# US 2013/0284007 A1 · Ballistic resistant article comprising a self-crosslinking acrylic resin and/or a crosslinkable acrylic resin and process to manufacture said article.

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284007 A1
- Document ID: US20130284007A1
- Status: Published application
- Kind: A1
- Application number: 13/979,667
- Filed: 2012-01-18
- Published: 2013-10-31
- Earliest claimed: 2011-01-18
- Assignees: Barrday Inc.; Teijin Aramid B.V.
- Inventors: Marc-Jan de Haas; Alex van Norel; Vincent van Bommel; Ramon van Rooij; Nicolas Cunningham; Chinkalben Patel
- Web page: https://patentgrep.com/patent/US20130284007A1

## CPC

- F41H 5/0485: {all the layers being only fibre- or fabric-reinforced layers}
- F41H 5/0435: {the additional layers being only fibre- or fabric-reinforced layers}
- F41H 5/0464: {the additional layers being only fibre- or fabric-reinforced layers}
- F41H 5/0478: {Fibre- or fabric-reinforced layers in combination with plastics layers}
- Y10T 156/10: Methods of surface bonding and/or assembly therefor
- F41H: ARMOUR; ARMOURED TURRETS; ARMOURED OR ARMED VEHICLES; MEANS OF ATTACK OR DEFENCE, e.g. CAMOUFLAGE, IN GENERAL
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A ballistic resistant article is presented comprising a plurality of fibrous layers, each of said layers comprising a network of fibers, wherein the fibers have a strength of at least 800 mN/tex (1100 MPa) according to ASTM D 7269-07 and a matrix material, wherein the matrix material comprises a mixture comprising at least one self-crosslinking acrylic resin and/or at least one crosslinkable acrylic resin, and at least one tackifier. Compared with an article of the same construction but with a matrix material without tackifier the article according to the invention comprises a higher adhesion between the fibrous layers both in the unaged and aged state and a lower water pick up after water soak and the article passes the gasoline soak test. The article additionally comprising a plate of metal or ceramic exhibits minimal or even no delamination of the fibrous layers after ballistic attack, whereas an article of the same construction but with a matrix material without tackifier exhibits interior delamination of the fibrous layers.

## Claims

### Claim 1

A ballistic resistant article comprising a plurality of fibrous layers, each of said layers comprising a network of fibers, wherein the fibers have a strength of at least 800 mN/tex (1100 MPa) according to ASTM D 7269-07 and a matrix material, wherein the matrix material comprises a mixture comprising
at least one self-crosslinking acrylic resin and/or at least one crosslinkable acrylic resin,
and at least one tackifier.

### Claim 2 (depends on 1)

The ballistic resistant article according to claim 1, wherein the tackifier is selected from the group consisting of rosin resins or terpene resins or hydrocarbon resins.

### Claim 3 (depends on 1, 2)

The ballistic resistant article according to claim 1 or 2, wherein the tackifier is present in the matrix material in a weight percentage with respect to the weight of the matrix material ranging from 1 wt. % to 20 wt. %.

### Claim 4 (depends on 1, 2, 3)

The ballistic resistant article according to one or more of claims 1 to 3, wherein the network of fibers is a unidirectional alignment of the fibers.

### Claim 5 (depends on 1, 4)

The ballistic resistant article according to one or more of claim 1 or 4, wherein the fibers are aramid fibers.

### Claim 6 (depends on 1, 2, 3, 4, 5)

The ballistic resistant article according article to one or more of claims 1 to 5, wherein the fibers have a weight wf, the matrix material has a weight wm and a weight percentage of the matrix material with respect to (wf+wm) is from 5 wt. % to 50 wt. %.

### Claim 7 (depends on 1, 2, 3, 4, 5, 6)

The ballistic resistant article according article to one or more of claims 1 to 6, wherein the areal density of the fibers in a single fibrous layer ranges from 10 g/m2 to 250 g/m2.

### Claim 8 (depends on 1, 2, 3, 4, 5, 6, 7)

The ballistic resistant article according article to one or more of claims 1 to 7, wherein the total areal density of a single fibrous layer ranges from 11 g/m2 to 350 g/m2.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

The ballistic resistant article according article to one or more of claims 1 to 8, wherein the plurality of fibrous layers is formed into a panel and the panel is joined to a plate of metal or ceramic.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9)

Ballistic resistant article according to one or more of claims 1 to 9, wherein a scrim comprising a thermoplastic material is situated between the fibrous layers.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

A process to manufacture a ballistic resistant article of one or more of claims 1 to 10 comprising the steps:
(1) Manufacture of a single unidirectional fibrous layer comprising a matrix material, which comprises a mixture comprising
at least one self-crosslinking acrylic resin and/or at least one crosslinkable acrylic resin, and
at least one tackifier,
(2) manufacture of an adherent cross-ply from at least two unidirectional single fibrous layers resulting from step (1),
(3) manufacture of a consolidated panel from a number of adherent cross-plies resulting from step (2), and optionally
(4) joining of the consolidated panel resulting from step (3) to a plate of metal or ceramic to yield a hard-ballistic resistant article.

### Claim 12 (depends on 11)

The process according to claim 11, wherein a cross-linking reaction of the at least one self-crosslinking acrylic resin and/or of the at least one crosslinkable acrylic resin is comprised in at least one of the steps (1), (2) and (3).