# US 2013/0284160 A1 · Method for manufacturing hexagonal semiconductor plate crystal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284160 A1
- Document ID: US20130284160A1
- Status: Published application
- Kind: A1
- Application number: 13/930,323
- Filed: 2013-06-28
- Published: 2013-10-31
- Earliest claimed: 2010-12-28
- Assignees: Mitsubishi Chemical Corporation
- Applicants: Mitsubishi Chemical Corporation
- Inventors: Hirofumi UCHIDA; Yukio OKANO
- Web page: https://patentgrep.com/patent/US20130284160A1

## CPC

- B28D 5/045: {by cutting with wires or closed-loop blades (B28D5/042 takes precedence)}
- B24B 27/0633: {using a cutting wire}
- C30B 29/403: {AIII-nitrides}
- C30B 29/406: {Gallium nitride}
- C30B 29/64: Flat crystals, e.g. plates, strips or discs
- C30B 33/06: Joining of crystals
- B28D: WORKING STONE OR STONE-LIKE MATERIALS
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A method of efficiently manufacturing a hexagonal semiconductor plate crystal with small warpage is provided. The method of manufacturing a hexagonal semiconductor plate crystal is a method of manufacturing a hexagonal semiconductor plate crystal by cutting a hexagonal semiconductor crystal using a crystal cutting wire, wherein the hexagonal semiconductor crystal is cut by causing the crystal cutting wire to move relative to the hexagonal semiconductor crystal so as to satisfy the conditions of 25°<α≦90° and β=90°±5° where α represents an angle formed by the c axis of the hexagonal semiconductor crystal and the normal line of the crystal face cut out by the wire and β represents an angle formed by a reference axis, which is obtained by perpendicularly projecting the c axis of the hexagonal semiconductor crystal to the crystal face cut out by the wire, and a cutting direction.

## Claims

### Claim 1

A method of manufacturing a hexagonal semiconductor plate crystal by cutting a hexagonal semiconductor crystal using a crystal cutting wire,
wherein the hexagonal semiconductor crystal is cut by causing the crystal cutting wire to move relative to the hexagonal semiconductor crystal so as to satisfy conditions of Expressions (A) and (B):
25°<α≦90° Expression (A); and
β=90°±5° Expression (B)
where α represents an angle formed by a c axis of the hexagonal semiconductor crystal and a normal line of a crystal face cut out by the wire, and β represents an angle formed by a reference axis, which is obtained by perpendicularly projecting the c axis of the hexagonal semiconductor crystal to the crystal face cut out by the wire, and a cutting direction.

### Claim 2 (depends on 1)

The method of manufacturing a hexagonal semiconductor plate crystal according to claim 1, wherein a moving speed of the crystal cutting wire in the cutting direction is equal to or more than 1 mm/h.

### Claim 3 (depends on 1)

The method of manufacturing a hexagonal semiconductor plate crystal according to claim 1, wherein the hexagonal semiconductor plate crystal is cut by causing the crystal cutting wire to move so as to satisfy a condition of Expression (C):
0°≦γ<75° Expression (C)
where γ represents an angle formed by an extending direction of the crystal cutting wire and the reference axis.

### Claim 4 (depends on 1)

The method of manufacturing a hexagonal semiconductor plate crystal according to claim 1, wherein a magnitude of warpage of the plate crystal is equal to or less than 1.0 μm/mm.

### Claim 5 (depends on 1)

The method of manufacturing a hexagonal semiconductor plate crystal according to claim 1, wherein a maximum diameter of the plate crystal is equal to or more than 10 mm.

### Claim 6 (depends on 1)

The method of manufacturing a hexagonal semiconductor plate crystal according to claim 1, wherein the plate crystal is manufactured by cutting two or more faces at a time using a plurality of crystal cutting wires installed in parallel with a specific gap therebetween.

### Claim 7 (depends on 1)

The method of manufacturing a hexagonal semiconductor plate crystal according to claim 1, wherein a face formed by the cutting is ground after the cutting.

### Claim 8 (depends on 1)

The method of manufacturing a hexagonal semiconductor plate crystal according to claim 1, wherein the hexagonal semiconductor crystal is a Group-III nitride semiconductor crystal.

### Claim 9 (depends on 1)

The method of manufacturing a hexagonal semiconductor plate crystal according to claim 1, wherein the hexagonal semiconductor crystal is a gallium nitride crystal.