# US 2013/0295387 A1 · Method for synthesis of cubic boron nitride and cubic boron nitride structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0295387 A1
- Document ID: US20130295387A1
- Status: Published application
- Kind: A1
- Application number: 13/744,557
- Filed: 2013-01-18
- Published: 2013-11-07
- Earliest claimed: 2012-05-03
- Assignees: Korea Institute of Science and Technology
- Applicants: Korea Institute of Science and Technology
- Inventors: Young Joon BAIK; Jong Keuk PARK; Wook Seong LEE
- Web page: https://patentgrep.com/patent/US20130295387A1

## CPC

- C23C 16/342: {Boron nitride}
- C23C 14/024: {Deposition of sublayers, e.g. to promote adhesion of the coating (C23C14/027 takes precedence)}
- C23C 14/06: characterised by the coating material ({C23C14/0021} , C23C14/04 take precedence)
- C23C 14/0647: {Boron nitride}
- C23C 14/34: Sputtering
- C23C 14/46: by ion beam produced by an external ion source
- C23C 16/271: {using hot filaments}
- Y10T 428/30: Self-sustaining carbon mass or layer with impregnant or other layer
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for producing a cubic boron nitride (cBN) thin film includes depositing cBN onto nanocrystalline diamond having controlled surface irregularity characteristics to improve the adhesion at the interface of cBN/nanocrystalline diamond, while incorporating hydrogen to a reaction gas upon the synthesis of cBN and controlling the feed time of hydrogen, so that harmful reactions occurring on a surface of nanocrystalline diamond and residual stress applied to cBN may be inhibited. Also, a cBN thin film structure is obtained by the method. The cBN thin film is formed on the nanocrystalline diamond thin film by using a physical vapor deposition process, wherein a reaction gas supplied when the deposition of a thin film occurs is a mixed gas of argon (Ar) with nitrogen (N2), and hydrogen (H2) is added to the reaction gas at a time after the deposition of a thin film occurs.

## Claims

### Claim 1

A method for producing a cubic boron nitride (cBN) thin film, comprising forming a cBN thin film on a nanocrystalline diamond thin film by using a physical vapor deposition process,
wherein, in the forming the cBN thin film, a reaction gas supplied when the deposition of a thin film occurs is a mixed gas of argon (Ar) with nitrogen (N2), and hydrogen (H2) is added to the reaction gas at a time after the deposition of a thin film occurs.

### Claim 2 (depends on 1)

The method according to claim 1, wherein a turbostratic BN (tBN) thin film is formed before the cBN thin film is formed on the nanocrystalline diamond thin film, wherein a mixed gas of Ar with N2 is supplied as a reaction gas until the time of the tBN thin film formation, and wherein a mixed gas of Ar, N2 and H2 is supplied as a reaction gas after the completion of the growth of the tBN thin film.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the physical vapor deposition process is a sputtering process or ion beam deposition process.

### Claim 4

A cBN thin film structure comprising a tBN thin film and a cBN thin film grown sequentially on a nanocrystalline diamond thin film,
wherein the tBN thin film and the cBN thin film are formed through a sputtering process or ion beam deposition process, and wherein a mixed gas of Ar with N2 is used as a reaction gas during the growth of the tBN thin film, while a mixed gas of Ar, N2 and H2 is used as the reaction gas after the growth of the tBN thin film is completed on a surface of the nanocrystalline diamond thin film.