# US 2013/0295357 A1 · Light-weight hybrid glass laminates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0295357 A1
- Document ID: US20130295357A1
- Status: Published application
- Kind: A1
- Application number: 13/937,707
- Filed: 2013-07-09
- Published: 2013-11-07
- Earliest claimed: 2011-06-24
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Thomas Michael Cleary; Timothy Scott Huten; Michael John Moore
- Web page: https://patentgrep.com/patent/US20130295357A1

## CPC

- B32B 17/10091: {thermally hardened}
- B32B 17/10036: {comprising two outer glass sheets}
- B32B 17/10119: {having a composition deviating from the basic composition of soda-lime glass, e.g. borosilicate}
- B32B 17/10137: {Chemical strengthening}
- B32B 17/10761: {containing vinyl acetal}
- B32B 2605/006: Transparent parts other than made from inorganic glass, e.g. polycarbonate glazings
- Y10T 428/24967: Absolute thicknesses specified
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A glass laminate comprises an external glass sheet, an internal glass sheet, and a polymer interlayer formed between the external glass sheet and the internal glass sheet. The external glass sheet can be a thin chemically-strengthened glass sheet or can be a non-chemically strengthened glass sheet, the polymer interlayer can have a thickness of less than 1.6 mm, and the internal glass sheet can be a non-chemically-strengthened glass sheet or a thin chemically strengthened glass sheet.

## Claims

### Claim 1

A glass laminate structure comprising:
a non-chemically strengthened external glass sheet;
a chemically strengthened internal glass sheet; and
at least one polymer interlayer intermediate the external and internal glass sheets,
wherein the internal glass sheet has a thickness ranging from about 0.5 mm to about 1.5 mm, and
wherein the external glass sheet has a thickness ranging from about 1.5 mm to about 3.0 mm.

### Claim 2 (depends on 1)

The glass laminate structure of claim 1, wherein the internal glass sheet includes one or more alkaline earth oxides, such that a content of alkaline earth oxides is at least about 5 wt. %.

### Claim 3 (depends on 1)

The glass laminate structure of claim 1, wherein the internal glass sheet includes at least about 6 wt. % aluminum oxide.

### Claim 4 (depends on 1)

The glass laminate structure of claim 1, wherein the internal glass sheet has a thickness of between about 0.5 mm to about 0.7 mm.

### Claim 5 (depends on 1)

The glass laminate structure of claim 1, wherein the polymer interlayer comprises a single polymer sheet, a multilayer polymer sheet, or a composite polymer sheet.

### Claim 6 (depends on 1)

The glass laminate structure of claim 1, wherein the polymer interlayer comprises a material selected from the group consisting of poly vinyl butyral (PVB), polycarbonate, acoustic PVB, ethylene vinyl acetate (EVA), thermoplastic polyurethane (TPU), ionomer, a thermoplastic material, and combinations thereof.

### Claim 7 (depends on 1)

The glass laminate structure of claim 1, wherein the polymer interlayer has a thickness of between about 0.4 to about 1.2 mm.

### Claim 8 (depends on 1)

The glass laminate structure of claim 1, wherein the external glass sheet comprises a material selected from the group consisting of soda-lime glass and annealed glass.

### Claim 9 (depends on 1)

The glass laminate structure of claim 1, wherein the external glass sheet has a thickness of about 2.1 mm.

### Claim 10 (depends on 1)

The glass laminate structure of claim 1, wherein the glass laminate has an area greater than 1 m2.

### Claim 11 (depends on 1)

The glass laminate structure of claim 1, wherein the glass laminate is an automotive windshield, sunroof or cover plate.

### Claim 12 (depends on 1)

The glass laminate structure of claim 1, wherein the inner glass layer has a surface compressive stress between about 250 MPa and about 900 MPa.

### Claim 13 (depends on 1)

The glass laminate structure of claim 1, wherein the inner glass layer has a surface compressive stress of between about 250 MPa and about 350 MPa and a DOL of compressive stress greater than about 20 μm.

### Claim 14 (depends on 1)

The glass laminate structure of claim 1 wherein a surface of the external glass layer adjacent the interlayer is acid etched.

### Claim 15 (depends on 1)

The glass laminate structure of claim 1 wherein a surface of the internal glass layer opposite the interlayer is acid etched.

### Claim 16

A glass laminate structure comprising:
a non-chemically strengthened external glass sheet;
a chemically strengthened internal glass sheet; and
at least one polymer interlayer intermediate the external and internal glass sheets,
wherein the inner glass layer has a surface compressive stress between about 250 MPa and about 900 MPa.

### Claim 17 (depends on 16)

The glass laminate structure of claim 16, wherein the inner glass layer has a surface compressive stress of between about 250 MPa and about 350 MPa and a DOL of compressive stress greater than about 20 μm.

### Claim 18 (depends on 16)

The glass laminate structure of claim 16, wherein the internal glass sheet has a thickness ranging from about 0.5 mm to about 1.5 mm, and
wherein the external glass sheet has a thickness ranging from about 1.5 mm to about 3.0 mm.

### Claim 19 (depends on 16)

The glass laminate structure of claim 16, wherein the polymer interlayer comprises a material selected from the group consisting of poly vinyl butyral (PVB), polycarbonate, acoustic PVB, ethylene vinyl acetate (EVA), thermoplastic polyurethane (TPU), ionomer, a thermoplastic material, and combinations thereof.

### Claim 20 (depends on 16)

The glass laminate structure of claim 16, wherein the polymer interlayer has a thickness of between about 0.4 to about 1.2 mm.