# US 2013/0284004 A1 · Composite material; a ballistic resistant article made from same and method of making the article

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0284004 A1
- Document ID: US20130284004A1
- Status: Published application
- Kind: A1
- Application number: 13/545,503
- Filed: 2012-07-10
- Published: 2013-10-31
- Earliest claimed: 2011-10-17
- Assignees: E. I. Du Pont de Nemours and Company
- Inventors: Jeffrey Alan Hanks; Brian Charles West; John Henry McMinn; Bryce Vanarsdalen
- Web page: https://patentgrep.com/patent/US20130284004A1

## CPC

- B32B 38/0004: {Cutting, tearing or severing, e.g. bursting; Cutter details (cutting in general B26D; laminating combined with punching or perforating B32B38/04; removing all or part of the layers B32B38/10; cutting in combination with laying up and registration B32B38/185 takes precedence)}
- A42B 3/063: {using layered structures}
- B29C 70/222: {the structure being shaped to form a three dimensional configuration}
- B29C 70/56: Tensioning reinforcements before or during shaping
- B32B 5/024: {Woven fabric}
- B32B 5/12: characterised by the relative arrangement of fibres or filaments of {different layers, e.g. the fibres or filaments being parallel or perpendicular to each other}
- B32B 5/26: another layer {next to it} also being fibrous or filamentary {(relative arrangement of fibres or filaments of different layers B32B5/12)}
- F41H 1/08: of plastics; Plastic head-shields
- F41H 5/0485: {all the layers being only fibre- or fabric-reinforced layers}
- A42C 2/00: Manufacturing helmets by processes not otherwise provided for
- B29L 2031/4821: {Helmets}
- B29L 2031/768: {Protective equipment (B29L2031/4821 takes precedence)}
- B32B 2260/021: Fibrous or filamentary layer
- B32B 2260/046: Synthetic resin
- B32B 2305/188: Woven fabrics
- B32B 2307/718: Weight, e.g. weight per square meter
- B32B 2309/06: Angles
- B32B 2571/02: defensive, e.g. armour plates or anti-ballistic clothing
- Y10T 156/1075: of plural laminae from single stock and assembling to each other or to additional lamina
- Y10T 428/24942: including components having same physical characteristic in differing degree
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- A42B: HATS; HEAD COVERINGS (headbands A41D20/00; head-scarves A41D23/00)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- F41H: ARMOUR; ARMOURED TURRETS; ARMOURED OR ARMED VEHICLES; MEANS OF ATTACK OR DEFENCE, e.g. CAMOUFLAGE, IN GENERAL
- A42C: MANUFACTURING OR TRIMMING HEAD COVERINGS, e.g. HATS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A fiber reinforced resin composite for ballistic protection comprising a plurality of first and second plies wherein the first and second plies further comprise a woven fabric and a polymeric resin. The fabric has a Russell tightness factor of from 0.2 to 0.7 and a cover factor of at least 0.45, The fabric is impregnated with the resin, the resin comprising from 5 to 30 weight percent of the total weight of fabric plus resin. The fabric of each first and second ply comprises regions wherein the fabric is distorted from an orthogonal woven state by a distortion angle of least 30 degrees. The composite may further comprising a third ply having a surface area no greater than 50% of the surface area of a first and second ply. The ratio of the number of first plus second plies to the number of third plies is from 2:1 to 12:1.

## Claims

### Claim 1

A contoured fiber reinforced resin composite for ballistic protection comprising a plurality of first and second plies arranged such that a plurality of first plies is followed by a plurality of second plies, wherein, yarn orientations in the weave of each plurality of plies, are substantially aligned to each other, and wherein the plurality of first and second plies further comprise (i) a woven fabric made from a plurality of polymeric yarns having a yarn tenacity of from 15 grams per dtex to 50 grams per dtex and a modulus of from 200 grams per dtex to 2200 grams per dtex, and (ii) a polymeric resin,
wherein
(a) the fabric has a Russell tightness factor of from 0.2 to 0.7,
(b) the fabric has an areal weight of from 80 gsm to 510 gsm,
(c) the fabric has a cover factor of at least 0.45,
(d) the fabric is impregnated with the resin, the resin comprising from 5 to 30 weight percent of the total weight of fabric plus resin, and
(e) the fabric of each first and second ply comprises regions wherein the fabric is distorted from an orthogonal woven state by a distortion angle of least 30 degrees.

### Claim 2 (depends on 1)

The composite of claim 1 wherein the number of plies comprising the plurality of first or second plies is from 2 to 250.

### Claim 3 (depends on 1)

The composite of claim 1 wherein the polymer of the yarns of the fabric of the first and second plies is para-aramid, polyethylene, polyazole or mixtures thereof.

### Claim 4 (depends on 1)

The composite of claim 1 wherein the fabric of each first and second ply comprises regions wherein the fabric is distorted from an orthogonal woven state by a distortion angle of least 40 degrees.

### Claim 5 (depends on 1)

The composite of claim 1 wherein the yarn orientation of a second ply is offset at an angle of from 20 to 70 degrees with respect to the yarn orientation of a first ply.

### Claim 6 (depends on 5)

The composite of claim 5 wherein the yarn orientation of a second ply is offset at an angle of from 40 to 50 degrees with respect to the yarn orientation of a first ply.

