# US 2013/0284070 A1 · Dimensionally stable geopolymer composition and method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284070 A1
- Document ID: US20130284070A1
- Status: Published application
- Kind: A1
- Application number: 13/842,100
- Filed: 2013-03-15
- Published: 2013-10-31
- Earliest claimed: 2012-04-27
- Assignees: United States Gypsum Company
- Inventors: Ashish DUBEY
- Web page: https://patentgrep.com/patent/US20130284070A1

## CPC

- C04B 28/006: {containing mineral polymers, e.g. geopolymers of the Davidovits type}
- C04B 11/28: Mixtures thereof with other inorganic cementitious materials (C04B7/04, C04B7/153 take precedence)
- C04B 12/005: {Geopolymer cements, e.g. reaction products of aluminosilicates with alkali metal hydroxides or silicates}
- C04B 24/32: Polyethers, e.g. alkylphenol polyglycolether
- C04B 28/003: {containing hybrid binders other than those of the polycarboxylate type}
- C04B 28/18: containing mixtures of the silica-lime type
- C04B 2103/32: Superplasticisers
- C04B 2111/00482: {Coating or impregnation materials}
- C04B 2111/00586: {Roofing materials}
- C04B 2111/0075: {for road construction}
- C04B 2111/34: Non-shrinking or non-cracking materials
- C04B 2111/343: {Crack resistant materials}
- C04B 2111/346: {Materials exhibiting reduced plastic shrinkage cracking}
- C04B 2111/62: Self-levelling compositions
- C04B 2111/72: Repairing or restoring existing buildings or building materials
- Y02P 40/10: Production of cement, e.g. improving or optimising the production methods; Cement grinding
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method for making geopolymer cementitious binder compositions for cementitious products such as concrete, precast construction elements and panels, mortar, patching materials for road repairs and other repair materials, and the like is disclosed. The geopolymer cementitious compositions of some embodiments are made by mixing a synergistic mixture of thermally activated aluminosilicate mineral, calcium sulfoaluminate cement, a calcium sulfate and a chemical activator with water.

## Claims

### Claim 1

An aluminosilicate geopolymer composition comprising the reaction product of a thermally activated aluminosilicate mineral; a calcium sulfoaluminate cement; a calcium sulfate selected from the group consisting of calcium sulfate dihydrate, calcium sulfate hemihydrate, anhydrous calcium sulfate and mixtures thereof; a chemical activator selected from the group consisting of an alkali metal salt and an alkali metal base and mixtures thereof, and water.

### Claim 2 (depends on 1)

The aluminosilicate geopolymer composition of claim 1 comprising the reaction product of about 33 to about 97% by weight of the thermally activated aluminosilicate mineral, about 1 to about 40% by weight of the calcium sulfoaluminate cement, about 1 to about 40% by weight of the calcium sulfate, about 1.0 to about 6.0% by weight of the chemical activator selected from the group consisting of an alkali metal salt and an alkali metal base, and water.

### Claim 3 (depends on 1)

The composition of claim 1, wherein the chemical activator comprises an alkali metal citrate, and the thermally activated aluminosilicate mineral comprises Class C fly ash.

### Claim 4 (depends on 1)

The composition of claim 1, comprising a reaction product of amounts of the chemical activator and calcium sulfate relative to the amounts of the thermally activated aluminosilicate mineral and calcium sulfoaluminate cement effective to cause the reaction product to set in a predetermined time after mixing with water.

### Claim 5 (depends on 4)

The composition of claim 4, wherein the amounts of the chemical activator and calcium sulfate relative to the amounts of thermally activated aluminosilicate mineral and calcium sulfoaluminate cement are effective to cause the reaction product to set in about 120 minutes or less after mixing with water.

### Claim 6 (depends on 1)

The composition of claim 1, comprising a reaction product of an amount of calcium sulfoaluminate cement relative to the amounts of the chemical activator, calcium sulfate and thermally activated aluminosilicate mineral effective to cause the reaction product to set in a predetermined time after mixing with water.

### Claim 7 (depends on 6)

The composition of claim 6, wherein the amount of calcium sulfoaluminate cement relative to the amounts of chemical activator, calcium sulfate and thermally activated aluminosilicate mineral is effective to cause the reaction product to set in about 120 minutes or less after mixing with water.

### Claim 8 (depends on 1)

The composition of claim 1, comprising a reaction product of an amount of calcium sulfoaluminate cement, calcium sulfate and chemical activator relative to the amount of thermally activated aluminosilicate mineral effective to limit shrinkage of the composition to less than about 0.3%.

### Claim 9 (depends on 8)

The composition of claim 8, wherein the shrinkage of the composition is limited to less than about 0.05%.

### Claim 10 (depends on 1)

The composition of claim 1 wherein the reaction product is formed from water and a thermally activated aluminosilicate mineral comprising about 60% to about 90% by weight thermally activated aluminosilicate mineral and Class C fly ash; about 4% to about 35% by weight calcium sulfoaluminate cement, about 4.0% to about 15% by weight calcium sulfate, and about 1.25 to 4.00% by weight chemical activators.

