# US 2013/0284439 A1 · Wide temperature range cement retarder

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284439 A1
- Document ID: US20130284439A1
- Status: Published application
- Kind: A1
- Application number: 13/458,718
- Filed: 2012-04-27
- Published: 2013-10-31
- Earliest claimed: 2012-04-27
- Assignees: Halliburton Energy Services, Inc.
- Inventors: Tushar Sureshgir Gosavi; Ramesh Muthusamy; Rahul Chandrakant Patil; Sandip Prabhakar Patil
- Web page: https://patentgrep.com/patent/US20130284439A1

## CPC

- C04B 24/2688: {Copolymers containing at least three different monomers}
- C04B 24/163: {obtained by reactions only involving carbon-to-carbon unsaturated bonds}
- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C09K 8/467: containing additives for specific purposes
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

According to an embodiment, a composition is provided that can be used in a cementing. The composition includes at least: (i) a hydraulic cement; and (ii) a copolymer comprising at least the monomeric units (a) through (d) of the following formula: wherein the monomeric units (a) through (d) can be any sequence and any proportion in the copolymer. With water, the composition of the hydraulic cement and such a copolymer becomes a cement composition. According to the method, the cement composition is introduced into a well and allowed to set in the well.

## Claims

### Claim 1

A composition comprising:
(i) a hydraulic cement; and
(ii) a copolymer comprising at least the monomeric units (a) through (d) of the following formula:
wherein the monomeric units (a) through (d) can be any sequence and any proportion in the copolymer.

### Claim 2 (depends on 1)

The composition according to claim 1, wherein the hydraulic cement is a cementitious material selected from the group consisting of Portland cements, pozzolanic cements, gypsum cements, phosphate cements, high alumina content cements, silica cements, high alkalinity cements, shale cements, acid/base cements, magnesia cements, fly ash cement, zeolite cement systems, cement kiln dust cement systems, slag cements, micro-fine cement, metakaolin, or combinations thereof.

### Claim 3 (depends on 1)

The composition according to claim 1, wherein the monomeric units (a) through (d) are acrylic acid, 2-acrylamido-2-methylpropane sulfonic acid sodium salt, 2-hydroxypropyl acrylate, and phosphinic acid, respectively.

### Claim 4 (depends on 1)

The composition according to claim 1, wherein the monomeric units (a) through (d) in the copolymer are in the following ranges:
(a) is in the range of 65 to 75% by weight;
(b) is in the range of 10 to 15% by weight;
(c) is in the range of 10 to 15% by weight; and
(d) is in the range of 3 to 7% by weight.

### Claim 5 (depends on 1)

The composition according to claim 1, wherein the concentration of the copolymer is between 0.05% by weight of the cement and 3% by weight of the cement.

### Claim 6 (depends on 1)

The composition according to claim 1, further comprising silica flour.

### Claim 7 (depends on 1)

The composition according to claim 1, further comprising a fluid-loss control additive.

### Claim 8 (depends on 7)

The composition according to claim 7, wherein the fluid-loss control additive is selected from the group consisting of: sulfonic acid copolymer, acrylamide copolymers, cellulosic polymers and derivatives thereof, and modified cellulosic polymers.

### Claim 9 (depends on 1)

The composition according to claim 1, further comprising a retarder intensifier.

### Claim 10 (depends on 9)

The composition according to claim 9, wherein the retarder intensifier is tartaric acid.

### Claim 11 (depends on 1)

The composition according to claim 1, further comprising water.

### Claim 12 (depends on 11)

The composition according to claim 11, wherein the composition has a thickening time of at least 2 hours at any temperature between 100° F. and 360° F.

### Claim 13

A method of cementing in a well, the method comprising the steps of:
(A) introducing a cement composition into the well, the cement composition comprising:
(i) a hydraulic cement;
(ii) a copolymer comprising at least the monomeric units (a) through (d) of the following formula:
wherein the monomeric units (a) through (d) can be any sequence and any proportion in the copolymer; and
(iii) water; and
(B) allowing the cement composition to set in the well.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the hydraulic cement is a cementitious material selected from the group consisting of Portland cements, pozzolanic cements, gypsum cements, phosphate cements, high alumina content cements, silica cements, high alkalinity cements, shale cements, acid/base cements, magnesia cements, fly ash cement, zeolite cement systems, cement kiln dust cement systems, slag cements, micro-fine cement, metakaolin, or combinations thereof.

### Claim 15 (depends on 13)

The composition according to claim 13, wherein the monomeric units (a) through (d) are acrylic acid, 2-acrylamido-2-methylpropane sulfonic acid sodium salt, 2-hydroxypropyl acrylate, and phosphinic acid, respectively.

### Claim 16 (depends on 13)

The method according to claim 13, wherein the monomeric units (a) through (d) in the copolymer are in the following ranges:
(a) is in the range of 65 to 75% by weight;
(b) is in the range of 10 to 15% by weight;
(c) is in the range of 10 to 15% by weight; and
(d) is in the range of 3 to 7% by weight.

### Claim 17 (depends on 13)

The method according to claim 13, wherein the concentration of the copolymer is between 0.05% by weight of the cement and 3% by weight of the cement.

### Claim 18 (depends on 13)

The method according to claim 13, wherein the cement composition further comprises silica flour.

### Claim 19 (depends on 13)

The method according to claim 13, further comprising a fluid-loss control additive.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the fluid-loss control additive is selected from the group consisting of: sulfonic acid copolymer, acrylamide copolymers, cellulosic polymers and derivatives thereof, and modified cellulosic polymers.

### Claim 21 (depends on 13)

The method according to claim 13, further comprising a retarder intensifier.

### Claim 22 (depends on 21)

The method according to claim 21, wherein the retarder intensifier is tartaric acid.

### Claim 23 (depends on 22)

The method according to claim 22, wherein the composition has a thickening time of at least 2 hours at any temperature between 100° F. and 360° F.