# US 2013/0295392 A1 · Anti-reflection glass with tin oxide nanoparticles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0295392 A1
- Document ID: US20130295392A1
- Status: Published application
- Kind: A1
- Application number: 13/465,311
- Filed: 2012-05-07
- Published: 2013-11-07
- Earliest claimed: 2012-05-07
- Assignees: Guardian Industries Corp.
- Inventors: Liang LIANG; Richard Blacker
- Web page: https://patentgrep.com/patent/US20130295392A1

## CPC

- C03C 17/007: {containing a dispersed phase, e.g. particles, fibres or flakes, in a continuous phase}
- G02B 1/115: Multilayers
- C03C 2217/211: SnO2
- C03C 2217/213: SiO2
- C03C 2217/42: consisting of particles only
- C03C 2217/732: made of a single layer
- C03C 2217/77: Coatings having a rough surface
- C03C 2218/113: by sol-gel processes
- C03C 2218/116: by spin-coating, centrifugation
- C03C 2218/365: Coating different sides of a glass substrate
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

An improved anti-reflection glass with higher transmittance (ΔTqe %) results from a coating of or including tin oxide (e.g., SnO2) nanoparticles (e.g., 10-20 nm in size) applied to a surface of solar float or matte/matte glass. The tin oxide based coating layer shows improved chemical stability and durability and can be prepared using a sol-gel process and applied by spin coating. Matte/matte anti-reflection glass samples may have two coating layers (e.g., SnO2 nanoparticles on the rough side and SiO2 nanoparticles on the smooth side) and exhibit an improved transmittance (e.g., visible transmittance) of at least 2.0%, e.g., about 3.5%. As high as a 30% increase of ΔTqe % has been observed when anti-reflection matte/matte glass coated with SnO2 is exposed in a salt fog chamber for 5 days. The increase in transmittance may be due to the different pore structure of the SnO2 coating layer, while the increase of Tqe % in a salt fog chamber may be due to the crystalline SnO2 formation.

## Claims

### Claim 1

A method of forming a coated article comprising an anti-reflection coating on a glass substrate to increase transmittance, the method comprising:
providing a colloidal solution comprising tin oxide based nanoparticles;
depositing at least a portion of said colloidal solution comprising tin oxide based nanoparticles on a glass substrate to form a substantially uniform coating;
curing said coating at least by heating said glass substrate and said coating.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the thickness of said coating is between 20 and 100 nm.

### Claim 3 (depends on 1)

A method according to claim 1, wherein the amount of increase in said glass transmittance is about 3.5%.

### Claim 4 (depends on 1)

A method according to claim 1, wherein said glass substrate is a matte/matte glass.

### Claim 5 (depends on 1)

A method according to claim 1, wherein said glass substrate is a solar float glass.

### Claim 6 (depends on 1)

A method according to claim 1, wherein said colloidal solution contains a binder comprising tetraethyl orthosilicate.

### Claim 7 (depends on 1)

A method according to claim 1, wherein said tin oxide based nanoparticles comprise SnO2 nanoparticles ranging in size from about 10 to 20 nm.

### Claim 8 (depends on 1)

A method according to claim 1, wherein the weight percentage of said nanoparticles is about 2-5%.

### Claim 9 (depends on 1)

A method according to claim 1, wherein said colloidal solution containing tin oxide based nanoparticles is applied directly to said glass substrate using a spin coating method.

### Claim 10 (depends on 9)

A method according to claim 9, wherein said colloidal solution is applied using spin coating to a roughened side of said glass substrate.

### Claim 11 (depends on 1)

A method according to claim 1, further comprising applying a colloidal solution comprising silica to a smooth side of said glass substrate.

### Claim 12 (depends on 11)

A method according to claim 11, wherein the amount of said silica in said coating is about 3% by wt.

### Claim 13 (depends on 1)

A method according to claim 1, wherein said transmittance is defined as:
Tqe

%
=
∑
i
=
400
1200


(
Tqe

%
)
i
∑
i
=
400
1200


N
i

### Claim 14 (depends on 1)

A method according to claim 1, wherein said increase in transmittance is defined as: Tqe %=(Tqe %)AR−(Tqe %)raw

### Claim 15

An anti-reflection coating for a glass substrate comprising:
a colloidal solution;
a plurality of SnO2 nanoparticles uniformly dispersed in said colloidal solution; and
a binder composition.

### Claim 16 (depends on 15)

An anti-reflection coating according to claim 15, wherein said colloidal solution comprises a mixture of deionized water, acetic acid and n-propyl alcohol.

### Claim 17 (depends on 15)

An anti-reflection coating according to claim 15, wherein said binder composition comprises tetraethyl orthosilicate.

### Claim 18 (depends on 15)

An anti-reflection coating according to claim 15, wherein the amount of said SnO2 nanoparticles is about 2-5% by wt.

### Claim 19 (depends on 15)

An anti-reflection coating according to claim 15, wherein the size range of said SnO2 nanoparticles is between 10-20 nm.

### Claim 20

A glass article containing an anti-reflection coating, comprising:
a glass substrate;
a coating applied directly onto a surface of said substrate, said coating comprising a colloidal solution containing a plurality of SnO2 nanoparticles.