# US 2013/0284558 A1 · Friction discs having a structured ceramic friction layer and method of manufacturing the friction discs

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284558 A1
- Document ID: US20130284558A1
- Status: Published application
- Kind: A1
- Application number: 13/930,564
- Filed: 2013-06-28
- Published: 2013-10-31
- Earliest claimed: 2010-12-28
- Assignees: Sgl Carbon SE
- Applicants: Sgl Carbon SE
- Inventors: ANDREAS KIENZLE; INGRID KRAETSCHMER
- Web page: https://patentgrep.com/patent/US20130284558A1

## CPC

- C04B 35/80: Fibres, filaments, whiskers, platelets, or the like
- C04B 35/573: obtained by reaction sintering {or recrystallisation}
- C04B 35/62873: {Carbon}
- C04B 35/76: Fibres, filaments, whiskers, platelets, or the like
- C04B 35/83: Carbon fibres in a carbon matrix
- C04B 37/005: {consisting of glass or ceramic material}
- C04B 37/008: {by means of an interlayer consisting of an organic adhesive, e.g. phenol resin or pitch}
- F16D 13/64: Clutch-plates; Clutch-lamellae (brake-plates, brake-lamellae F16D65/12)
- F16D 69/023: {Composite materials containing carbon and carbon fibres or fibres made of carbonizable material}
- C04B 2235/3813: Refractory metal borides
- C04B 2235/3826: Silicon carbides
- C04B 2235/425: Graphite
- C04B 2235/48: Organic compounds becoming part of a ceramic after heat treatment, e.g. carbonising phenol resins
- C04B 2235/522: Oxidic
- C04B 2235/5232: Silica or silicates other than aluminosilicates, e.g. quartz
- C04B 2235/524: Non-oxidic, e.g. borides, carbides, silicides or nitrides
- C04B 2235/5248: Carbon, e.g. graphite
- C04B 2235/5256: Two-dimensional, e.g. woven structures
- C04B 2235/5276: Whiskers, spindles, needles or pins
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2237/08: Non-oxidic interlayers
- C04B 2237/083: Carbide interlayers, e.g. silicon carbide interlayers
- C04B 2237/086: Carbon interlayers
- C04B 2237/363: Carbon
- C04B 2237/365: Silicon carbide
- C04B 2237/385: Carbon or carbon composite
- C04B 2237/61: Joining two substrates of which at least one is porous by infiltrating the porous substrate with a liquid, such as a molten metal, causing bonding of the two substrates, e.g. joining two porous carbon substrates by infiltrating with molten silicon
- F16D 2069/004: {Profiled friction surfaces, e.g. grooves, dimples}
- F16D 2200/0047: Ceramic composite, e.g. C/C composite infiltrated with Si or B, or ceramic matrix infiltrated with metal
- F16D 2200/0052: Carbon
- F16D 2200/006: containing fibres or particles
- F16D 2200/0082: Production methods therefor
- Y10T 156/10: Methods of surface bonding and/or assembly therefor
- Y10T 428/213: Frictional
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- F16D: COUPLINGS FOR TRANSMITTING ROTATION; CLUTCHES; BRAKES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A cylindrical ring-shaped friction disc contains a support body, at least one friction layer, and in each case an intermediate layer arranged between the support body and the friction layer. The intermediate layer has mutually adjoining flat regions with different coefficients of thermal expansion. A method teaches how to produce such a friction disc, and to the use the friction disc as parts of brake and clutch systems, in particular for motor vehicles.

## Claims

### Claim 1

A cylindrical annular friction disc, comprising:
a support body;
at least one friction layer; and
an intermediate layer disposed between each said support body and said friction layer, said intermediate layer having contiguous areal zones with differing coefficients of thermal expansion.

### Claim 2 (depends on 1)

The cylindrical annular friction disc according to claim 1, wherein a difference in the coefficients of thermal expansion of adjacent said areal zones with the different coefficients of thermal expansion is at least 5% of a respective higher value for a coefficient of linear thermal expansion.

### Claim 3 (depends on 1)

The cylindrical annular friction disc according to claim 1, wherein said areal zones in said intermediate layer have dimensions of at least 0.5 mm and not more than 10 mm in a plane parallel to a bottom surface or cover surface of the cylindrical annular friction disc.