### Claim 11 (depends on 1)

The composition of claim 1 wherein the reaction product is formed from water; and about 60% to about 85% by weight of a thermally activated mineral comprising Class C fly ash, about 8% to about 30% by weight calcium sulfoaluminate cement, about 4.0% to about 15% by weight calcium sulfate, and about 1.5 to 3.00% by weight chemical activator.

### Claim 12 (depends on 1)

The composition of claim 1 wherein the reaction product is formed from calcium sulfate with an average particle size from about 1 to about 100 microns.

### Claim 13 (depends on 1)

The composition of claim 1 having a 4-hour compressive strength from about 1000 psi (6.9 MPa) to about 2500 psi (17.2 MPa)

### Claim 14 (depends on 1)

The composition of claim 1 having a 24-hour compressive strength about 1500 psi (10.3 MPa) to about 3500 psi (24.1 MPa).

### Claim 15 (depends on 1)

The composition of claim 1 having a 28-day compressive strength from about 3500 psi (24.1 MPa) to about 10000 psi (69 MPa).

### Claim 16 (depends on 1)

The composition of claim 1 having a water saturated compressive strength at 28-days from about 3500 psi (24.1 MPa) to about 10000 psi (69 MPa).

### Claim 17 (depends on 1)

The composition of claim 1 having a 4-hour compressive strength from about 1000 psi (6.9 MPa) to about 2500 psi (17.2 MPa) and a 24-hour compressive strength about 1500 psi (10.3 MPa) to about 3500 psi (24.1 MPa).

### Claim 18 (depends on 1)

The composition of claim 1 having a 4-hour compressive strength from about 1000 psi (6.9 MPa) to about 2500 psi (17.2 MPa), and a 28-day compressive strength from about 3500 psi (24.1 MPa) to about 10000 psi (69 MPa).

### Claim 19 (depends on 1)

The composition of claim 1 having a 4-hour compressive strength from about 1000 psi (6.9 MPa) to about 2500 psi (17.2 MPa) and a water saturated compressive strength at 28-days from about 3500 psi (24.1 MPa) to about 10000 psi (69 MPa).

### Claim 20 (depends on 1)

The composition of claim 1, wherein the composition has a tensile bonding strength to substrates in excess of 200 psi.

### Claim 21 (depends on 1)

The composition of claim 1 wherein the reaction product is formed from water; and a thermally activated aluminosilicate mineral; a calcium sulfoaluminate cement; a calcium sulfate selected from the group consisting of calcium sulfate dihydrate, calcium sulfate hemihydrate, anhydrous calcium sulfate and mixtures thereof; a chemical activator selected from the group consisting of an alkali metal salt and an alkali metal base; and a filler.

### Claim 22 (depends on 1)

The composition of claim 1, wherein the reaction product results from an exothermic reaction in a water slurry, wherein the amount of calcium sulfoaluminate cement, calcium sulfate and chemical activator relative to the amount of thermally activated aluminosilicate mineral is effective to limit the maximum slurry temperature rise to about 50° F. or less.

### Claim 23 (depends on 22)

The composition of claim 22, wherein the maximum slurry temperature rise is limited to less than about 40° F.

### Claim 24 (depends on 22)

The composition of claim 22, wherein the reaction product exhibits lower thermal expansion and enhance resistance to thermal cracking.

### Claim 25 (depends on 1)

The composition of claim 1, wherein the weight ratio of the mixture to water is less than about 0.4.

### Claim 26 (depends on 1)

The composition of claim 1, wherein the weight ratio of the mixture to water is less than about 0.3.

### Claim 27 (depends on 1)

The composition of claim 1, wherein the composition has improved fluidity and workability as shown in slump testing of the composition wherein the slump patties have relatively large diameters and no early age cracking upon drying.

### Claim 28

A settable mixture for forming an aluminosilicate geopolymer composition when reacted in water, comprising:
about 33 to about 97% by weight of a thermally activated aluminosilicate mineral;
about 1 to about 40% by weight of a calcium sulfoaluminate cement,
about 1 to about 40% by weight of a calcium sulfate selected from the group consisting of calcium sulfate dihydrate, calcium sulfate hemihydrate, anhydrous calcium sulfate and mixtures thereof; and
about 1.0 to about 6.0% by weight of a chemical activator selected from the group consisting of an alkali metal salt and an alkali metal base, and mixtures thereof.

### Claim 29 (depends on 28)

The aluminosilicate geopolymer composition formed from the reaction of the mixture of claim 28 in water, wherein the shrinkage of the composition is less than about 0.3%.

### Claim 30 (depends on 28)

The aluminosilicate geopolymer compositon formed from the reaction of the mixture of claim 28 in water, wherein the shrinkage of the reaction product is less than about 0.05%

### Claim 31 (depends on 28)

The aluminosilicate geopolymer composition formed from the reaction of the mixture of claim 28 in water, wherein the composition has tensile bonding strength to other substrates in excess of 200 psi.

