# US 2013/0284083 A1 · MANUFACTURING APPARATUS OF SiC SINGLE CRYSTAL AND METHOD FOR MANUFACTURING SiC SINGLE CRYSTAL

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284083 A1
- Document ID: US20130284083A1
- Status: Published application
- Kind: A1
- Application number: 13/997,722
- Filed: 2011-12-26
- Published: 2013-10-31
- Earliest claimed: 2010-12-27
- Assignees: Toyota Jidosha Kabushiki Kaisha; Nippon Steel & Sumitomo Metal Corporation
- Inventors: Nobuhiro Okada; Kazuhito Kamei; Kazuhiko Kasunoki; Nobuyoshi Yashiro; Kouji Moriguchi; Hironori Daikoku; Hiroshi Suzuki; Tomokazu Ishii; Hidemitsu Sakamoto; Motohisa Kado; Yoichiro Kawai
- Web page: https://patentgrep.com/patent/US20130284083A1

## CPC

- C30B 15/20: Controlling or regulating (controlling or regulating in general G05)
- C30B 15/14: Heating of the melt or the crystallised materials
- C30B 15/30: Mechanisms for rotating or moving either the melt or the crystal (flotation methods C30B15/28)
- C30B 17/00: Single-crystal growth onto a seed which remains in the melt during growth, e.g. Nacken-Kyropoulos method (C30B15/00 takes precedence)
- C30B 29/36: Carbides
- C30B 15/305: {Stirring of the melt}
- Y10T 117/1068: including heating or cooling details [e.g., shield configuration]
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A manufacturing apparatus for SiC single crystal has a control unit to control induction heating such that frequency f (Hz) of alternating current to be passed to the induction heating unit satisfies Formula (1); D1 (mm) is permeation depth of electromagnetic waves into a side wall of a crucible by the heating unit, D2 (mm) is permeation depth of electromagnetic waves into a SiC solution, T (mm) is thickness of the crucible side wall of the crucible, and R (mm) is crucible inner radius: (D1−T)×D2/R>1 (1) where, D1 is defined by Formula (2), and D2 by Formula (3): D1=503292×(1/(f×σc×μc))1/2 (2) D2=503292×(1/(f×σs×μs))1/2 (3); σc is electric conductivity (S/m) of the sidewall, σs is electric conductivity (S/m) of the SiC solution; μc is relative permeability of the sidewall, and μs relative permeability of the SiC solution.

## Claims

### Claim 1

A manufacturing apparatus of a SiC single crystal, comprising:
a crucible including a tubular side wall and a bottom wall disposed at a lower end of the side wall, the crucible being able to house a SiC solution;
a chamber housing the crucible;
a vertical seed shaft having a lower end surface to which a SiC seed crystal is to be attached, the seed shaft being able to bring the SiC seed crystal attached to the lower end surface into contact with the SiC solution;
an induction heating unit disposed around the side wall of the crucible in the chamber; and
a control unit for controlling the induction heating unit, wherein
the control unit controls the induction heating unit such that a frequency f (Hz) of alternating current to be passed to the induction heating unit satisfies Formula (1), where D1 (mm) indicates a permeation depth of electromagnetic waves into the side wall by the induction heating unit, D2 (mm) indicates a permeation depth of electromagnetic waves into the SiC solution by the induction heating unit, T (mm) indicates a thickness of the side wall, and R (mm) indicates an inner radius of the crucible:
(D1−T)×D2/R>1 (1)
where, D1 is defined by Formula (2), and D2 is defined by Formula (3):
D1=503292×(1/(f×σc×μc))1/2 (2)
D2=503292×(1/(f×σs×μs))1/2 (3)
where, σc is an electric conductivity (S/m) of the side wall, σs is an electric conductivity (S/m) of the SiC solution, μc is a relative permeability (dimensionless quantity) of the side wall, and μs a relative permeability (dimensionless quantity) of the SiC solution.

### Claim 2 (depends on 1)

The manufacturing apparatus according to claim 1, wherein
an inner surface of the side wall of the crucible contains carbon.

### Claim 3

A method for manufacturing a SiC single crystal, comprising the steps of:
providing a manufacturing apparatus comprising: a crucible including a tubular side wall and a bottom wall disposed at a lower end of the side wall, the crucible housing a SiC solution; a chamber housing the crucible; a vertical seed shaft, a SiC seed crystal attached to a lower end surface of the seed shaft; and an induction heating unit disposed around the side wall of the crucible in the chamber;
bringing the SiC seed crystal attached to the seed shaft into contact with the SiC solution in the crucible;
controlling the induction heating unit such that a frequency f (Hz) of alternating current to be passed to the induction heating unit satisfies Formula (1), where D1 (mm) indicates a permeation depth of electromagnetic waves into the side wall by the induction heating unit, D2 (mm) indicates a permeation depth of electromagnetic waves into the SiC solution by the induction heating unit, T (mm) indicates a thickness of the side wall, and R (mm) indicates an inner radius of the crucible; and
growing a SiC single crystal on the SiC seed crystal while rotating the seed shaft:
(D1−T)×D2/R>1 (1)
where, D1 is defined by Formula (2), and D2 is defined by Formula (3):
D1=503292×(1/(f×σc×μc))1/2 (2)
D2=503292×(1/(f×σs×μs))1/2 (3)
where, σc is an electric conductivity (S/m) of the side wall, and σs is an electric conductivity (S/m) of the SiC solution; μc is a relative permeability (dimensionless quantity) of the side wall, and μs is a relative permeability (dimensionless quantity) of the SiC solution.