### Claim 7 (depends on 5)

The composite of claim 5 further comprising a third ply, the third ply comprising (i) a woven fabric made from a plurality of polymeric yarns having a yarn tenacity of from 15 grams per dtex to 50 grams per dtex and a modulus of from 200 grams per dtex to 2200 grams per dtex, and (ii) a polymeric resin, wherein,
(a) the surface area of a third ply is no greater than 50% of the surface area of a first and second ply,
(b) the fabric has a Russell tightness factor of from 0.2 to 0.7,
(c) the fabric has an areal weight of from 80 gsm to 510 gsm,
(d) the fabric has a cover factor of at least 0.45,
(e) the fabric is impregnated with the resin, the resin comprising from 5 to 30 weight percent of the total weight of fabric plus resin, and
(f) the ratio of the number of first plus second plies to the number of third plies in the composite is in the range of from 2:1 to 12:1.

### Claim 8 (depends on 7)

The composite of claim 7 wherein a third ply located between any two first plies has the same yarn orientation as the yarns of a first ply.

### Claim 9 (depends on 7)

The composite of claim 7 wherein a third ply located between any two second plies has the same yarn orientation as the yarns of a second ply.

### Claim 10 (depends on 7)

The composite of claim 7 wherein a third ply is located at the intersection between a plurality of first plies and a plurality of second plies.

### Claim 11 (depends on 7)

The composite of claim 7 wherein there are no cuts, darts, pleats or folds in the first, second and third plies.

### Claim 12 (depends on 7)

The composite of claim 7 wherein the geometric shape of the third ply is circular, oval, square, rectangular, diamond, pentagonal, hexagonal, octagonal or cross shaped.

### Claim 13 (depends on 7)

The composite of claim 7 wherein the polymer of the yarns of the third ply is para-aramid, polyethylene, polyazole or mixtures thereof.

### Claim 14 (depends on 1)

A ballistic resistant article comprising the composite of claim 1.

### Claim 15 (depends on 7)

A ballistic resistant article comprising the composite of claim 7.

### Claim 16

A method of forming a curved fiber reinforced resin composite article comprising the steps of
(i) providing a roll of resin impregnated fabric composite comprising a woven fabric made from a plurality of polymeric yarns having a yarn tenacity of from 15 grams per dtex to 50 grams per dtex and a modulus of from 200 grams per dtex to 2200 grams per dtex, and a polymeric resin, wherein
(a) the fabric has a Russell tightness factor of from 0.2 to 0.7, (b) the fabric has an areal weight of from 80 gsm to 510 gsm,
(c) the fabric has a cover factor of at least 0.5, and,
(d) the fabric is impregnated with the polymeric resin, the resin comprising from 5 to 30 weight percent of the of the total weight of fabric plus resin,
(ii) cutting a plurality of plies from the fabric composite roll to provide first and second plies such that the plies have a shape profile similar to the final shape profile of the article being formed,
(iii) cutting a plurality of plies from the fabric composite roll to provide third plies such that the surface area of a third ply is no greater than 50% of the surface area of the first or second plies,
(iv) tensioning the corners or edges of the first and second plies to cause regions of the ply to distort by a distortion angle of at least 30 degrees,
(v) assembling a plurality of first plies followed by a plurality of second plies with third plies interspersed at a pre-determined frequency within the pluralities of first and second plies such that the ratio of the number of first plus second plies to the number of third plies is in the range of from 2:1 to 12:1 and the orientation of a second ply is offset at an angle of from 20 to 70 degrees with respect to the orientation of a first ply, and
(vi) consolidating the assembly of step (v) at a temperature of from 115° C. to 230° C. and an applied force of from 34 to 800 tonnes for between 5 to 60 minutes to form a cured composite article.

### Claim 17 (depends on 16)

The method of claim 16 wherein the polymer of the yarns of the first, second and third plies is para-aramid, polyethylene, polyazole or mixtures thereof.

### Claim 18 (depends on 16)

The method of claim 16 wherein the fabric of each first and second ply comprises regions wherein the fabric is distorted from an orthogonal woven state by a distortion angle of least 40 degrees.

### Claim 19

A method of forming a curved fiber reinforced resin composite article comprising the steps of
(i) providing a roll of resin impregnated fabric composite comprising a woven fabric made from a plurality of polymeric yarns having a yarn tenacity of from 15 grams per dtex to 50 grams per dtex and a modulus of from 200 grams per dtex to 2200 grams per dtex, and a polymeric resin, wherein
(a) the fabric has a Russell tightness factor of from 0.2 to 0.7,
(b) the fabric has an areal weight of from 80 gsm to 510 gsm,
(c) the fabric has a cover factor of at least 0.5, and,
(d) the fabric is impregnated with the polymeric resin, the resin comprising from 5 to 30 weight percent of the of the total weight of fabric plus resin,
(ii) cutting a plurality of plies from the fabric composite roll to provide first and second plies such that the plies have a shape profile similar to the final shape profile of the article being formed,
(iii) cutting a plurality of plies from the fabric composite roll to provide third plies such that the surface area of a third ply is no greater than 50% of the surface area of the first or second plies, the third plies having at least two different shapes,
(iv) tensioning the corners or edges of the first and second plies to cause regions of the ply to distort by a distortion angle of at least 30 degrees,
(v) assembling a plurality of first plies followed by a plurality of second plies with third plies interspersed at a pre-determined frequency within the pluralities of first and second plies such that
the ratio of the number of first plus second plies to the number of third plies is in the range of from 2:1 to 12:1,
the yarn orientation of a second ply is offset at an angle of from 20 to 70 degrees with respect to the yarn orientation of a first ply,
the third plies interspersed within a plurality of first or second plies have the same orientation as the plies between which they are interspersed, and
(vi) consolidating the assembly of step (v) at a temperature of from 115° C. to 230° C. and an applied force of from 34 to 800 tonnes for between 5 to 60 minutes to form a cured composite article.

### Claim 20 (depends on 19)

The method of claim 19 further comprising the step of positioning a third ply at the intersection of a plurality of first plies and a plurality of second plies.