# US 2013/0284266 A1 · Electronic device and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284266 A1
- Document ID: US20130284266A1
- Status: Published application
- Kind: A1
- Application number: 13/928,679
- Filed: 2013-06-27
- Published: 2013-10-31
- Earliest claimed: 2010-12-27
- Assignees: Asahi Glass Company, Limited
- Applicants: Asahi Glass Company, Limited
- Inventors: Satoshi TAKEDA; Kazuo Yamada; Toshihiro Takeuchi; Yoko Mitsui; Hiroyuki Yamamoto
- Web page: https://patentgrep.com/patent/US20130284266A1

## CPC

- C03C 27/06: Joining glass to glass by processes other than fusing (fusing C03B23/20; units for use as elements for closing wall or like openings and comprising two or more parallel glass panes in spaced relationship, the panes being permanently secured together E06B3/66)
- H10F 19/807: {Double-glass encapsulation, e.g. photovoltaic cells arranged between front and rear glass sheets}
- H10F 77/169: Thin semiconductor films on metallic or insulating substrates
- H10F 77/1694: {the films including Group I-III-VI materials, e.g. CIS or CIGS}
- H10F 77/1696: {the films including Group II-VI materials, e.g. CdTe or CdS}
- H10F 77/50: Encapsulations or containers (for photovoltaic modules H10F19/80)
- H10K 59/8722: {Peripheral sealing arrangements, e.g. adhesives, sealants}
- Y02E 10/541: CuInSe2 material PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An electronic device 1 includes a first glass substrate 2, a second glass substrate 3, and an electronic element part 4 provided between these glass substrates 2, 3. The electronic element part 4 provided between the first and second glass substrates 2, 3 is sealed with a sealing layer 9 made up of a molten fixed layer of a sealing glass material having an electromagnetic wave absorption ability. At least one of the first and second glass substrates 2, 3 is made up of a chemically tempered glass having a surface compressive stress value of 900 MPa or less.

## Claims

### Claim 1

An electronic device, comprising:
a first glass substrate having a first surface including a first sealing region;
a second glass substrate having a second surface including a second sealing region corresponding to the first sealing region, and disposed with a predetermined gap above the first glass substrate such that the second surface faces the first surface;
an electronic element part provided between the first glass substrate and the second glass substrate; and
a sealing layer formed between the first sealing region of the first glass substrate and the second sealing region of the second glass substrate to seal the electronic element part, and made up of a molten fixed layer of a sealing glass material having an electromagnetic wave absorption ability,
wherein at least one of the first glass substrate and the second glass substrate is made up of a chemically tempered glass having a surface compressive stress value of 900 MPa or less.

### Claim 2 (depends on 1)

The electronic device according to claim 1,
wherein a central tension stress value of the chemically tempered glass is 70 MPa or less.

### Claim 3 (depends on 1)

The electronic device according to claim 1,
wherein the surface compressive stress value of the chemically tempered glass is in a range of 300 MPa or more and 900 MPa or less.

### Claim 4 (depends on 1)

The electronic device according to claim 1,
wherein a thickness of the glass substrate made up of the chemically tempered glass is 4 mm or less.

### Claim 5 (depends on 1)

The electronic device according to claim 1,
wherein the sealing glass material contains a sealing glass made up of a low-melting glass, an electromagnetic wave absorbing material of 0.1 vol % to 10 vol %, and a low-expansion filler of “0” (zero) vol % to 50 vol %.

### Claim 6 (depends on 5)

The electronic device according to claim 5,
wherein a standard deviation of a total area ratio of the low-expansion filler and the electromagnetic wave absorbing material existing per unit area of each of cross sections is 5% or less when the cross sections at arbitrary 20 points of the sealing layer are observed.

### Claim 7 (depends on 5)

The electronic device according to claim 5,
wherein a line width distribution of the sealing layer is within ±20% when the sealing layer is planarly observed.

### Claim 8 (depends on 5)

The electronic device according to claim 5,
wherein the sealing glass is made up of a bismuth-based glass containing Bi2O3 for 70% to 90%, ZnO for 1% to 20%, and B2O3 for 2% to 12% in mass fraction.

### Claim 9 (depends on 1)

The electronic device according to claim 1,
wherein the electronic element part includes a solar cell element.

