# US 2013/0284604 A1 · Method and apparatus for electroplating semiconductor wafer when controlling cations in electrolyte

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284604 A1
- Document ID: US20130284604A1
- Status: Published application
- Kind: A1
- Application number: 13/869,891
- Filed: 2013-04-24
- Published: 2013-10-31
- Earliest claimed: 2012-04-27
- Assignees: Novellus Systems, Inc.
- Inventors: Tighe A. Spurlin; Charles L. Merrill; Ludan Huang; Matthew Thorum; Lee Brogan; James E. Duncan; Frederick D. Wilmot; Marshall R. Stowell; Steven T. Mayer; Haiying Fu; David W. Porter; Shantinath Ghongadi; Jonathan D. Reid; Hyosang S. Lee; Mark J. Willey
- Web page: https://patentgrep.com/patent/US20130284604A1

## CPC

- C25D 21/14: Controlled addition of electrolyte components
- C25D 3/38: of copper
- C25D 17/001: {Apparatus specially adapted for electrolytic coating of wafers, e.g. semiconductors or solar cells}
- C25D 17/002: {Cell separation, e.g. membranes, diaphragms}
- C25D 21/12: Process control or regulation (controlling or regulating in general G05)
- C25D 21/18: of electrolytes (C25D21/22 takes precedence)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

Apparatus and methods for electroplating metal onto substrates are disclosed. The electroplating apparatus comprise an electroplating cell and at least one oxidization device. The electroplating cell comprises a cathode chamber and an anode chamber separated by a porous barrier that allows metal cations to pass through but prevents organic particles from crossing. The oxidation device (ODD) is configured to oxidize cations of the metal to be electroplated onto the substrate, which cations are present in the anolyte during electroplating. In some embodiments, the ODD is implemented as a carbon anode that removes Cu(I) from the anolyte electrochemically. In other embodiments, the ODD is implemented as an oxygenation device (OGD) or an impressed current cathodic protection anode (ICCP anode), both of which increase oxygen concentration in anolyte solutions. Methods for efficient electroplating are also disclosed.

## Claims

### Claim 1

An apparatus for electroplating a metal onto a substrate, the apparatus comprising:
(a) an electroplating cell comprising:
a cathode chamber for containing catholyte during electroplating;
a cathode electrical connection in the cathode chamber, the cathode electrical connection being able to connect to the substrate and apply a potential allowing the substrate to become a cathode;
an anode chamber for containing anolyte during electroplating;
an anode electrical connection in the anode chamber, the anode electrical connection being able to connect to an electroplating anode and apply a potential to the electroplating anode; and
a porous transport barrier placed between the anode chamber and the cathode chamber, which transport barrier enables migration of ionic species in an electrolyte, including metal cations, across the transport barrier while substantially preventing organic additives from passing across the transport barrier; and
(b) at least one oxidation device (ODD) configured to oxidize cations of the metal to be electroplated onto the substrate, which cations are present in the anolyte during electroplating.

### Claim 2 (depends on 1)

The apparatus of claim 1, wherein the metal to be electroplated onto the substrate is copper, the anolyte comprises one or more copper salts dissolved in a solvent, and the oxidation device (ODD) oxidizes Cu(I) to Cu(II).

### Claim 3 (depends on 2)

The apparatus of claim 2, wherein the catholyte contains a substantially greater concentration of the organic plating additives than the anolyte does.

### Claim 4 (depends on 2)

The apparatus of claim 2, wherein the porous transport barrier comprises a material selected from the group consisting of porous glasses, porous ceramics, silica areogels, organic aerogels, porous polymeric materials, and filter membranes.

### Claim 5 (depends on 2)

The apparatus of claim 2, wherein the at least one oxidation device (ODD) is selected from the group comprising an oxygenation device (OGD), a membrane electrode assembly (MEA), an impressed current cathodic protection anode (ICCP anode), and combinations thereof.

### Claim 6 (depends on 2)

The apparatus of claim 2, further comprising an anolyte re-circulation loop fluidically coupled to the electroplating cell, wherein the anolyte circulation loop comprises an anolyte storage reservoir connected to the anode chamber, and an anolyte recirculation pump that recirculates anolyte to the anode chamber.

### Claim 7 (depends on 6)

The apparatus of claim 6, wherein the oxidation device (ODD) comprises an oxygenation device (OGD), which OGD is disposed in the anolyte re-circulation loop and exposes the anolyte to oxygen.

### Claim 8 (depends on 7)

The apparatus of claim 7, wherein the OGD is placed in line with the anolyte recirculation pump.

### Claim 9 (depends on 7)

The apparatus of claim 7, wherein the OGD comprises a dwell tank fluidly coupled to the anode chamber.

### Claim 10 (depends on 7)

The apparatus of claim 7, wherein the OGD comprises an oxygen sparging device disposed in the anolyte storage reservoir.

### Claim 11 (depends on 7)

The apparatus of claim 7, wherein the OGD comprises a contractor or a membrane contractor.

