# US 2013/0284518 A1 · Method of using multi-component fibers as lost-circulation material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284518 A1
- Document ID: US20130284518A1
- Status: Published application
- Kind: A1
- Application number: 13/833,807
- Filed: 2013-03-15
- Published: 2013-10-31
- Earliest claimed: 2012-04-27
- Assignees: 3M Innovative Properties Company
- Applicants: 3M Innovative Properties Company
- Inventors: Yong K. Wu; Keith A. Rutkowski; Clara E. Mata; Ignatius A. Kadoma; Michael D. Crandall
- Web page: https://patentgrep.com/patent/US20130284518A1

## CPC

- C09K 8/035: Organic additives
- E21B 21/003: {Means for stopping loss of drilling fluid (plastering the borehole wall E21B33/138)}
- C09K 2208/08: Fiber-containing well treatment fluids
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS

## Abstract

A method of forming a subterranean well and a method of reducing lost circulation in a subterranean well while drilling the subterranean well are disclosed. The methods include using multi-component fibers as lost-circulation materials. The multi-component fibers having external surfaces and include at least a first polymeric composition and a second polymeric composition. At least a portion of the external surfaces of the multi-component fibers includes the first polymeric composition, which at least partially adhesively bonds the mud cake formed during the method.

## Claims

### Claim 1

A method of forming a subterranean well, the method comprising:
drilling the subterranean well with a drilling mud comprising lost-circulation material; and
forming a mud cake comprising drill cuttings and the lost-circulation material, wherein the lost-circulation material comprises multi-component fibers having external surfaces and comprising at least a first polymeric composition and a second polymeric composition, wherein at least a portion of the external surfaces of the multi-component fibers comprises the first polymeric composition, and wherein the first polymeric composition at least partially adhesively bonds the mud cake.

### Claim 2 (depends on 1)

The method of claim 1, wherein the drilling mud comprises an oil-based drilling fluid comprising at least one of crude oil, diesel oil, biodiesel oil, kerosene, mineral oil, gasoline, naphtha, or toluene.

### Claim 3 (depends on 1)

The method of claim 1, wherein the drilling mud comprises an aqueous drilling fluid.

### Claim 4 (depends on 1)

The method of claim 1, wherein the multi-component fibers are non-fusing at a temperature encountered in the well.

### Claim 5 (depends on 1)

The method of claim 1, wherein the second polymeric composition has a melting point higher than a temperature encountered in the well.

### Claim 6 (depends on 1)

The method of claim 1, wherein the second polymeric composition comprises at least one of an ethylene-vinyl alcohol copolymer, a polyamide, a polyoxymethylene, a polypropylene, a polyester, a polyurethane, a polysulfone, a polyimide, a polyetheretherketone, or a polycarbonate.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first polymeric composition has an elastic modulus of less than 3×105 N/m2 at a temperature of at least 80° C. measured at a frequency of one hertz.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first polymeric composition comprises at least one of ethylene-vinyl alcohol copolymer, at least partially neutralized ethylene-methacrylic acid or ethylene-acrylic acid copolymer, polyurethane, polyoxymethylene, polypropylene, polyolefin, ethylene-vinyl acetate copolymer, polyester, polyamide, phenoxy, vinyl, or acrylic.

### Claim 9 (depends on 1)

The method of claim 1, wherein the first polymeric composition has a softening temperature of up to 150° C., wherein the second polymeric composition has a melting point of at least 130° C., and wherein the difference between the softening temperature of the first polymeric composition and the melting point of the second polymeric composition is at least 10° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the multi-component fiber further comprises a curable resin.

### Claim 11 (depends on 1)

The method of claim 1, wherein the lost-circulation material further comprises at least one of other fibers, different from the multi-component fibers, or particles.

### Claim 12

A method of reducing lost circulation in a subterranean well while drilling the subterranean well, the method comprising:
injecting a composition comprising lost-circulation material into the subterranean well through a drill pipe;
forming a mud cake comprising the lost-circulation material;
resuming drilling of the subterranean well after injecting the lost-circulation material, wherein the lost-circulation material comprises multi-component fibers having external surfaces and comprising at least a first polymeric composition and a second polymeric composition, wherein at least a portion of the external surfaces of the multi-component fibers comprises the first polymeric composition, and wherein the first polymeric composition at least partially adhesively bonds the mud cake.

### Claim 13 (depends on 12)

The method of claim 12, further comprising at least one of injecting a first spacer into the subterranean well before injecting the lost-circulation material into the subterranean well or injecting a second spacer into the subterranean well after injecting the lost-circulation material into the subterranean well and before resuming drilling.

### Claim 14 (depends on 12)

The method of claim 12, wherein the multi-component fibers are non-fusing at a temperature encountered in the well.

### Claim 15 (depends on 12)

The method of claim 12, wherein the second polymeric composition has a melting point higher than a temperature encountered in the well.

### Claim 16 (depends on 12)

The method of claim 12, wherein the second polymeric composition comprises at least one of an ethylene-vinyl alcohol copolymer, a polyamide, a polyoxymethylene, a polypropylene, a polyester, a polyurethane, a polysulfone, a polyimide, a polyetheretherketone, or a polycarbonate.

### Claim 17 (depends on 12)

The method of claim 12, wherein the first polymeric composition has an elastic modulus of less than 3×105 N/m2 at a temperature of at least 80° C. measured at a frequency of one hertz.

### Claim 18 (depends on 12)

The method of claim 12, wherein the first polymeric composition comprises at least one of ethylene-vinyl alcohol copolymer, at least partially neutralized ethylene-methacrylic acid or ethylene-acrylic acid copolymer, polyurethane, polyoxymethylene, polypropylene, polyolefin, ethylene-vinyl acetate copolymer, polyester, polyamide, phenoxy, vinyl, or acrylic.

### Claim 19 (depends on 12)

The method of claim 12, wherein the first polymeric composition has a softening temperature of up to 150° C., wherein the second polymeric composition has a melting point of at least 130° C., and wherein the difference between the softening temperature of the first polymeric composition and the melting point of the second polymeric composition is at least 10° C.

### Claim 20 (depends on 12)

The method of claim 12, wherein the lost-circulation material further comprises at least one of other fibers, different from the multi-component fibers, or particles.