# US 2013/0284084 A1 · Crucibles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284084 A1
- Document ID: US20130284084A1
- Status: Published application
- Kind: A1
- Application number: 13/997,155
- Filed: 2011-12-19
- Published: 2013-10-31
- Earliest claimed: 2010-12-22
- Assignees: Steuler Solor GMBH
- Inventors: Rune Roligheten
- Web page: https://patentgrep.com/patent/US20130284084A1

## CPC

- C30B 28/06: by normal freezing or freezing under temperature gradient
- C04B 35/591: obtained by reaction sintering
- C30B 11/002: {Crucibles or containers for supporting the melt}
- C30B 29/06: Silicon
- C04B 2235/3272: Iron oxides or oxide forming salts thereof, e.g. hematite, magnetite
- C04B 2235/3826: Silicon carbides
- C04B 2235/428: Silicon
- C04B 2235/46: Gases other than oxygen used as reactant, e.g. nitrogen used to make a nitride phase
- C04B 2235/5436: micrometer sized, i.e. from 1 to 100 micron
- C04B 2235/5472: Bimodal, multi-modal or multi-fraction
- C04B 2235/656: characterised by specific heating conditions during heat treatment
- C04B 2235/6562: Heating rate
- C04B 2235/6567: Treatment time
- C04B 2235/77: Density
- Y10T 117/1024: for crystallization from liquid or supercritical state
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for manufacturing a crucible for the crystallization of silicium comprising the steps of •preparing a slurry of solids and liquids, said solids consisting of •silicon metal powder •up to 25% (w/w) SiC powder •up to 10% (w/w) SiN •up to 0.5% (w/w) of a catalyst •up to 1% (w/w) of a binder •forming the slurry into a green body of a crucible •heating the green body in a nitrogen atmosphere, optionally comprising inert gas, to react the silicon at least partially to silicon nitride.

## Claims

### Claim 1

A method for manufacturing a crucible for the crystallization of silicon comprising the steps of
preparing a slurry of solids and liquids, said solids consisting of
silicon metal powder
up to 25% (w/w) SiC powder
up to 10% (w/w) SiN
up to 0.5% (w/w) of a catalyst
up to 1% (w/w) of a binder
forming the slurry into a green body of a crucible
heating the green body in a nitrogen atmosphere, optionally comprising inert gas, to react the silicon at least partially to silicon nitride.

### Claim 2 (depends on 1)

The method of claim 1, wherein the particle size of the silicon metal powder is in the range of 0 to 100 μm, preferably 0 to 45 μm.

### Claim 3 (depends on 1)

The method of claim 1, wherein at least 75% (w/w) of the solids are silicon metal powder.

### Claim 4 (depends on 1)

The method of claim 1, wherein the solids comprise up to 15% (w/w) SiC powder.

### Claim 5 (depends on 1)

The method of claim 1, wherein the catalyst is FeO and/or the binder is an aqueous polymer dispersion.

### Claim 6 (depends on 1)

The method of claim 1, wherein the inert gas is selected from argon, helium and mixtures thereof.

### Claim 7 (depends on 1)

The method of claim 1, wherein the pressure of the nitrogen, optionally including inert gas, atmosphere is between 200 and 1400 mbar.

### Claim 8 (depends on 1)

The method of claim 1, wherein heating is conducted at temperatures above 1050° C., preferably above 1250° C., more preferably above 1400° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein heating is conducted for 3 to 14 days at temperatures above 1000° C.

### Claim 10 (depends on 1)

The method of claim 1, wherein the silicon metal powder is in a bimodal or multimodal particle size distribution.

### Claim 11 (depends on 1)

A crucible obtainable by the method of claim 1.

### Claim 12 (depends on 11)

The crucible of claim 11 having an apparent porosity of 14 to 25%, measured according to ASTM C-20.

### Claim 13 (depends on 11)

The crucible of claim 11 having a density of 2.3 to 2.6 kg/dm3.

### Claim 14 (depends on 11)

A method of using the crucible of claim 11 for the crystallization of silicon, comprising the steps of
filling melted silicon into the crucible
allowing the melted silicon to crystallize.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the silicon is monocrystalline.

### Claim 16 (depends on 14)

The method according to claim 14, wherein the silicon is polycrystalline.

### Claim 17 (depends on 11)

A method for crystallization of silicon, comprising utilizing the crucible of claim 11, in which silicon is melted and then allowed to crystallize.

### Claim 18 (depends on 1)

A method for crystallization of silicon, comprising:
filling melted silicon into the crucible made according to the method of claim 1; and
allowing the melted silicon to crystallize.