# US 2013/0284323 A1 · Cu-Co-Si-Zr ALLOY MATERIAL AND MANUFACTURING METHOD THEREOF

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284323 A1
- Document ID: US20130284323A1
- Status: Published application
- Kind: A1
- Application number: 13/979,103
- Filed: 2012-01-12
- Published: 2013-10-31
- Earliest claimed: 2011-01-13
- Assignees: JX Nippon Mining & Metals Corporation
- Inventors: Yasuhiro Okafuji
- Web page: https://patentgrep.com/patent/US20130284323A1

## CPC

- C22F 1/08: of copper or alloys based thereon
- C22C 9/06: with nickel or cobalt as the next major constituent
- H01B 1/026: {Alloys based on copper}
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})

## Abstract

The present invention relates to a Cu—Co—Si—Zr alloy material which contains 1.0-2.5 wt % of Co, 0.2-0.7 wt % of Si and 0.001-0.5 wt % of Zr with the elemental ratio Co/Si being 3.5-5.0. The Cu—Co—Si—Zr alloy material contains second phase particles having a diameter of 0.20 μm or more but less than 1.00 μm at a density of 3,000-500,000 particles/mm2, and has a crystal grain size of 10 μm or less, an electrical conductivity of 60% IACS or more and good bending workability. The alloy material can be produced by setting the temperature of heating that is carried out after casting and before a solution heat treatment to a temperature that is higher than the later-described solution heat treatment temperature by 45° C. or more, by setting the cooling rate from the start temperature of hot rolling to 600° C. to 100° C./min or less, and by selecting the solution heat treatment temperature from (50× Co wt %+775)° C. to (50× Co wt %+825)° C. (inclusive). The aging treatment after the solution heat treatment is preferably carried out at 450-650° C. for 1-20 hours.

## Claims

### Claim 1

A Cu—Co—Si—Zr alloy material with good bending workability wherein said material comprises: 1.0 to 2.5 wt % of Co; 0.2 to 0.7 wt % of Si; and 0.001 to 0.5 wt % of Zr, and wherein a Co/Si elemental ratio is 3.5 to 5.0 and wherein said material contains 3,000 to 500,000 second phase particles per mm2 having diameters of from 0.20 μm or more to less than 1.00 μm, and has an electrical conductivity EC of 60% IACS or more, and a grain size of 10 μm or less.

### Claim 2 (depends on 1)

The copper alloy material of claim 1 containing 10 to 2,000 second phase particles per mm2 having diameters of from 1.00 μm or more to 10.00 μm or less.

### Claim 3 (depends on 1)

The copper alloy material of claim 1, wherein the 0.2% yield strength YS is 600 MPa or more.

### Claim 4 (depends on 1)

A method of manufacturing the copper alloy material of claim 1, wherein the temperature of hot rolling (hot heating) performed after casting and before solution treatment is a temperature that is 45° C. or more higher than the solution treatment temperature selected below, the cooling rate from the temperature at the start of hot rolling to 600° C. is 100° C./min or lower, and the solution treatment temperature is selected from the range of from (50× Co wt %+775)° C. or more to (50× Co wt %+825)° C. or less.

### Claim 5 (depends on 4)

The method of manufacturing the copper alloy material of claim 4, wherein the aging treatment after solution treatment is at 450 to 650° C. for 1 to 20 hours.