### Claim 4 (depends on 1)

The cylindrical annular friction disc according to claim 1, wherein a difference in the coefficients of thermal expansion of adjacent said areal zones with the different coefficients of thermal expansion is at least 10% of a respective higher value for a coefficient of linear thermal expansion.

### Claim 5

A method for producing a cylindrical annular friction disc having a microstructure being planned and formed deliberately in a friction layer, which comprises the steps of:
preparing a preform for a support body of porous carbon;
preparing a preform for a friction layer body of porous carbon;
adhesively bonding at least one friction layer preform on the preform for the support body by means of an adhesive layer containing as an organic binder a thermosetting resin, and at least one additive selected from the group consisting of elemental carbon, carbides, nitrides and silicides of metals and semi-metals of groups 13, 14, and 15 according to the current IUPAC nomenclature of periodic table of elements, high temperature-resistant fibers selected from carbon fibers, fibers of binary and ternary compounds of elements Si, C, N, B, O, and P, and whiskers of refractory metals;
pyrolysing a resulting composite material in an absence of oxidizing agents, thereby obtaining carbon from the organic binder resulting in a carbonized composite;
infiltrating the carbonized composite with one of a liquid silicon or a liquid alloy containing a mass fraction of at least 50% silicon, thereby forming carbides of silicon and possibly of the other alloy components resulting in a siliconized composite; and
cooling the siliconized composite according to a selectable temperature profile in which an intermediate layer is formed from the adhesive layer by the steps of carbonization and infiltration with subsequent reaction to form carbides.

### Claim 6 (depends on 5)

The method according to claim 5, which further comprises forming the adhesive layer with the further steps of:
providing a carbon filament bundle mesh weave fabric with a plain weave impregnated or coated with an adhesive, and can be converted into carbon by heating in an absence of oxidizing substances to temperatures of about 800° C. or more;
performing an uneven application of the adhesive by one of screen printing or a computer-controlled applicator; and
solidifying the adhesive on an anti-adhesively treated smooth surface to form a film, from which a grid-shaped overlay is punched out, which later returns to an adhesive state under further heating before reaching a state of a cross-linked and non-melting thermoset.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the adhesive is a thermosetting resin or pitch, or a mixture thereof, and the adhesive also contains other additives of heat-resistant inorganic materials.

### Claim 8 (depends on 7)

The method according to claim 7, which further comprises providing heat-resistant inorganic materials as the additives, selected from the group consisting of powders of silicon carbide, boron carbide, titanium boride, boron nitride, and mixtures thereof.

### Claim 9 (depends on 6)

The method according to claim 6, which further comprises modifying the adhesive by performing one of
sprinkling in heat-resistant fibers selected from the group consisting of fibers of carbon, fibers of silicon carbide, fibers of silicon nitride, whiskers of ceramic materials, and whiskers of metallic materials; or
mixing in heat-resistant fibers selected from the group consisting of fibers of carbon, fibers of silicon carbide, fibers of silicon nitride, whiskers of ceramic materials, and whiskers of metallic materials with the adhesive in such manner that when the adhesive solidifies the heat-resistant fibers cause a formation of anisotropic structures.

### Claim 10 (depends on 5)

The method according to claim 5, wherein an average dimension of individual areal zones in a structure formed in the intermediate layer that are transformed by carbonization into carbon-containing layers with different coefficients of thermal expansion ranges from 2 mm to 8 mm.

### Claim 11 (depends on 10)

The method according to claim 10, wherein a thickness of the areal zones in the intermediate layer is between 0.2 mm and 2 mm in a carbonized state.

### Claim 12 (depends on 5)

The method according to claim 5, which further comprises:
reinforcing the preform for the support body of porous carbon with high-temperature-resistant fibers;
forming the preform for the friction layer body of porous carbon with silicon carbide as a filler; and
forming the adhesive layer with at least one of a pitch or a thermoplastic plastic.

### Claim 13 (depends on 6)

The method according to claim 6, which further comprises performing the uneven application of the adhesive to a form of a grid that intersects at right angles or in a form of a spider's web with concentric circles or spirals and radii that intersect the circles or the spirals.

### Claim 14

A system selected from the group consisting of a braking system and a clutch system, comprising:
a cylindrical annular friction disc containing a support body, at least one friction layer, and an intermediate layer disposed between each said support body and said friction layer, said intermediate layer having contiguous areal zones with differing coefficients of thermal expansion.

### Claim 15 (depends on 14)

The system according to claim 14, wherein the system is part of a motor vehicle.