# US 2013/0284324 A1 · Steel Sheet for an Oil Sand Slurry Pipe Having Excellent Abrasion Resistance, Corrosion Resistance, and Low-Temperature Toughness and Method for Manufacturing Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284324 A1
- Document ID: US20130284324A1
- Status: Published application
- Kind: A1
- Application number: 13/996,563
- Filed: 2011-12-21
- Published: 2013-10-31
- Earliest claimed: 2010-12-23
- Assignees: Posco
- Inventors: Seong-Ung Koh; Hwan-Gyo Jung
- Web page: https://patentgrep.com/patent/US20130284324A1

## CPC

- C21D 8/0263: {following hot rolling}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 9/46: for sheet metals
- C22C 38/001: {containing N}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/58: with more than 1.5% by weight of manganese
- C21D 8/0226: {Hot rolling}
- C21D 9/14: wear-resistant or pressure-resistant pipes
- C21D 2211/005: Ferrite
- C21D 2211/009: Pearlite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided is a steel sheet for an oil sand slurry pipe having excellent abrasion resistance, corrosion resistance, and low-temperature toughness including 0.2 wt % to 0.35 wt % of carbon (C), 0.1 wt % to 0.5 wt % of silicon (Si), 0.5 wt % to 1.8 wt % of manganese (Mn), 0.1 wt % to 0.6 wt % of nickel (Ni), 0.005 wt % to 0.05 wt % of niobium (Nb), 0.005 wt % to 0.02 wt % of titanium (Ti), 0.03 wt % or less of phosphorous (P), 0.03 wt % or less of sulfur (S), 0.05 wt % or less (excluding 0 wt %) of aluminum (Al), 0.01 wt % or less (excluding 0 wt %) of nitrogen (N), and iron (Fe) as well as other unavoidable impurities as a remainder.

## Claims

### Claim 1

A steel sheet for an oil sand slurry pipe having excellent abrasion resistance, corrosion resistance, and low-temperature toughness, the steel sheet comprising:
0.2 wt % to 0.35 wt % of carbon (C);
0.1 wt % to 0.5 wt % of silicon (Si);
0.5 wt % to 1.8 wt % of manganese (Mn);
0.1 wt % to 0.6 wt % of nickel (Ni);
0.005 wt % to 0.05 wt % of niobium (Nb);
0.005 wt % to 0.02 wt % of titanium (Ti);
0.03 wt % or less of phosphorous (P);
0.03 wt % or less of sulfur (S);
0.05 wt % or less (excluding 0 wt %) of aluminum (Al);
0.01 wt % or less (excluding 0 wt %) of nitrogen (N); and
iron (Fe) as well as other unavoidable impurities as a remainder.

### Claim 2 (depends on 1)

The steel sheet for an oil sand slurry pipe having excellent abrasion resistance, corrosion resistance, and low-temperature toughness of claim 1, further comprising 0.1 wt % to 1.0 wt % or less (excluding 0 wt %) of chromium (Cr),
wherein a sum of Mn and Cr is 2 wt % or less.

### Claim 3 (depends on 2)

The steel sheet for an oil sand slurry pipe having excellent abrasion resistance, corrosion resistance, and low-temperature toughness of claim 2, wherein a sum of Mn, Cr, and Ni in the steel sheet is 2.5 wt % or less.

### Claim 4 (depends on 1)

The steel sheet for an oil sand slurry pipe having excellent abrasion resistance, corrosion resistance, and low-temperature toughness of claim 1, wherein a microstructure of the steel sheet is composed of 50 area % to 80 area % of pearlite and ferrite as a remainder.

### Claim 5 (depends on 4)

The steel sheet for an oil sand slurry pipe having excellent abrasion resistance, corrosion resistance, and low-temperature toughness of claim 4, wherein a spacing between pearlite grains is 200 μm or less.

### Claim 6 (depends on 5)

The steel sheet for an oil sand slurry pipe having excellent abrasion resistance, corrosion resistance, and low-temperature toughness of claim 5, wherein a Vickers hardness value of the steel sheet is in a range of 180 Hv to 220 Hv.

### Claim 7

A method of manufacturing a steel sheet for an oil sand slurry pipe having excellent abrasion resistance, corrosion resistance, and low-temperature toughness, the method comprising:
finish hot rolling a steel slab including 0.2 wt % to 0.35 wt % of carbon (C), 0.1 wt % to 0.5 wt % of silicon (Si), 0.5 wt % to 1.8 wt % of manganese (Mn), 0.1 wt % to 0.6 wt % of nickel (Ni), 0.005 wt % to 0.05 wt % of niobium (Nb), 0.005 wt % to 0.02 wt % of titanium (Ti), 0.03 wt % or less of phosphorous (P), 0.03 wt % or less of sulfur (S), 0.05 wt % or less (excluding 0 wt %) of aluminum (Al), 0.01 wt % or less (excluding 0 wt %) of nitrogen (N), and iron (Fe) as well as other unavoidable impurities as a remainder at a residual reduction rate of 50% or more and a temperature ranging from Ar3 to Ar3+200° C.; and
then cooling at a cooling rate ranging from 0.2° C./sec to 4° C./sec.

### Claim 8 (depends on 7)

The method of claim 7, wherein the steel slab further comprises 0.1 wt % to 1.0 wt % or less (excluding 0 wt %) of chromium (Cr) and a sum of Mn and Cr is 2 wt % or less.

### Claim 9 (depends on 8)

The method of claim 8, wherein a sum of Mn, Cr, and Ni in the steel slab is 2.5 wt % or less.

### Claim 10 (depends on 7)

The method of claim 7, wherein the cooling is initiated at a temperature ranging from Ar3 to Ar3+200° C. and is terminated at a temperature of 500° C. or less.

### Claim 11 (depends on 2)

The steel sheet for an oil sand slurry pipe having excellent abrasion resistance, corrosion resistance, and low-temperature toughness of claim 2, wherein a microstructure of the steel sheet is composed of 50 area % to 80 area % of pearlite and ferrite as a remainder.

### Claim 12 (depends on 3)

The steel sheet for an oil sand slurry pipe having excellent abrasion resistance, corrosion resistance, and low-temperature toughness of claim 3, wherein a microstructure of the steel sheet is composed of 50 area % to 80 area % of pearlite and ferrite as a remainder.

### Claim 13 (depends on 8)

The method of claim 8, wherein the cooling is initiated at a temperature ranging from Ar3 to Ar3+200° C. and is terminated at a temperature of 500° C. or less.

### Claim 14 (depends on 9)

The method of claim 9, wherein the cooling is initiated at a temperature ranging from Ar3 to Ar3+200° C. and is terminated at a temperature of 500° C. or less.