# US 2013/0284358 A1 · Halogen-Free Resin Composition And Method For Fabricating Halogen-Free Copper Clad Laminate Using The Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284358 A1
- Document ID: US20130284358A1
- Status: Published application
- Kind: A1
- Application number: 13/997,542
- Filed: 2011-09-03
- Published: 2013-10-31
- Earliest claimed: 2010-12-23
- Assignees: Guangdong Shengyi Sci. Tech Co., Ltd.
- Inventors: Yueshan He; Shiguo Su
- Web page: https://patentgrep.com/patent/US20130284358A1

## CPC

- H01B 3/40: epoxy resins
- B32B 5/024: {Woven fabric}
- B32B 15/14: next to a fibrous or filamentary layer
- C08J 5/244: {using glass fibres}
- C08L 63/00: Compositions of epoxy resins; Compositions of derivatives of epoxy resins
- H01B 19/04: Treating the surfaces, e.g. applying coatings
- B32B 2260/021: Fibrous or filamentary layer
- B32B 2260/046: Synthetic resin
- B32B 2262/101: Glass fibres
- C08J 2363/00: Characterised by the use of epoxy resins; Derivatives of epoxy resins
- C08J 2371/12: Polyphenylene oxides
- C08J 2379/04: Polycondensates having nitrogen-containing heterocyclic rings in the main chain; Polyhydrazides; Polyamide acids or similar polyimide precursors
- Y10T 156/1062: Prior to assembly
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention relate to a halogen-free resin composition and a method for fabricating a halogen-free copper clad laminate using the same. The halogen-free resin composition comprises the following components: reactive small molecular polyphenylene oxide with a number average molecular weight of 500-3000, a polybenzoxazine resin, a phosphorus-containing epoxy resin, a composite curing agent, a curing promoter, a filler, and a benzene or ketone solvent. The method for fabricating a halogen-free copper clad laminate comprises: Step 1: dissolving reactive small molecular polyphenylene oxide with a number average molecular weight of 500-3000 in a benzene or ketone solvent, adding a polybenzoxazine resin after dissolution, and mixing by stirring, to prepare a solution for use; Step 2: adding a phosphorus-containing epoxy resin, a composite curing agent, a curing promoter, and a filler to the solution for use, and stirring uniformly, to obtain a colloidal solution; Step 3: evenly coating the prepared colloidal solution to E-glass cloth with an even surface and baking, to produce a B-stage partially cured prepreg; and Step 4: cutting the B-stage partially cured prepreg into a suitable size according to the size of a compressor, precisely overlaying, placing a copper foil on and under the laminated B-stage partially cured Prepregs, and pressing in a vacuum hot pressing machine, to obtain a halogen-free copper clad laminate.

## Claims

### Claim 1

A halogen-free resin composition, comprising from 5 to 30 parts by weight of reactive small molecular polyphenylene oxide with a number average molecular weight of 500-3000, from 5 to 50 parts by weight of a polybenzoxazine resin, from 15 to 65 parts by weight of a phosphorus-containing epoxy resin, from 1 to 25 parts by weight of a composite curing agent, from 0 to 5 parts by weight of a curing promoter, from 0 to 100 parts by weight of a filler, and a suitable amount of benzene or ketone solvent.

### Claim 2 (depends on 1)

The halogen-free resin composition according to claim 1, wherein the reactive small molecular polyphenylene oxide has the following chemical structural formula
wherein m and n are 0-25, at least one of m and n is not 0; Y is selected from
X is alkyl, —S—, —O—,
R1, R2, R7, R8, R9, R10, R11, R15 and R16 are identical or different alkyl groups having a carbon atom number of less than 6 or phenyl; R3, R4, R5, R6, R12, R13 and R14 are identical or different, are hydrogen atom or alkyl groups having a carbon atom number or a number of less than 6 or phenyl;

### Claim 3 (depends on 1)

The halogen-free resin composition according to claim 1, wherein the polybenzoxazine resin comprises one or more selected from the group consisting of the following structures
wherein R2 and R3 are mono- or poly-substituted; R2 and R3 are H, methyl, allyl, alkynyl or aldehyde group; R1 is
R4 and R5 are each independently allyl, unsubstituted or substituted phenyl, unsubstituted or substituted C1-C8-alkyl, unsubstituted or substituted C1-C8-cycloalkyl.

### Claim 4 (depends on 1)

The halogen-free resin composition according to claim 1, wherein the basic epoxy resin in the phosphorus-containing epoxy resin is difunctional epoxy resin, polyfunctional epoxy resin, or mixture thereof, and has a sulfur content of 2-5%, and an epoxy equivalent of 200-600 g/mol.

### Claim 5 (depends on 1)

The halogen-free resin composition according to claim 1, wherein the composite curing agent is one or more selected from the group consisting of dicyandiamide, aromatic amine, anhydride, phenols and phosphorus-containing phenolic aldehyde.

### Claim 6 (depends on 1)

The halogen-free resin composition according to claim 1, wherein the curing promoter is one or more selected from the group consisting of 2-methylimidazole, 2-ethyl-4-methylimidazole, 2-phenylimidazole, DMP-30 and hexamethylenetetramine; the filler is an inorganic or organic filler, wherein the inorganic filler is one or more selected from the group consisting of aluminium hydroxide, magnesium hydroxide, zeolite, wollastonite, silica, magnesia, calcium silicate, calcium carbonate, clay, talc and mica.

### Claim 7 (depends on 1)

A method for fabricating a halogen-free copper clad laminate using the halogen-free resin composition according to claim 1, comprises:
Step 1: dissolving from 5 to 30 parts by weight of a reactive small molecular polyphenylene oxide with a number average molecular weight of 500-3000 in a benzene or ketone solvent, adding from 5 to 50 parts by weight of a polybenzoxazine resin after complete dissolution at normal temperature or moderate temperature, and mixing by stirring, to prepare a solution for use;
Step 2: adding from 15 to 65 parts by weight of a phosphorus-containing epoxy resin, from 1 to 25 parts by weight of a composite curing agent, from 0 to 5 parts by weight of a curing promoter, and from 0 to 100 parts by weight of a filler to the solution for use, and stirring uniformly, to obtain a colloidal solution;
Step 3: evenly coating the prepared colloidal solution to E-glass cloth with an even surface and baking, to produce a B-stage partially cured prepreg; and
Step 4: cutting the B-stage partially cured prepreg into a suitable size according to the size of a compressor, precisely overlaying, placing a copper foil on and under the laminated B-stage partially cured Prepregs, and pressing in a vacuum hot pressing machine, to obtain a halogen-free copper clad laminate.

### Claim 8 (depends on 7)

The method for fabricating a halogen-free copper clad laminate according to claim 7, characterized in that the moderate temperature in Step 1 ranges from 30-80° C.

### Claim 9 (depends on 7)

The method for fabricating a halogen-free copper clad laminate according to claim 7, wherein, during the baking of a B-stage partially cured prepreg, the baking is set up according to the boiling point of the solvent used for the colloidal solution to be 85-175° C. for 5-20 minutes.

### Claim 10 (depends on 7)

The method for fabricating a halogen-free copper clad laminate according to claim 7, wherein, in Step 4, the pressing is conducted by using bench pressing, having the specific steps of increasing from room temperature to 150° C. within 15 min, remaining for 30 min, increasing to 180° C. within 5 min, remaining for 2 h, finally decreasing to room temperature within 30 min; increasing the pressure from 0 to 0.6 Mpa within 1 min, remaining for 20 min, then increasing to 1.0 Mpa within 1 min, remaining for 2.5 h, post-processing at 200-245° C. and remaining for 0-5 h.