# US 2013/0295709 A1 · Method for manufacturing photoelectric conversion elements

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0295709 A1
- Document ID: US20130295709A1
- Status: Published application
- Kind: A1
- Application number: 13/900,945
- Filed: 2013-05-23
- Published: 2013-11-07
- Earliest claimed: 2007-12-19
- Assignees: Tohoku University; Tokyo Electron Limited
- Applicants: Tohoku University; Tokyo Electron Limited
- Inventors: Tadahiro OHMI; Akinobu TERAMOTO; Tetsuya GOTO; Kouji TANAKA
- Web page: https://patentgrep.com/patent/US20130295709A1

## CPC

- H10F 71/135: {Application of a bias; Current injection}
- C23C 16/24: Deposition of silicon only
- C23C 16/511: using microwave discharges
- H10F 10/00: Individual photovoltaic cells, e.g. solar cells (electrolytic light-sensitive devices, e.g. dye-sensitised solar cells, H01G9/20)
- H10F 10/165: the heterojunctions being Group IV-IV heterojunctions, e.g. Si/Ge, SiGe/Si or Si/SiC photovoltaic cells
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 71/1215: {comprising at least two Group IV elements, e.g. SiGe}
- H10F 71/1218: {in microcrystalline form}
- H10F 77/122: comprising only Group IV materials
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

“The invention provides a photoelectric conversion element manufacturing apparatus that forms a semiconductor stack film on a substrate by using microwave plasma CVD. The apparatus includes a chamber which is a enclosed space containing a base, on which the a subject substrate for thin-film formation is mounted, a first gas supply unit which supplies plasma excitation gas to a plasma excitation region in the chamber, a pressure regulation unit which regulates pressure in the chamber, a second gas supply unit which supplies raw gas to a plasma diffusion region in the chamber, a microwave application unit which applies microwaves into the chamber, and a bias voltage application unit which selects and applies a substrate bias voltage to the substrate according to the type of gas.”

## Claims

### Claim 1

A method of manufacturing photoelectric conversion elements, the method comprising:
introducing plasma excitation gas into a chamber containing a base on which a substrate for thin-film formation is mounted;
introducing raw gas into the chamber after introducing microwaves into the chamber, or introducing microwaves into the chamber after introducing raw gas into the chamber; and
applying a predetermined substrate bias voltage to the substrate so that a defect concentration of a thin film formed on the substrate is equal to or less than 1017 /cm3.

### Claim 2 (depends on 1)

The method of claim 1, wherein a radio frequency of the predetermined substrate bias voltage applied to the substrate is adjusted according to a type of gas.

### Claim 3 (depends on 1)

The method of claim 1, further comprising:
after the introducing of plasma excitation gas into the chamber and before the introducing of raw gas into the chamber, regulating pressure in the chamber.

### Claim 4 (depends on 1)

The method of claim 1, wherein the applying of the predetermined bias voltage to the substrate is performed by using an electrode disposed in the base.

### Claim 5

A method of manufacturing photoelectric conversion elements, the method comprising:
introducing plasma excitation gas into a chamber containing a base on which a substrate for thin-film formation is mounted;
introducing raw gas into the chamber after introducing microwaves into the chamber, or introducing microwaves into the chamber after introducing raw gas into the chamber; and
applying a predetermined substrate bias voltage to the substrate so that an oxygen concentration of a thin film formed on the substrate is equal to or less than 1019 atom/cm3.

### Claim 6 (depends on 5)

The method of claim 5, wherein a radio frequency of the predetermined substrate bias voltage applied to the substrate is adjusted according to a type of gas.

### Claim 7 (depends on 5)

The method of claim 5, further comprising:
after the introducing of plasma excitation gas into the chamber and before the introducing of raw gas into the chamber, regulating pressure in the chamber.

### Claim 8 (depends on 5)

The method of claim 5, wherein the applying of the predetermined bias voltage to the substrate is performed by using an electrode disposed in the base.

### Claim 9

A method of manufacturing a photoelectric conversion element, the method comprising:
introducing plasma excitation gas into a chamber containing a base on which a substrate for thin-film formation is mounted;
introducing raw gas into the chamber after introducing microwaves into the chamber, or introducing microwaves into the chamber after introducing raw gas into the chamber; and
applying a predetermined substrate bias voltage to the substrate so that a defect concentration of a thin film formed on the substrate is equal to or less than 1017/cm3 and is an oxygen concentration of a thin film formed on the substrate is equal to or less than 1019 atom/cm3.

### Claim 10 (depends on 9)

The method of claim 9, wherein a radio frequency of the predetermined substrate bias voltage applied to the substrate is adjusted according to a type of gas.

### Claim 11 (depends on 9)

The method of claim 9, further comprising:
after the introducing of plasma excitation gas into the chamber and before the introducing of raw gas into the chamber, regulating pressure in the chamber.

### Claim 12 (depends on 9)