# US 2013/0283883 A1 · Metal Gasket

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0283883 A1
- Document ID: US20130283883A1
- Status: Published application
- Kind: A1
- Application number: 13/925,038
- Filed: 2013-06-24
- Published: 2013-10-31
- Earliest claimed: 2007-03-09
- Assignees: Federal-Mogul Corporation
- Applicants: Federal-Mogul Corporation
- Inventors: Bhawani Tripathy; Thomas O. Zurfluh
- Web page: https://patentgrep.com/patent/US20130283883A1

## CPC

- F16J 15/0806: {characterised by material or surface treatment}
- F16J 15/0818: {Flat gaskets}
- F16J: PISTONS {(specially adapted for dampers F16F9/32)}; CYLINDERS; SEALINGS

## Abstract

A metal gasket includes embossments that exhibit essentially full functional recovery and full retained internal stress at temperatures up to about 1000° F. which is made from sheet material that is cold rolled and whose embossments are work hardened without any post embossment heat treating that would act to harden the material. This material may also receive a precipitation hardening heat treatment prior to being embossed. The gasket materials include alloys having greater than about 18% Ni, greater than about 14% Cr, from about 0.1 to 10% of at least one of Mo, Ti, V, Al, Co, Nb, Ta or Cu and the balance Fe with incidental impurities, which are cold rolled without any post embossment heat treating that would act to harden the material.

## Claims

### Claim 1

A method of making an embossed metal gasket, comprising the steps of
forming an annealed sheet of an iron-nickel-chromium alloy;
deforming said annealed sheet to form a deformed sheet having a deformed microstructure; and
forming a gasket from said deformed sheet having a least one embossed sealing bead; said embossed sealing bead sealably operable with an amount of retained stress greater than a critical level of retained stress in a fully-clamped, sealed joint at an operating temperature up to about 1000° F.

### Claim 2 (depends on 1)

The method of claim 1, wherein said embossed sealing bead is sealably operable with substantially full retained stress in a fully-clamped, sealed joint at an operating temperature up to about 1000° F.

### Claim 3 (depends on 1)

The method of claim 1, wherein said step of deforming comprises cold rolling the annealed sheet to produce a cold-rolled microstructure having a degree of deformation that varies as a function of a percentage of cold reduction.

### Claim 4 (depends on 3)

The method of claim 3, wherein said percentage of cold reduction ranges from 10-70%.

### Claim 5 (depends on 3)

The method of claim 3, wherein said percentage of cold reduction ranges from 30-40%.

### Claim 6 (depends on 3)

The method of claim 3, wherein said step of deforming produces a degree of deformation sufficient to provide said deformed sheet with a tensile elongation in a rolling direction of about 6-25%.

### Claim 7 (depends on 6)

The method of claim 6, wherein said step of deforming produces a degree of deformation sufficient to provide said deformed sheet with a tensile elongation in a rolling direction of about 7-10%.

### Claim 8 (depends on 2)

The method of claim 2, wherein said iron-nickel-chromium alloy comprises, by weight: greater than 18% nickel; greater than 14% Cr; 0.1-10% of at least one element selected from the group consisting of Mo, Ti, V, Al, Co, Nb, Ta and Cu; and the balance substantially Fe.

### Claim 9 (depends on 8)

The method of claim 8, wherein said alloy comprises, by weight: 24-55% Ni; 13.5-21% Cr; 1-3.3% Mo; 0-.15% Cu; 0-1% Si; 0-2% Mn; 0.65-2.3% Ti; 0-0.8% Al; 0.5% V; 0.001-0.01% B; 0-1.0% Co; 4.75-5.5% of the sum of Nb or Ta; 0-0-0.08% C; 0-0.015% S; 0-0.015% P; and the balance substantially Fe.

### Claim 10 (depends on 8)

The method of claim 8, wherein said alloy comprises, by weight: 50.00-55.00% Ni; 17.00-21.00% Cr; 2.80-3.30% Mo; 0-0.15% Cu; 0-0.35% Si; 0-0.35% Mn; 0.65-1.15% Ti; 0.35-0.80% Al; 0.001-0.006% B; 0-1.00% Co; 4.75-5.5% of the sum of Nb or Ta; 0-0.08% C; 0-0.015% S; 0-0.015% P; and the balance substantially Fe.

### Claim 11 (depends on 1)

The method of claim 1, further comprising a step of: providing a precipitation hardening heat treatment, wherein said deformed microstructure further comprises a deformed and precipitation hardened microstructure, wherein said deformed and precipitation hardened microstructure has a hardness which is greater than a hardness of said deformed microstructure.

### Claim 12 (depends on 1)

The method of claim 1, further comprising a step of: coating said gasket with a heat resistant coating.

### Claim 13 (depends on 12)

The method of claim 12, wherein said heat resistant coating comprises:
chemically exfoliated vermiculite wherein at least 90 weight percent of the vermiculite has a thickness of less than or equal to 30 microns and no dimension is greater than 1 millimeter;
a high temperature organic resin that is heat resistant to at least 300 degrees Celsius;
a supplementary inorganic resin; and
a flaky filler.