# US 2013/0284326 A1 · Nickel-titanium-rare earth alloy and method of processing the alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284326 A1
- Document ID: US20130284326A1
- Status: Published application
- Kind: A1
- Application number: 13/863,760
- Filed: 2013-04-16
- Published: 2013-10-31
- Earliest claimed: 2009-11-17
- Assignees: Cook Medical Technologies LLC; University of Limerick
- Inventors: Syed A.M. Tofail; James M. Carlson; Abbasi A. Gandhi; James Butler; Peter Tiernan; Lisa O'Donoghue
- Web page: https://patentgrep.com/patent/US20130284326A1

## CPC

- C22F 1/10: of nickel or cobalt or alloys based thereon
- C22C 14/00: Alloys based on titanium
- C22C 19/03: based on nickel
- C22F 1/183: {of titanium or alloys based thereon}
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A nickel-titanium-rare earth (Ni—Ti-RE) alloy comprises nickel at a concentration of from about 35 at. % to about 65 at. %, a rare earth element at a concentration of from about 1.5 at. % to about 15 at. %, boron at a concentration of up to about 0.1 at. %, with the balance of the alloy being titanium. In addition to enhanced radiopacity compared to binary Ni—Ti alloys and improved workability, the Ni—Ti-RE alloy preferably exhibits superelastic behavior. A method of processing a Ni—Ti-RE alloy includes providing a nickel-titanium-rare earth alloy comprising nickel at a concentration of from about 35 at. % to about 65 at. %, a rare earth element at a concentration of from about 1.5 at. % to about 15 at. %, the balance being titanium; heating the alloy in a homogenization temperature range below a critical temperature; and forming spheroids of a rare earth-rich second phase in the alloy while in the homogenization temperature range.

## Claims

### Claim 1

A method of processing a nickel-titanium-rare earth alloy, the method comprising:
providing a nickel-titanium-rare earth alloy comprising nickel at a concentration of from about 34 at. % to about 60 at. %, titanium at a concentration of 34 at. % to about 60 at. %, and at least one rare earth element at a concentration of from about 0.1 at. % to about 15 at. %;
heating the nickel-titanium-rare earth alloy in a homogenization temperature range below a critical temperature; and
forming spheroids of a rare earth-rich second phase in the nickel-titanium-rare earth alloy while in the homogenization temperature range.

### Claim 2 (depends on 1)

The method of claim 1, wherein the critical temperature is an incipient melting temperature of the rare earth-rich second phase.

### Claim 3 (depends on 1)

The method of claim 1, wherein the rare earth element comprises Er and the critical temperature is about 925° C.

### Claim 4 (depends on 3)

The method of claim 3, wherein the homogenization temperature range is from about 750° C. to about 875° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein forming the spheroids includes keeping the nickel-titanium-rare earth alloy in the homogenization temperature range over a time duration of from about 24 h to about 72 h.

### Claim 6 (depends on 1)

The method of claim 1, further comprising thermal cycling the nickel-titanium-rare earth alloy.

### Claim 7 (depends on 1)

The method of claim 1, further comprising hot working the alloy.

### Claim 8 (depends on 7)

The method of claim 7, wherein the hot working comprises applying pressure to the alloy at an elevated temperature below the critical temperature after the heating.

### Claim 9 (depends on 8)

The method of claim 8, wherein the elevated temperature is within the homogenization temperature range.

### Claim 10 (depends on 7)

The method of claim 7, further comprising, after hot working, cold working the alloy.

### Claim 11 (depends on 10)

The method of claim 10, wherein the alloy is cold worked to achieve at least a 30% reduction in dimension without cracking.

### Claim 12 (depends on 1)

The method of claim 1, wherein the rare earth element is selected from the group consisting of: La, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, and Lu.

### Claim 13 (depends on 12)

The method of claim 12, wherein the alloy comprises nickel at a concentration of from about 45 at. % to about 55 at. %; erbium at a concentration of from about 4.5 at. % to about 6 at. %; boron at a concentration of from about 0.005 at. % to about 0.1 at. %.; the balance being titanium, wherein the alloy has a radiopacity greater than that of a binary nickel-titanium alloy.

### Claim 14 (depends on 1)

The method of claim 1, wherein the alloy comprises nickel at a concentration of about 40 at. % to about 60 at. % and the rare earth element at a concentration of from about 1.5 at. % to about 12 at. %.

### Claim 15 (depends on 14)

The method of claim 14, wherein the alloy further includes boron at a concentration of up to about 0.1 at. %.