# US 2013/0284693 A1 · Differentiated liftoff process for ultra-shallow mask defined narrow trackwidth magnetic sensor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284693 A1
- Document ID: US20130284693A1
- Status: Published application
- Kind: A1
- Application number: 13/458,374
- Filed: 2012-04-27
- Published: 2013-10-31
- Earliest claimed: 2012-04-27
- Assignees: Hitachi Global Storage Technologies Netherlands B.V.
- Inventors: Yi Zheng; Guomin Mao; Hicham M. Sougrati; Xiaozhong Dang
- Web page: https://patentgrep.com/patent/US20130284693A1

## CPC

- G11B 5/3163: {Fabrication methods or processes specially adapted for a particular head structure, e.g. using base layers for electroplating, using functional layers for masking, using energy or particle beams for shaping the structure or modifying the properties of the basic layers}
- G11B 5/398: {Specially shaped layers}
- Y10T 29/49043: Depositing magnetic layer or coating
- Y10T 29/49044: Plural magnetic deposition layers
- Y10T 29/49046: with etching or machining of magnetic material
- Y10T 29/49048: Machining magnetic material [e.g., grinding, etching, polishing]
- Y10T 29/49052: by etching
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for manufacturing a magnetic read sensor allows for the construction of a very narrow trackwidth sensor while avoiding problems related to mask liftoff and shadowing related process variations across a wafer. The process involves depositing a plurality of sensor layers and forming a first mask structure. The first mask structure has a relatively large opening that encompasses a sensor area and an area adjacent to the sensor area where a hard bias structure can be deposited. A second mask structure is formed over the first mask structure and includes a first portion that is configured to define a sensor dimension and a second portion that is over the first mask structure in the field area.

## Claims

### Claim 1

A method for manufacturing a magnetic read sensor, comprising:
depositing a plurality of sensor layers;
forming a first mask structure over the plurality of sensor layers, the first mask structure covering a field area removed from a sensor area and having an opening that extends over the sensor area and also over an area adjacent to the sensor area;
forming a second mask structure, the second mask structure having a first portion that covers an area configured to define a sensor dimension and having a second portion that is formed over the portion of the first mask structure that is in the field area removed from the sensor; and
performing an ion milling to remove portion of the sensor material that are not covered by the first or the second mask structure.

### Claim 2 (depends on 1)

The method as in claim 1 further comprising after performing the ion milling, performing a liftoff process to remove the portions of the first and second mask structures located in the field; and
performing a chemical mechanical polishing to remove the first portion of the second mask structure located over the sensor area.

### Claim 3 (depends on 2)

The method as in claim 2 wherein the liftoff process includes a wrinkle bake process and a NMP chemical liftoff.

### Claim 4 (depends on 2)

The method as in claim 2 wherein the liftoff process includes a wrinkle bake process, a NMP chemical liftoff, and cleaning with CO2.

### Claim 5 (depends on 1)

The method as in claim 1 wherein the opening in the first mask structure encompasses the sensor area and a hard bias region at first and second sides of the sensor area.

### Claim 6 (depends on 5)

The method as in claim 5, further comprising:
after performing the ion milling, depositing a thin insulation layer, depositing a hard magnetic material over the thin insulation layer, and depositing a layer of material that is resistant to chemical mechanical polishing; and thereafter;
performing a liftoff process to remove the first mask layer and the second portion of the second mask structure that is formed over the first mask structure; and
performing a chemical mechanical polishing to remove the first portion of the first mask structure that is formed over the sensor area.

### Claim 7

A method for manufacturing a magnetic read sensor, comprising:
depositing a plurality of sensor layers;
depositing a CMP stop layer over the plurality of sensor layers;
depositing an image transfer layer over the CMP stop layer;
forming a first mask structure over the image transfer layer, the first mask structure covering a field area removed from a sensor area and having an opening that extends over the sensor area and also over an area adjacent to the sensor area;
depositing a hard mask layer over the image transfer layer and over the first mask structure;
forming a second mask structure, the second mask structure having a first portion that covers an area configured to define a sensor dimension and having a second portion that is formed over the portion of the first mask structure that is in the field area removed from the sensor;
transferring the image of the second mask structure onto the under-lying image transfer layer and hard mask layer; and
performing an ion milling to remove portion of the sensor material that are not covered by the first mask structure, hard mask layer and image transfer layer.

### Claim 8 (depends on 7)

The method as in claim 7 wherein the image transfer layer comprises a soluble polyimide having a thickness of 20-100 nm.

### Claim 9 (depends on 7)

The method as in claim 7 wherein the image transfer layer comprises a soluble polyimide having a thickness of about 50 nm.

### Claim 10 (depends on 7)

The method as in claim 7 wherein the hard mask layer comprises SiO2.

### Claim 11 (depends on 7)

The method as in claim 7 wherein the hard mask layer comprises SiO2, SiN, SiOxNy, TaO or Ta2O5, SiC, Al2O3, TiN or Cr.

### Claim 12 (depends on 7)

The method as in claim 7 wherein the hard mask is deposited by sputter deposition or ion beam deposition.

### Claim 13 (depends on 7)

The method as in claim 7 wherein the hard mask comprises Si and the first mask structure is constructed of photo sensitive polymer material that can sustain high temperature baking without being fully cured.

### Claim 14 (depends on 7)

The method as in claim 7 wherein the hard mask comprises Si and is deposited by a spin-on process and wherein the first mask structure is constructed of a photoresist that can withstand a high temperature of 200 degrees C. without becoming fully cured.

### Claim 15 (depends on 14)

The method as in claim 14 wherein the hard mask comprises a material that can be cured at temperature lower than 200 C.

### Claim 16

A method for manufacturing a magnetic read sensor, comprising:
depositing a plurality of sensor layers;
depositing CMP stop layer over the plurality of sensor layers;
forming a first mask structure directly onto the CMP stop layer, the first mask structure covering a field area removed from a sensor area and having an opening that extends over the sensor area and also over an area adjacent to the sensor area;
depositing a hard mask layer over the CMP stop layer and over the first mask structure;
forming a second mask structure, the second mask structure having a first portion that covers an area configured to define a sensor dimension and having a second portion that is formed over the portion of the first mask structure that is in the field area removed from the sensor;
transferring the image of the second mask structure onto the hard mask layer; and
performing an ion milling to remove portion of the sensor material that are not covered by the first mask structure and the hard mask layer.

### Claim 17 (depends on 16)

The method as in claim 16 wherein the hard mask layer comprises C, DLC, SiC, Al2O3, TaO, Ta2O5 or TiN.

### Claim 18 (depends on 16)

The method as in claim 16 wherein the hard mask layer is a multi-layer hard mask having formed of inorganic materials.

### Claim 19 (depends on 16)

The method as in claim 16 wherein the second mask is formed by first depositing a second hard mask, depositing and photolithographically patterning the second photoresist layer; performing image transferring of photoresist layer pattern into the second hard mask, and then further image transferring the second hard mask pattern into the hardmask through one or more reactive ion etching (RIE) processes.