### Claim 10

A manufacturing method of an electronic device, comprising:
preparing a first glass substrate having a first surface including a first sealing region;
preparing a second glass substrate having a second surface including a second sealing region corresponding to the first sealing region and a sealing material layer formed on the second sealing region and made up of a baked layer of a sealing glass material having an electromagnetic wave absorption ability;
laminating the first glass substrate and the second glass substrate via the sealing material layer while facing the first surface and the second surface; and
forming a sealing layer sealing an electronic element part provided between the first glass substrate and the second glass substrate by irradiating an electromagnetic wave and locally heating the sealing material layer through the first glass substrate or the second glass substrate to melt and solidify the sealing material layer,
wherein at least one of the first glass substrate and the second glass substrate is made up of a chemically tempered glass having a surface compressive stress value of 900 MPa or less.

### Claim 11 (depends on 10)

The manufacturing method of the electronic device according to claim 10,
wherein a central tension stress value of the chemically tempered glass is 70 MPa or less.

### Claim 12 (depends on 10)

The manufacturing method of the electronic device according to claim 10,
wherein the surface compressive stress value of the chemically tempered glass is within a range of 300 MPa or more and 900 MPa or less.

### Claim 13 (depends on 10)

The manufacturing method of the electronic device according to claim 10,
wherein a thickness of the glass substrate made up of the chemically tempered glass is 4 mm or less.

### Claim 14 (depends on 10)

The manufacturing method of the electronic device according to claim 10,
wherein the preparing the second glass substrate comprises:
preparing a sealing material paste including a mixture of the sealing glass material containing: a sealing glass made up of a low-melting glass; an electromagnetic wave absorbing material of 0.1 vol % to 10 vol %; and a low-expansion filler of “0” (zero) vol % to 50 vol %, and a vehicle;
baking a coating layer formed by coating the sealing material paste at the second sealing region of the second glass substrate to form the sealing material layer.

### Claim 15 (depends on 14)

The manufacturing method of the electronic device according to claim 14,
wherein a film thickness distribution of the sealing material layer in a surface of the glass substrate is within ±20%.

### Claim 16 (depends on 14)

The manufacturing method of the electronic device according to claim 14,
wherein the electromagnetic wave absorbing material and the low-expansion filler are dispersed in the sealing material paste such that a standard deviation of a total area ratio of the low-expansion filler and the electromagnetic wave absorbing material existing per unit area of each of cross sections is 5% or less when the cross sections at arbitrary 20 points of the sealing layer are observed.

### Claim 17 (depends on 14)

The manufacturing method of the electronic device according to claim 14,
wherein a laser light is irradiated while scanning along the sealing material layer as the electromagnetic wave.

### Claim 18 (depends on 10)

The manufacturing method of the electronic device according to claim 10,
wherein the electronic element part includes a solar cell element.

### Claim 19

A manufacturing method of an electronic device, comprising:
preparing a first glass substrate having a first surface including a first sealing region;
preparing a second glass substrate having a second surface including a second sealing region corresponding to the first sealing region;
preparing a sealing material paste including a mixture of a sealing glass material containing: a sealing glass made up of a low-melting glass; an electromagnetic wave absorbing material of 0.1 vol % to 10 vol %; and a low-expansion filler of “0” (zero) vol % to 50 vol %, and a vehicle;
baking a coating layer formed by coating the sealing material paste at the second sealing region of the second glass substrate to form the sealing material layer of which film thickness distribution is within ±20%;
laminating the first glass substrate and the second glass substrate via the sealing material layer while facing the first surface and the second surface; and
forming a sealing layer sealing an electronic element part provided between the first glass substrate and the second glass substrate by irradiating an electromagnetic wave and locally heating the sealing material layer through the first glass substrate or the second glass substrate to melt and solidify the sealing material layer,
wherein at least one of the first glass substrate and the second glass substrate is made up of a chemically tempered glass, and
wherein the sealing material paste in which the electromagnetic wave absorbing material and the low-expansion filler are uniformly dispersed is used such that a standard deviation of a total area ratio of the low-expansion filler and the electromagnetic wave absorbing material existing per unit area of each of cross sections is 5% or less when the cross sections at arbitrary 20 points of the sealing layer are observed.

### Claim 20 (depends on 19)

The manufacturing method of the electronic device according to claim 19,
wherein a laser light is irradiated while scanning along the sealing material layer as the electromagnetic wave.