# US 2013/0284322 A1 · Thick products made of 7xxx alloy and manufacturing process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284322 A1
- Document ID: US20130284322A1
- Status: Published application
- Kind: A1
- Application number: 13/994,097
- Filed: 2011-12-06
- Published: 2013-10-31
- Earliest claimed: 2010-12-14
- Assignees: Constellium Valais SA; Constellium France
- Inventors: Cedric Gasqueres; Jean-Etienne Fournier
- Web page: https://patentgrep.com/patent/US20130284322A1

## CPC

- C22F 1/053: of alloys with zinc as the next major constituent
- C22C 21/00: Alloys based on aluminium
- C22C 21/10: with zinc as the next major constituent
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present invention relates to an aluminum alloy for the manufacture of thick blocks comprising (as a percentage by weight), Zn: 5.3-5.9%, Mg: 0.8-1.8%, Cu: <0.2%, Zr: 0.05 to 0.12%, Ti<0.15%, Mn<0.1%, Cr<0.1%, Si<0.15%, Fe<0.20%, impurities having an individual content of <0.05% each and <0.15% in total, the rest aluminum, The alloy may be used in a process comprising the steps of: (a) casting a thick block of an alloy according to the invention (b) solution heat treating said cast block at a temperature of 500 to 560° C. for 10 minutes to 20 hours, (c) cooling said solution heat treated block to a temperature below 100° C., (d) tempering said solution heat treated and cooled block by heating to 120 to 170° C. for 4 to 48 hours, In this process, said block is not subjected to any significant deformation by working between the casting and the tempering. The alloy and the method according to the invention are particularly useful for the manufacture of molds for injection-molding plastics.

## Claims

### Claim 1

An aluminum alloy for manufacturing thick blocks comprising (as a percentage by weight);
Zn: 5.3-5.9%,
Mg: 0.8-1.8%,
Cu: <0.2%,
Zr: 0.05-0.12%,
Ti: <0.15%,
Mn: <0.1%,
Cr: <0.1%,
Si: <0.15%,
Fe: <0.20%;
impurities with individual content <0.05% each and <0.15% of the total, rest aluminum.

### Claim 2 (depends on 1)

The alloy according to claim 1, comprising (as a percentage by weight):
Zn: 5.4-5.8% and/or
Mg: 1.0-−1.4% and/or
Cu: <0.05%.

### Claim 3 (depends on 1)

The alloy according to claim 1, wherein maximum Zr content is 0.10% by weight and optionally 0.08% by weight.

### Claim 4 (depends on 1)

The alloy according to claim 1, in which
Ti: 0.01-0.05% and/or
Mn: <0.05% and/or:
Cr: <0.05% and/or:
Si: <0.10% and/or:
Fe: <0.15%,

### Claim 5 (depends on 1)

A method of manufacturing a thick block of aluminum comprising:
(a) casting a rough alloy shape according to claim 1.
(b) optionally homogenizing at a temperature of from 450 to 550° C. for a period of from 10 minutes to 30 hours and/or stress-relieving at a temperature of from 300 to 400° C. for a period of from 10 minutes to 30 hours followed by cooling to a temperature of not more than 100° C.;
(c) solution heat treating said cast block at a temperature of from 500 to 560° C. for 10 minutes to 20 hours,
(d) cooling said solution heat treated block to a temperature of not more than 100° C.,
(e) tempering said solution heat treated and cooled block by heating to from 120 to 170° C. for 4 to 48 hours,
wherein said block is not subjected to any significant deformation by working between the casting and the tempering.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the cooling of (c) is carried out with a cooling rate of at least 800° C./h, and wherein the solution heat treated block is stress-relieved and cooled by controlled compression with a permanent deformation ranging from 1% to 5% and optionally from 2 to 4%.

### Claim 7 (depends on 6)

The method according to claim 6, comprising immersion in water carried out by immersing in water at at least 50° C., and optionally at at least 70° C.

### Claim 8 (depends on 6)

A thick block of aluminum obtainable by the process according to claim 6, wherein at ¼ thickness in direction TL, yield strength RP0.2 and a ratio called NSR between the mechanical strength on a notched bar and the yield strength RP0.2 measured according to ASTM E602-03, section 9.2 are such that:
NSR>−0.017*Rp0.2+6.7 and
Rp0.2>320 MPa, optionally 330 MPa.

### Claim 9 (depends on 8)

A thick aluminum block according to claim 8, wherein NSR>0.8, optionally 1.0.

### Claim 10 (depends on 8)

A thick block according to claim 8, capable of being used for manufacturing molds for injection-molding plastics.