# US 2013/0284736 A1 · Housing and method for making same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284736 A1
- Document ID: US20130284736A1
- Status: Published application
- Kind: A1
- Application number: 13/524,317
- Filed: 2012-06-15
- Published: 2013-10-31
- Earliest claimed: 2012-04-25
- Assignees: FIH (Hong Kong) Limited; Shenzhen Futaihong Precision Industry Co., Ltd.
- Inventors: Shu-Xiang ZHOU; Qiu-Jiang XU; He-Xian LIN
- Web page: https://patentgrep.com/patent/US20130284736A1

## CPC

- C09D 183/04: Polysiloxanes
- C08J 7/042: {with two or more layers, where at least one layer of a composition contains a polymer binder}
- C08J 7/046: Forming abrasion-resistant coatings; Forming surface-hardening coatings
- C08J 7/06: with compositions not containing macromolecular substances
- C08J 2369/00: Characterised by the use of polycarbonates; Derivatives of polycarbonates
- C08J 2483/04: Polysiloxanes
- Y10T 428/31663: As siloxane, silicone or silane
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A housing includes a plastic substrate, an active layer formed on the plastic substrate, and an exterior layer formed on the active layer. The active layer contains polysiloxane and cetyl trimethyl ammonium bromide. The exterior layer contains silicon dioxide or titanium dioxide, and cetyl trimethyl ammonium bromide.

## Claims

### Claim 1

A method for making a housing, comprising:
providing a plastic substrate;
forming an activator by mixing silane coupling agent, organic solvent, deionized water, and a leveling agent, the mass ratio of the silane coupling agent, organic solvent, deionized water, and leveling agent being (3-5):(85-92):(3-5):(5-10);
coating the activator on the surface of the plastic substrate and drying to form an active layer;
Forming a coating solution by mixing silicon ester or titanium ester, organic solvent, deionized water, and a leveling agent, the mass ratio of the silicon ester or titanium ester, organic solvent, deionized water, and leveling agent being (45-55):(35-45):(3-5):(3-5); and
coating the surface of the active layer with the coating solution and drying the coating solution to form an exterior layer.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the organic solvent of the activator and the coating solution is isopropyl alcohol or ethanol.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the leveling agent of the activator and the coating solution is cetyl trimethyl ammonium bromide.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the drying of the activator is carried out at an environmental temperature of about 80° C. to about 100° C. for about 20 min to about 40 min.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the active layer has a thickness of about 0.1 μm to about 0.3 μm.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein the silicon ester is methyl silicate or tetraethyl silicate.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the titanium ester is tetrabutyl titanate.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein the coating solution further comprises nano calcium carbonate.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein the drying of the coating solution is carried out at an environmental temperature of about 100° C. to about 120° C. for about 30 min to about 50 min.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein the exterior layer has a thickness of about 0.6 μm to about 1.0 μm.

### Claim 11

A housing, comprising:
a plastic substrate;
an active layer formed on the plastic substrate; and
an exterior layer formed on the active layer;
wherein the active layer contains polysiloxane and cetyl trimethyl ammonium bromide, the exterior layer contains silicon dioxide or titanium dioxide, and cetyl trimethyl ammonium bromide.

### Claim 12 (depends on 11)

The coated article as claimed in claim 11, wherein mass ratio of the cetyl trimethyl ammonium bromide to polysiloxane in the active layer is (5-10):(90-95).

### Claim 13 (depends on 11)

The coated article as claimed in claim 11, wherein the active layer has a thickness of about 0.1 μm to about 0.3 μm.

### Claim 14 (depends on 11)

The coated article as claimed in claim 11, wherein the exterior layer further comprises nano calcium carbonate.

### Claim 15 (depends on 11)

The coated article as claimed in claim 11, wherein the exterior layer has a thickness of about 0.6 μm to about 1.0 μm.