# US 2013/0284327 A1 · Copper alloy for electronic device, method of producing copper alloy for electronic device, and copper alloy rolled material for electronic device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284327 A1
- Document ID: US20130284327A1
- Status: Published application
- Kind: A1
- Application number: 13/990,939
- Filed: 2011-11-24
- Published: 2013-10-31
- Earliest claimed: 2010-12-03
- Assignees: Mitsubishi Materials Corporation
- Inventors: Kazunari Maki; Yuki Ito
- Web page: https://patentgrep.com/patent/US20130284327A1

## CPC

- H01B 1/026: {Alloys based on copper}
- C22C 9/01: with aluminium as the next major constituent
- C22F 1/08: of copper or alloys based thereon
- H01B 13/0016: {for heat treatment}
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

A copper alloy for an electric device contains Mg in a range of 1.3 atomic % or more and less than 2.6 atomic %, Al in a range of 6.7 atomic % or more and 20 atomic % or less, and the balance substantially consisting of Cu and unavoidable impurities. A method of producing a copper alloy includes: performing heating of a copper material to a temperature of not lower than 500° C. and not higher than 1000° C.; performing quenching to cool the heated copper material to 200° C. or lower with a cooling rate of 200° C./min or more; and performing working of the cooled copper material, wherein the copper material is composed of a copper alloy containing Mg in a range of 1.3 atomic % or more and less than 2.6 atomic %, Al in a range of 6.7 atomic % or more and 20 atomic % or less.

## Claims

### Claim 1

A copper alloy for an electric device containing Mg in a range of 1.3 atomic % or more and less than 2.6 atomic %, Al in a range of 6.7 atomic % or more and 20 atomic % or less, and the balance substantially consisting of Cu and unavoidable impurities.

### Claim 2 (depends on 1)

The copper alloy for an electronic device according to the claim 1, further containing one or more selected from Zn, Sn, Si, Mn, and Ni in an amount of 0.05% atomic % or more and 5 atomic % or less.

### Claim 3 (depends on 1)

The copper alloy for an electronic device according to claim 1, further containing one or more selected from B, P, Zr, Fe, Co, Cr, Ag, Ca, and rare earth elements in an amount of 0.01% atomic % or more and 1 atomic % or less.

### Claim 4 (depends on 1)

The copper alloy for an electronic device according to claim 1, wherein yield strength σ0.2 at 0.2% is 400 MPa or more.

### Claim 5 (depends on 1)

The copper alloy for an electronic device according to claim 1, wherein Young's modulus E is 125 GPa or less.

### Claim 6 (depends on 1)

The copper alloy for an electronic device according to claim 1, wherein average number of intermetallic compounds having a particle diameter of 0.1 μm or more is 10/μm2 or less under the observation using a scanning electron microscope

### Claim 7 (depends on 1)

A method of producing a copper alloy for an electronic device according to claim 1, comprising:
performing heating of a copper material to a temperature of not lower than 500° C. and not higher than 1000° C.;
performing quenching to cool the heated copper material to 200° C. or lower with a cooling rate of 200° C./min or more; and
performing working of the cooled copper material,
wherein the copper material is composed of a copper alloy containing Mg in a range of 1.3 atomic % or more and less than 2.6 atomic %, Al in a range of 6.7 atomic % or more and 20 atomic % or less, and the balance being substantially consisting of Cu and unavoidable impurities.

### Claim 8 (depends on 7)

The method of producing a copper alloy for an electronic device according to claim 7, wherein the copper alloy that composes the copper material further contains one or more selected from Zn, Sn, Si, Mn, and Ni in an amount of 0.05% atomic % or more and 5 atomic % or less.

### Claim 9 (depends on 7)

The method of producing a copper alloy for an electronic device according to claim 7, wherein the copper alloy that composes the copper material further contains one or more selected from B, P, Zr, Fe, Co, Cr, Ag, Ca, and rare earth elements in an amount of 0.01% atomic % or more and 1 atomic % or less.

### Claim 10 (depends on 1)

A copper alloy rolled material for an electronic device, comprising the copper alloy for an electronic device according to claim 1, wherein Young's modulus E in the rolling direction is 125 GPa or less and a yield strength σ0.2 at 0.2% in the rolling direction is 400 MPa or more.

### Claim 11 (depends on 10)

The copper alloy rolled material for an electronic device according to claim 10 that is used as terminals, connectors, or relays.

### Claim 12 (depends on 2)

The copper alloy for an electronic device according to claim 2, further containing one or more selected from B, P, Zr, Fe, Co, Cr, Ag, Ca, and rare earth elements in an amount of 0.01% atomic % or more and 1 atomic % or less.

### Claim 13 (depends on 2)

The copper alloy for an electronic device according to claim 2, wherein yield strength σ0.2 at 0.2% is 400 MPa or more.

### Claim 14 (depends on 2)

The copper alloy for an electronic device according to claim 2, wherein Young's modulus E is 125 GPa or less.

### Claim 15 (depends on 2)

The copper alloy for an electronic device according to claim 2, wherein average number of intermetallic compounds having a particle diameter of 0.1 μm or more is 10/μm2 or less under the observation using a scanning electron microscope

### Claim 16 (depends on 2)

A method of producing a copper alloy for an electronic device according to claim 2, comprising:
performing heating of a copper material to a temperature of not lower than 500° C. and not higher than 1000° C.;
performing quenching to cool the heated copper material to 200° C. or lower with a cooling rate of 200° C./min or more; and
performing working of the cooled copper material,
wherein the copper material is composed of a copper alloy containing Mg in a range of 1.3 atomic % or more and less than 2.6 atomic %, Al in a range of 6.7 atomic % or more and 20 atomic % or less, and the balance being substantially consisting of Cu and unavoidable impurities.

### Claim 17 (depends on 16)

The method of producing a copper alloy for an electronic device according to claim 16, wherein the copper alloy that composes the copper material further contains one or more selected from Zn, Sn, Si, Mn, and Ni in an amount of 0.05% atomic % or more and 5 atomic % or less.

### Claim 18 (depends on 8)

The method of producing a copper alloy for an electronic device according to claim 8, wherein the copper alloy that composes the copper material further contains one or more selected from B, P, Zr, Fe, Co, Cr, Ag, Ca, and rare earth elements in an amount of 0.01% atomic % or more and 1 atomic % or less.

### Claim 19 (depends on 2)

A copper alloy rolled material for an electronic device, comprising the copper alloy for an electronic device according to claim 2, wherein Young's modulus E in the rolling direction is 125 GPa or less and a yield strength σ0.2 at 0.2% in the rolling direction is 400 MPa or more.

### Claim 20 (depends on 19)

The copper alloy rolled material for an electronic device according to claim 19 that is used as terminals, connectors, or relays.