (Å).

### Claim 13 (depends on 12)

The method of claim 12, wherein the gate line comprises copper.

### Claim 14 (depends on 1)

The method of claim 1, wherein the gate line comprises copper.