### Claim 12 (depends on 7)

The apparatus of claim 7, wherein the anolyte re-circulation loop is configured to operate with a flow rate at about 0.25 liters per minute (lpm) to about 1 lpm.

### Claim 13 (depends on 7)

The apparatus of claim 7, wherein the source of oxygen is selected from the group consisting of atmospheric air, clean dry air, substantially pure oxygen, and combinations thereof.

### Claim 14 (depends on 7)

The apparatus of claim 7, further comprising an oxygen concentration meter that provides feedback for controlling oxygen concentration of the anolyte.

### Claim 15 (depends on 5)

The apparatus of claim 5, wherein the oxidation device (ODD) comprises a membrane electrode assembly (MEA) or an impressed current cathodic protection anode (ICCP anode) disposed in the electroplating cell.

### Claim 16 (depends on 15)

The apparatus of claim 15, wherein the MEA comprises a carbon cloth on the side of the MEA facing the electroplating anode, and the carbon cloth is electrically coupled to an electrical source for applying a bias relative to the electroplating anode.

### Claim 17 (depends on 16)

The apparatus of claim 16, wherein the carbon cloth has a thickness of about 50 microns to 1 millimeter.

### Claim 18 (depends on 16)

The apparatus of claim 16, wherein the carbon cloth is electrically coupled to an electrical source for applying a bias of about +0.25 to 0.75 V relative to the copper anode.

### Claim 19 (depends on 5)

The apparatus of claim 5, wherein the ICCP anode comprises platinum.

### Claim 20 (depends on 5)

The apparatus of claim 5, wherein the ICCP anode, when biased, is configured to generate oxygen by electrolyzing water.

### Claim 21 (depends on 5)

The apparatus of claim 5, wherein the electroplating anode comprises an active anode, and the ICCP anode, when biased, is configured to decrease the corrosion of the electroplating anode by reducing copper cations to copper at the electroplating anode.

### Claim 22 (depends on 1)

The apparatus of claim 1, further comprising a catholyte storage reservoir connected to the cathode chamber to provide a catholyte to the cathode chamber.

### Claim 23

A method of electroplating a metal onto a substrate, the method comprising:
(a) providing an anolyte in an anode chamber having an anode and being separated from a cathode chamber by a porous transport barrier that enables migration of ionic species, including metal cations, across the transport barrier while substantially blocking organic plating additives from diffusing across the transport barrier;
(b) providing a catholyte to the cathode chamber containing the substrate attached to a cathode electrical connection, wherein the catholyte contains a substantially greater concentration of the organic plating additives than the anolyte;
(c) oxidizing cations of the metal to be electroplated onto the substrate, which cations are present in the anolyte during electroplating; and
(d) applying a potential difference between the substrate and the anode, thereby plating the metal onto the substrate without substantially increasing the concentration of plating additives in the anolyte.

### Claim 24 (depends on 23)

The method of claim 23, wherein the metal to be electroplated onto the substrate is copper, the anolyte comprises one or more copper salts dissolved in a solvent, and the step of oxidizing cations of the metal comprises oxidizing Cu(I) to Cu(II).

### Claim 25 (depends on 24)

The method of claim 24, wherein the step of oxidizing cations of the metal comprises maintaining the oxygen concentration of the anolyte at about 0.05 ppm to 9 ppm.

### Claim 26 (depends on 24)

The method of claim 24, wherein the step of oxidizing cations of the metal comprises maintaining the oxygen concentration of the anolyte at about 0.5 ppm to 2 ppm.

### Claim 27 (depends on 24)

The method of claim 24, wherein the step of oxidizing cations of the metal comprises:
removing the anolyte from the anode chamber;
treating the anolyte by allowing the anolyte to contact oxygen, thereby increasing the oxygen concentration of the anolyte; and
re-introducing the treated anolyte to the anode chamber.

### Claim 28 (depends on 24)

The method of claim 24, wherein the step of oxidizing cations of the metal comprises biasing an impressed current cathodic protection anode (ICCP anode), thereby electrolyzing water in the anolyte to yield oxygen and/or reducing copper cations to copper at the anode to prevent corrosion of the anode.

### Claim 29 (depends on 28)

The method of claim 28, wherein biasing the ICCP anode comprises applying a current at about 1 μA/cm2 to 100 μA/cm2 to the ICCP anode for an electroplating process for a 300 mm substrate.

### Claim 30 (depends on 29)

The method of claim 29, wherein biasing the ICCP anode comprises applying a current at less than about 50 μA/cm2 to the ICCP anode for an electroplating process for a 300 mm substrate.

### Claim 31 (depends on 24)

The method of claim 24, wherein the step of oxidizing cations of the metal comprises biasing a membrane electrode assembly (MEA) and contacting Cu(I) with the MEA, thereby oxidizing Cu(I) to Cu(II).

### Claim 32 (depends on 24)

The method of claim 24, wherein the anolyte is controlled at a temperature of about 20° C. to 35° C.

### Claim 33 (depends on 32)

The method of claim 32, wherein the anolyte is controlled at a temperature of about 23° C. to 30° C.