### Claim 32 (depends on 28)

The aluminosilicate geopolymer composition formed from the reaction of the mixture of claim 28 in water, wherein the geopolymer reaction product formed from the mixture has 4-hour compressive strength of from about 1000 psi (6.9 MPa) to greater than about 2500 psi (17.2 MPa); 24-hour compressive strength of about 1500 psi (10.3 MPa) to greater than about 3500 psi (24.1 MPa), and 28-day compressive strength of about 3500 psi (24.1 MPa) to about 10000 psi (69 MPa) and wherein the mixture has a set time of less than about 10 minutes to about 120 minutes after reacting the mixture in water.

### Claim 33 (depends on 28)

The aluminosilicate geopolymer composition formed from the reaction of the mixture of claim 28 in water, wherein the aluminosilicate geopolymer composition formed from the mixture has a controlled exothermic reaction with a maximum slurry temperature rise of less than about 50° F.

### Claim 34 (depends on 33)

The aluminosiicate geopolymer composition reaction of claim 33, wherein the composition exhibits low thermal expansion and enhanced resistance to thermal cracking.

### Claim 35 (depends on 28)

The aluminosiilcate geopolymer composition formed from the reaction of the mixture of claim 28 with water, wherein the weight ratio of the mixture to water is less than about 0.4.

### Claim 36 (depends on 28)

The aluminosilicate geopolymer composition formed from the reaction of the mixture of claim 28 with water, wherein the weight ratio of the mixture to water is less than about 0.3.

### Claim 37 (depends on 28)

The aluminosilicate geopolymer composition formed from the reaction of the mixture of claim 28 with water, wherein the composition has improved fluidity and workability as shown in slump testing of the composition wherein the slump patties have relatively large diameters and no early age cracking upon drying.

### Claim 38 (depends on 1)

The composition of claim 1 forming a construction repair material.

### Claim 39 (depends on 1)

The composition of claim 1 forming a floor repair material

### Claim 40 (depends on 1)

The composition of claim 1 forming a self leveling floor underlayment over a substrate.

### Claim 41 (depends on 1)

The composition of claim 1 forming a load bearing structure.

### Claim 42 (depends on 1)

The composition of claim 1 forming a panel surfacing material.

### Claim 43 (depends on 1)

The composition of claim 1 in the form of a binder in construction materials.

### Claim 44 (depends on 1)

The composition of claim 1 in the form of construction materials selected from the group consisting of brick, blocks and stones.

### Claim 45 (depends on 1)

The composition of claim 1 forming a wall surfacing material.

### Claim 46 (depends on 1)

The composition of claim 1 forming a pavement material for traffic bearing surfaces.

### Claim 47 (depends on 1)

The composition of claim 1 forming a repair material for traffic bearing surfaces.

### Claim 48 (depends on 1)

The composition of claim 1 in the form of a material for weight bearing structures.

### Claim 49 (depends on 1)

The composition of claim 1 in the form of a roofing material.

### Claim 50 (depends on 1)

The composition of claim 1 in the form of a shotcrete material.

### Claim 51 (depends on 1)

The composition of claim 1 in the form of a mortar.

### Claim 52

A method of preparing an aluminosilicate geopolymer composition, comprising:
reacting a thermally activated aluminosilicate mineral, a calcium sulfoaluminate cement, a calcium sulfate selected from the group consisting of calcium sulfate dihydrate, calcium sulfate hemihydrate, anhydrous calcium sulfate, and mixtures thereof, a chemical activator selected from the group consisting of an alkali metal salt and an alkali metal base and mixtures thereof, and water.

### Claim 53 (depends on 52)

The method of claim 52, wherein the aluminosilicate geopolymer comprises the reaction product of:
about 33 to about 97 parts by weight, of the thermally activated aluminosilicate mineral comprising class C fly ash,
about 1 to about 40 parts by weight of calcium sulfoaluminate cement,
about 1 to about 40 parts by weight of the calcium sulfate,
about 1.0 to about 6.0 parts of the chemical activator, and
water.

### Claim 54 (depends on 52)

The method of claim 52, wherein the chemical activator comprises an alkali metal citrate and wherein the thermally activated aluminosilicate mineral comprises Class C fly ash.

### Claim 55 (depends on 52)

The method of claim 52, wherein the composition further comprises a filler.

### Claim 56 (depends on 1)

The composition of claim 1 wherein the reaction product is formed from water; and a thermally activated aluminosilicate mineral; a calcium sulfoaluminate cement; a calcium sulfate selected from the group consisting of calcium sulfate dihydrate, calcium sulfate hemihydrate, anhydrous calcium sulfate and mixtures thereof; a chemical activator selected from the group consisting of an alkali metal salt and an alkali metal base or mixtures thereof; and less than about 15% by weight Portland cement.